| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.30 - 1.90 g/cc | 0.0470 - 0.0686 lb/in³ | Average value: 1.44 g/cc Grade Count:196 |
|
Overview of materials for Polyetheretherketone, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Carbon Fiber Filled". Each property range of values reported is minimum and maximu..
|
|||
| Density | 1.70 - 1.90 g/cc | 0.0614 - 0.0686 lb/in³ | Average value: 1.78 g/cc Grade Count:6 |
|
Overview of materials for Phenolic, Resole, Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Resole, Glass Fiber Filled". Each property range of values reported is minimum and maximum val..
|
|||
| Density | 1.75 - 1.90 g/cc | 0.0632 - 0.0686 lb/in³ | Compounded |
|
Polyphosphazene Rubber (PZ, FZ)
FZ refers to the fluorinated (55 wt%) polymer.
|
|||
| Density | 1.70 - 1.90 g/cc | 0.0614 - 0.0686 lb/in³ | theoretical |
|
Gwent Electronic Materials P2121112P11 Oxygen Plasma Modified Multiwalled Carbon Nanotubes
Production Method: CVDColor: BlackTrial product which has not yet been extensively tested.Information provided by Gwent Electronic Materials Ltd.
|
|||
| Density | 1.70 - 1.90 g/cc | 0.0614 - 0.0686 lb/in³ | theoretical |
|
Gwent Electronic Materials P2121112P12 Acid Vapor Plasma Modified Single and Double Walled Carbon Nanotubes
Production Method: CVDColor: BlackSome free amorphous carbon was detected.Trial product which has not yet been extensively tested.Information provided by Gwent Electronic Materials Ltd.
|
|||
| Density | 1.70 - 1.90 g/cc | 0.0614 - 0.0686 lb/in³ | theoretical |
|
Gwent Electronic Materials P2121112P13 Argon Plasma Modified Single and Double Walled Carbon Nanotubes
Production Method: CVDColor: BlackSome free amorphous carbon was detected.Trial product which has not yet been extensively tested.Information provided by Gwent Electronic Materials Ltd.
|
|||
| Density | 1.70 - 1.90 g/cc | 0.0614 - 0.0686 lb/in³ | theoretical |
|
Gwent Electronic Materials P2121112P14 Nitrogen Plasma Modified Single and Double Walled Carbon Nanotubes
Production Method: CVDColor: BlackSome free amorphous carbon was detected.Trial product which has not yet been extensively tested.Information provided by Gwent Electronic Materials Ltd.
|
|||
| Density | 1.70 - 1.90 g/cc | 0.0614 - 0.0686 lb/in³ | theoretical |
|
Gwent Electronic Materials P2121112P15 Ammonia Plasma Modified Single and Double Walled Carbon Nanotubes
Production Method: CVDColor: BlackSome free amorphous carbon was detected.Trial product which has not yet been extensively tested.Information provided by Gwent Electronic Materials Ltd.
|
|||
| Density | 1.70 - 1.90 g/cc | 0.0614 - 0.0686 lb/in³ | theoretical |
|
Gwent Electronic Materials P2121112P16 Oxygen Plasma Modified Single and Double Walled Carbon Nanotubes
Production Method: CVDColor: BlackSome free amorphous carbon was detected.Trial product which has not yet been extensively tested.Information provided by Gwent Electronic Materials Ltd.
|
|||
| Density | 1.70 - 1.90 g/cc | 0.0614 - 0.0686 lb/in³ | theoretical |
|
Gwent Electronic Materials P2121112P18 Nitrogen Plasma Modified Multiwalled Carbon Nanotubes
Production Method: CVDColor: BlackTrial product which has not yet been extensively tested.Information provided by Gwent Electronic Materials Ltd.
|
|||
| Density | 1.70 - 1.90 g/cc | 0.0614 - 0.0686 lb/in³ | theoretical |
|
Gwent Electronic Materials P2121112P19 Tetrafluoromethane Plasma modified Single and Double Walled Carbon Nanotubes
Production Method: CVDColor: BlackSome free amorphous carbon was detected.Trial product which has not yet been extensively tested.Information provided by Gwent Electronic Materials Ltd.
|
|||
| Density | 1.70 - 1.90 g/cc | 0.0614 - 0.0686 lb/in³ | theoretical |
|
Gwent Electronic Materials P2121112P7 Acid Vapor Plasma Modified Multiwalled Carbon Nanotubes
Production Method: CVDColor: BlackTrial product which has not yet been extensively tested.Information provided by Gwent Electronic Materials Ltd.
