Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Density = 1.82 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Density 0.850 - 1.82 g/cc
0.0307 - 0.0658 lb/in³
Average value: 1.00 g/cc Grade Count:381
Overview of materials for Thermoplastic Olefinic Elastomer (TPO)
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Olefinic Elastomer (TPO)". Each property range of values reported is minimum and maximum v..
Density 1.72 - 1.82 g/cc
0.0621 - 0.0658 lb/in³
Average value: 1.79 g/cc Grade Count:10
Overview of materials for Diallyl Phthalate (DAP) Molding Compound, Long Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Diallyl Phthalate (DAP) Molding Compound, Long Glass Fiber Filled". Each property range of values report..
Density 1.16 - 1.82 g/cc
0.0419 - 0.0658 lb/in³
Average value: 1.45 g/cc Grade Count:136
Overview of materials for Nylon 6, Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and max..
Density 1.11 - 1.82 g/cc
0.0401 - 0.0658 lb/in³
Average value: 1.38 g/cc Grade Count:811
Overview of materials for Nylon 66, 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. ..
Density 1.15 - 1.82 g/cc
0.0415 - 0.0658 lb/in³
Average value: 1.46 g/cc Grade Count:172
Overview of materials for Nylon 66, Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and ma..
Density 1.80 - 1.82 g/cc
0.0650 - 0.0658 lb/in³
ISO 1183
Solvay Specialty Polymers Solef® 60512/0550 and 60512/0150 Polyvinylidene Fluoride (PVDF)
Solef® 60512/0550 and Solef® 60512/0150 are PVDF grades compounded with PTFE for extrusion of anti-wear tapes.Features: CopolymerUses: TapeAdditional Properties: Crystallization Heat - ASTM D3..
Density 1.78 - 1.82 g/cc
0.0643 - 0.0658 lb/in³
ISO R 1183
Fainplast Compounds CR 0118 Flexible PVC, Electrical Bedding
Easy strip bedding
Density 1.62 - 1.82 g/cc
0.0585 - 0.0658 lb/in³
Molded
Bulk Molding Compounds BMC T60-6002A-WG Wear Resistant Molding Compound
BMC T60-6002A-WG is a wear resistant molding compound specifically formulated for applications that require excellent abrasion resistance. Due to its low specific gravity it has substantial cost pe..
Density 1.62 - 1.82 g/cc
0.0585 - 0.0658 lb/in³
Molded
Bulk Molding Compounds BMC T60-6002-WG(15) Wear Resistant Molding Compound
BMC T60-6002-WG-(15) is a wear resistant molding compound specifically formulated for applications that require excellent abrasion resistance. Due to its low specific gravity it has substantial cos..
Density 1.70 - 1.82 g/cc
0.0614 - 0.0658 lb/in³
Molding; IS 867-1963
Amity Thermosets ATO 1510 Phenolic Molding Glass fiber Filler, Compression Molded
Characteristics:Shock resistantElectrical low lossHigh mechanical strengthHeat stableHigh electrical insulationDimensional stabilityGood mechanical tension bearing strengthMedium copper adhesionColo..
Density 1.49 - 1.82 g/cc
0.0538 - 0.0658 lb/in³
Average value: 1.63 g/cc Grade Count:38
Overview of materials for Acetal Copolymer + Glass/PTFE
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer + Glass/PTFE". Each property range of values reported is minimum and maximum values of ..
Copyright © lookpolymers.com All Rights Reserved