| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 2.70 g/cc | 0.0975 lb/in³ | |
|
Mykroy/Mycalex MM 500 Machining Grade Glass-bonded Mica Composite
Synthetic mica filler. Does not burn. Better radiation resistance (3 x 10^10 Rads-Cobalt) than grade 400.This ceramoplastic material is a versatile and efficient insulating material designed to me..
|
|||
| Density | 2.70 g/cc | 0.0975 lb/in³ | Green Density |
|
Nabaltec NABALOX® NO 625-30 Reactive Alumina
NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula..
|
|||
| Density | 2.70 g/cc | 0.0975 lb/in³ | Green Density |
|
Nabaltec NABALOX® NO 625-31 Reactive Alumina
NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula..
|
|||
| Density | 2.70 g/cc | 0.0975 lb/in³ | |
|
Rogers Corporation RO3206 Woven-Glass Reinforced PTFE Laminate
Features and Benefits:Woven glass reinforcement - Improves rigidity for easier handlingUniform electrical and mechanical performance - ideal for complex multi-layer high frequency structuresLow diel..
|
|||
| Density | 2.70 g/cc | 0.0975 lb/in³ | ASTM D792 |
|
Rogers Corporation RT/duroid® 6006 Ceramic-PTFE Composite Microwave Laminate
Features:High dielectric constant for circuit size reductionLow loss - Ideal for operating at X-band or belowTight dielectric constant and thickness control for repeatable circuit performanceLow moi..
|
|||
| Density | 2.70 g/cc | 0.0975 lb/in³ | |
|
Ferro EG 2410 Specialty Glass
Glass Type: Si-MG-Al Typical Powder Form: MVG Typical Application: Sintering Aid / Glaze Ferro offers a wide range of compositions for specialty applications including sintering aids used in the gl..
|
|||
| Density | 2.70 g/cc | 0.0975 lb/in³ | Apparent |
|
Gouda Vuurvast AK 80 A Dense Refractory Brick
Description: A 78% alumina, bauxite based, quality with a high abrasion resistance, therefore very well suitable for rotary cement kilns.Remarks: This data represents average values, obtained from s..
|
|||
| Density | 2.70 g/cc | 0.0975 lb/in³ | Apparent |
|
Gouda Vuurvast AK 80 FM Dense Refractory Brick
Description: This fused mullite based brick has a very good thermal shock resistance and an excellent resistance against liquid slags at high temperature.Remarks: This data represents average values..
|
|||
| Density | 2.70 g/cc | 0.0975 lb/in³ | |
|
Schott S8802 Contrast Enhancement Filter
Contrast Enhancement FilterInformation Provided by SCHOTT North America, Inc.
|
|||
| Density | 2.70 g/cc | 0.0975 lb/in³ | ASTM D792 |
|
SABIC Innovative Plastics LNP THERMOCOMP WH0270B PBT
LNP THERMOCOMP* WH0270B is a compound based on Polybutylene Terephalate resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity.
|
|||
| Density | 2.70 g/cc | 0.0975 lb/in³ | ASTM D792 |
|
SABIC Innovative Plastics LNP THERMOCOMP WH0270B PBT (Asia Pacific)
LNP THERMOCOMP* WH0270B is a compound based on Polybutylene Terephalate resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity.
|
|||
| Density | 2.70 g/cc | 0.0975 lb/in³ | ISO 1183 |
|
SABIC Innovative Plastics LNP THERMOCOMP WH0270B PBT (Asia Pacific)
LNP THERMOCOMP* WH0270B is a compound based on Polybutylene Terephalate resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity.
|
|||
| Density | 2.70 g/cc | 0.0975 lb/in³ | |
|
Sapco C 221 Steatite
Information provided by Sapco.
|
|||
| Density | 2.70 g/cc | 0.0975 lb/in³ | |
|
Toho Tenax Besfight® MC Type I (12,000 Filament) Nickel Coated Carbon Fiber
Besfight MC Polyacrylonitrile (PAN) based fiber combines the mechanical properties and flexibility of carbon fiber with the electrical conductivity of nickel. It does not delaminate even at the mec..
|
|||
| Density | 2.70 g/cc | 0.0975 lb/in³ | |
|
Toho Tenax Besfight® MC Type I (6000 Filament) Nickel Coated Carbon Fiber
Besfight MC Polyacrylonitrile (PAN) based fiber combines the mechanical properties and flexibility of carbon fiber with the electrical conductivity of nickel. It does not delaminate even at the mec..