|
|||
| Density | 1.70 - 1.90 g/cc | 0.0614 - 0.0686 lb/in³ | theoretical |
|
Gwent Electronic Materials P2121112P8 Argon Plasma Modified Multiwalled Carbon Nanotubes
Production Method: CVDColor: BlackTrial product which has not yet been extensively tested.Information provided by Gwent Electronic Materials Ltd.
|
|||
| Density | 1.70 - 1.90 g/cc | 0.0614 - 0.0686 lb/in³ | theoretical |
|
Gwent Electronic Materials P2121112P9 Tetrafluoromethane Plasma Modified Multiwalled Carbon Nanotubes
Production Method: CVDColor: BlackTrial product which has not yet been extensively tested.Information provided by Gwent Electronic Materials Ltd.
|
|||
| Density | 1.70 - 1.90 g/cc | 0.0614 - 0.0686 lb/in³ | theoretical |
|
Gwent Electronic Materials P2121112P10 Ammonia Plasma Modified Multiwalled Carbon Nanotubes
Production Method: CVDColor: BlackTrial product which has not yet been extensively tested.Information provided by Gwent Electronic Materials Ltd.
|
|||
| Density | 1.80 - 1.90 g/cc | 0.0650 - 0.0686 lb/in³ | |
|
Aremco Ceramabond™ 618-N High Temperature Ceramic Adhesive/Paste, Silica Filled
Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and..
|
|||
| Density | 1.80 - 1.90 g/cc | 0.0650 - 0.0686 lb/in³ | Molded |
|
Bulk Molding Compounds BMC T12-17394 General Purpose Molding Compound
BMC T12-17394 is a general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T12 is well suited for injection, transfer or compression molding of intricate parts. ..
|
|||
| Density | 1.70 - 1.90 g/cc | 0.0614 - 0.0686 lb/in³ | ISO 1138 |
|
Bulk Molding Compounds tetra-DUR L 4305 Bulk Molding Compound
UL-licensed. Anchor wave-isolation.Typical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipation (explosion prote..
|
|||
| Density | 1.70 - 1.90 g/cc | 0.0614 - 0.0686 lb/in³ | Molding; IS 867-1963 |
|
Amity Thermosets ATS 157 Phenolic Molding Long glass fiber Filler, Compression Molded
Characteristics:Shock resistant ( High impact strength )Very good mechanical strengthGood dielectric strengthLow water absorptionLow shrinkageColor-pale brown, black, dark brown, green etc.Medium/st..
|
|||
| Density | 1.70 - 1.90 g/cc | 0.0614 - 0.0686 lb/in³ | Molded |
|
Bulk Molding Compounds BMC A20-(a) High Strength Grade Molding Compound
BMC A20 is a high strength, low shrink general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC A20 is well suited for injection, transfer or compression molding o..
|
|||
| Density | 1.80 - 1.90 g/cc | 0.0650 - 0.0686 lb/in³ | Molded |
|
Bulk Molding Compounds BMC T12(18) General Purpose Molding Compound
BMC T12(18) is a general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T12 is well suited for injection, transfer or compression molding of intricate parts. Ty..
|
|||
| Density | 1.80 - 1.90 g/cc | 0.0650 - 0.0686 lb/in³ | |
|
Pyrotek Pyromat TS-045 Electrical Insulating Board
Pyromat TS-045 is a black laminate, press molded from high-temperature thermoset resin and reinforced with glass filament mat. Its composition ensures excellent chemically resistance and antistatic..
|
|||
| Density | 0.850 - 1.90 g/cc | 0.0307 - 0.0686 lb/in³ | Average value: 1.09 g/cc Grade Count:250 |
|
Overview of materials for Polypropylene, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Flame Retardant". Each property range of values reported is minimum and maximum values of..
|
|||
| Density | 1.45 - 1.90 g/cc | 0.0524 - 0.0686 lb/in³ | Average value: 1.57 g/cc Grade Count:17 |
|
Overview of materials for Polyphthalamide (PPA), Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Mineral Filled". Each property range of values reported is minimum and maximum values o..
|
|||
| Density | 1.80 - 1.90 g/cc | 0.0650 - 0.0686 lb/in³ | Molded |
|
Bulk Molding Compounds BMC T40-4020-AQ High Strength Arc Quenching Molding Compound
BMC T40-4020-AQ was formulated as a high strength arc quenching material for electrical applications. Typical applications are arc hoods and electrical contactors.Information provided by Bulk Moldi..
|
|||
| Density | 1.80 - 1.90 g/cc | 0.0650 - 0.0686 lb/in³ | ISO 1138 |
|
Bulk Molding Compounds tetra-DUR F 4206 Bulk Molding Compound
General purpose productTypical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipation (explosion protection), ther..
|
|||