| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 2.17 g/cc | 0.0784 lb/in³ | ISO 1183 |
|
Polykemi AB POLYfill PPH BF4075 VT1 Polypropylene Homopolymer, Reinforced, Heat Resistant
Information provided by Polykemi AB
|
|||
| Density | 2.17 g/cc | 0.0784 lb/in³ | ASTM D792 |
|
Solvay Specialty Polymers Algoflon® S 111 PTFE (Polytetrafluoroethylene)
(discontinued **)
Data provided by the manufacturer.Type IV.G.1 Classification. Suspension polymer powder grade recommended for compression molding and extrusion. PTFE possesses high inertness, excellent dielectric p..
|
|||
| Density | 2.17 g/cc | 0.0784 lb/in³ | ASTM D792 |
|
Solvay Specialty Polymers Algoflon® S 131 PTFE (Polytetrafluoroethylene)
(discontinued **)
Data provided by the manufacturer.Type IV.G.2 Classification. Suspension polymer powder grade recommended for compression molding and extrusion. PTFE possesses high inertness, excellent dielectric p..
|
|||
| Density | 2.17 g/cc | 0.0784 lb/in³ | |
|
Materion AlBeCastâ„¢ IC910 Aluminum Beryllium Composite
Mechanical properties are typical values at RT. AlBeCastâ„¢ IC910 is an aluminum-beryllium alloy that combines the advantages of a net shape casting technology, investment casting, with the stif..
|
|||
| Density | 2.17 g/cc | 0.0784 lb/in³ | ASTM 1457-62 T |
|
Fluorseals PTFE 15% graphite filled
Improved thermal conductivity and coefficient of friction.Information provided by TEKU GmbH Fluorkunststoffe, a distributor of Fluorseals materials.
|
|||
| Density | 2.17 g/cc | 0.0784 lb/in³ | |
|
Schott WG225 Long Pass Filter
Base glass. Data provided by the manufacturer, Schott Glas Mainz.Similar glasses include GG395, GG400, GG420, GG435, GG455, GG475, GG495, OG515, OG530, OG550, OG570, OG590, RG610, RG630, RG645, RG66..
|
|||
| Density |
2.17
g/cc @Temperature 25.0 °C |
0.0784
lb/in³ @Temperature 77.0 °F |
|
|
Schott Glass 8229 Intermediate sealing glass
Used for sealing to Glass 8228 and Glass 8230 The heavy metal content for the elements lead, cadmium, mercury, and hexavalent chromium is below 100 ppmInformation provided by SCHOTT AG.
|
|||
| Density | 2.17 g/cc | 0.0784 lb/in³ | ASTM D792 |
|
Solvay Specialty Polymers Algoflon® F 5 Polytetrafluoroethylene (PTFE)
Algoflon® F 5 is a fine cut homopolymer PTFE powder that is white, granular and non-free flowing. It is designed for filled grades and in particular is recommended for compounds with glass fiber ..
|
|||
| Density | 2.17 g/cc | 0.0784 lb/in³ | ASTM D792 |
|
Solvay Specialty Polymers Algoflon® F 7 Polytetrafluoroethylene (PTFE)
Algoflon® F 7 is a fine cut homopolymer PTFE powder that is white, granular and non-free flowing. It is designed for normal compression molding and in particular molding of large billets for low ..
|
|||
| Density | 2.17 g/cc | 0.0784 lb/in³ | ASTM D792 |
|
SABIC Innovative Plastics LNP THERMOCOMP 2X00858 FP-F (FEP)
LNP* THERMOCOMP* 2X00858 is a compound based on FEP resin containing proprietary fillers.
|
|||
| Density | 2.17 g/cc | 0.0784 lb/in³ | DIN EN ISO 12086 |
|
3M Dyneon™ TF 2073Z PTFE Fine Powder
Dyneon™ TF 2073 Z PTFE is an ideal grade for the manufacture of high quality micro tubing as well as wire and cable insulations. This product is also ideal for very thin-wall, smallest diameter tub..
|
|||
| Density | 2.17 g/cc | 0.0784 lb/in³ | DIN EN ISO 12086 |
|
3M Dyneon™ TF 2072Z PTFE Fine Powder
Dyneon™ TF 2072 Z PTFE is an ideal grade for thin-wall, small diameter tubing and wire and cable insulations, processed by paste extrusion method at reduction ratio up to 3000:1. This product offer..
|
|||
| Density | 2.17 g/cc | 0.0784 lb/in³ | ASTM D792 |
|
Solvay Specialty Polymers Algoflon® A.30 PTFE (Polytetrafluoroethylene)
(discontinued **)
Data provided by the manufacturer.Type IV.G.2 (except elongation at break) Classification. Suspension polymer powder grade recommended for compression molding and extrusion. PTFE possesses high iner..
|
|||
| Density | 2.17 g/cc | 0.0784 lb/in³ | ASTM D792 |
|
Solvay Specialty Polymers Algoflon® A.15 PTFE (Polytetrafluoroethylene)
(discontinued **)
Data provided by the manufacturer.Type IV.G.1 Classification. Suspension polymer powder grade recommended for compression molding and extrusion. PTFE possesses high inertness, excellent dielectric p..
|
|||
| Density | 2.17 g/cc | 0.0784 lb/in³ | ASTM D792 |
|
Solvay Specialty Polymers Algoflon® A.27 PTFE (Polytetrafluoroethylene)
(discontinued **)
Data provided by the manufacturer.Type IV.G.2 (except elongation at break) Classification. Suspension polymer powder grade recommended for compression molding and extrusion. PTFE possesses high iner..
|
|||
| Density | 2.17 g/cc | 0.0784 lb/in³ | ASTM D792 |
|
Solvay Specialty Polymers Algoflon® S 121 PTFE (Polytetrafluoroethylene)
(discontinued **)
Data provided by the manufacturer.Type IV.G.1 Classification. Suspension polymer powder grade recommended for compression molding and extrusion. PTFE possesses high inertness, excellent dielectric p..
|
|||
| Density | 2.17 g/cc | 0.0784 lb/in³ | ASTM D792 |
|
Solvay Specialty Polymers Algoflon® 15GR PTFE; Graphite Filled
(discontinued **)
Data provided by the manufacturer.15 wt.% Graphite. Suspension polymer powder grade recommended for compression molding. Pure PTFE possesses high inertness, excellent dielectric properties, almost n..
|
|||
| Density | 2.17 g/cc | 0.0784 lb/in³ | ASTM D792 |
|
Solvay Specialty Polymers Algoflon® 0.1 Mos PTFE; Molybdenum Disulfide Filled
(discontinued **)
Data provided by the manufacturer.0.1 wt.% Molybdenum Disulfide. Suspension polymer powder grade recommended for compression molding. Pure PTFE possesses high inertness, excellent dielectric propert..
|
|||
| Density | 2.17 g/cc | 0.0784 lb/in³ | |
|
Mateck Sodium Chloride (NaCl)
Optical crystals
|
|||