|
|||
| Density | 2.70 g/cc | 0.0975 lb/in³ | |
|
Goodfellow Aluminum 99/Silicon 1 Alloy
An addition of 1% Silicon lowers the melting range without producing brittleness. Aluminum/Silicon alloys are used in brazing alloys and welding wire for joining Aluminum as well as bonding wire in ..
|
|||
| Density | 2.70 g/cc | 0.0975 lb/in³ | |
|
Constellium PLAN 6061 Aluminum Rolled Plate
Rolled plates in 6061 PLAN are optimized for minimum residual stress and improved dimensional tolerances. 6061 PLAN is mainly used for medium stressed mechanical components, manufactured by intensiv..
|
|||
| Density | 2.70 g/cc | 0.0975 lb/in³ | |
|
Constellium PLAN 6082 Aluminum Rolled Plate
Rolled plates in 6082 PLAN are optimized for minimum residual stress and improved dimensional tolerances. 6082 PLAN is mainly used for medium stressed mechanical components, manufactured by intensiv..
|
|||
| Density | 2.70 g/cc | 0.0975 lb/in³ | |
|
Constellium Planoxal® 60 Aluminum plate
The advantage of Planoxal®-60 plates over other standard EN AW-6082 alloy products is their low level of internal stress. They are also suitable for technical anodizing. Planoxal®-60 is mainly use..
|
|||
| Density | 2.70 g/cc | 0.0975 lb/in³ | |
|
Du-Co Ceramics CS-144-L-5 Steatite
Properties reported below are averages from unglazed specimens. Tests performed to ASTM specifications. Actual values may vary. Information provided by DU-CO Ceramics Company.
|
|||
| Density | 2.70 g/cc | 0.0975 lb/in³ | |
|
Constellium ALPLAN® 6082 Rolled Precision Aluminum Plate, Milled Both Sides
Precision plates in ALPLAN® 6082 are milled on both sides and have a very low level of residual stress, thus avoiding excessive deformation during machining. Thanks to its very good dimensional sta..
|
|||
| Density | 2.70 g/cc | 0.0975 lb/in³ | Cured |
|
Chesterton ARC MXC Castable Extreme Wear Compound
Description: An advanced ceramic composite, with flowable viscosity, for the repair and protection of all metal surfaces subjected to severe erosion, abrasion and chemical attack. It can be hand tro..
|
|||
| Density | 2.70 g/cc | 0.0975 lb/in³ | |
|
3M Nextel™ AF-10 Industrial Woven Fabric 312
Information provided by 3M
|
|||
| Density | 2.70 g/cc | 0.0975 lb/in³ | Alloy 1100 Property (Annealed) |
|
Arlon 90B32R016AC Aluminum Clad Press Pad with "C-Finish"
Design/Construction:Side 2: Alloy 1100 Aluminum FoilSide 1: Cured Silicone RubberThis data represents typical values for the production material and should not be used as material specifications.I..
|
|||
| Density | 2.70 g/cc | 0.0975 lb/in³ | Alloy 1100 Property (Annealed) |
|
Arlon 91B32R016AC Aluminum Clad Silicone Press Pad with "C-finish"
Design/Construction:Side 2: Alloy 1100 H18 Aluminum FoilSide 1: Cured Silicone RubberThis data represents typical values for the production material and should not be used as material specificatio..
|
|||
| Density | 2.70 g/cc | 0.0975 lb/in³ | |
|
ALIMEX 6082 T651 Aluminum Alloy Rolled
Rolled aluminium material according to DIN EN standard. Information provided by ALIMEX GmbHSolution heat treated, stress relieved by stretching a controlled amount and then artificially aged.
|
|||
| Density | 2.70 g/cc | 0.0975 lb/in³ | |
|
3M Nextel™ AF-11 Aerospace Woven Fabric 312
Information provided by 3M
|
|||
| Density | 2.70 g/cc | 0.0975 lb/in³ | |
|
3M Nextel™ AF-11 Industrial Woven Fabric 312
Information provided by 3M
|
|||
| Density | 2.70 g/cc | 0.0975 lb/in³ | |
|
3M Nextel™ AF-11 w/o sizing Aerospace Woven Fabric 312
Information provided by 3M
|
|||
| Density | 2.70 g/cc | 0.0975 lb/in³ | |
|
3M Nextel™ AF-12 w/o sizing Aerospace Woven Fabric 312
Information provided by 3M
|
|||