Polymer Property : Density = 2.84 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Density 2.84 g/cc
0.103 lb/in³
Constellium Alumold® 350 Aluminum
Alumold-350® has been specifically developed to achieve the best combination of strength at low and high temperatures, together with a good shape stability and machinability. Alumold-350® is parti..
Density 2.84 g/cc
0.103 lb/in³
Arlon AR1000 Glass, PTFE and Micro-Dispersed Ceramic
Used in the RF and microwave industries.Information provided by Arlon Materials for Electronics (MED).
Density 2.84 g/cc
0.103 lb/in³
Aleris Weldural Aluminum Alloy, 400 mm Thickness
Sample treatment not specified for property data.Applications include precise mechanical parts with high dimensional stability, machine components, molds, and refrigeration engineering. Good weldab..
Density 2.84 g/cc
0.103 lb/in³
Aleris Weldural Aluminum Alloy, 600 mm Thickness
Sample treatment not specified for property data.Applications include precise mechanical parts with high dimensional stability, machine components, molds, and refrigeration engineering. Good weldab..
Density 2.84 g/cc
0.103 lb/in³
Aleris Weldural Aluminum Alloy, 100 mm Thickness
Sample treatment not specified for property data.Applications include precise mechanical parts with high dimensional stability, machine components, molds, and refrigeration engineering. Good weldab..
Density 2.84 g/cc
0.103 lb/in³
Aleris Weldural Aluminum Alloy, 200 mm Thickness
Sample treatment not specified for property data.Applications include precise mechanical parts with high dimensional stability, machine components, molds, and refrigeration engineering. Good weldab..
Density 2.84 g/cc
0.103 lb/in³
Aleris Weldural Aluminum Alloy, 300 mm Thickness
Sample treatment not specified for property data.Applications include precise mechanical parts with high dimensional stability, machine components, molds, and refrigeration engineering. Good weldab..
Density 2.84 g/cc
0.103 lb/in³
Aleris Weldural Aluminum Alloy, 500 mm Thickness
Sample treatment not specified for property data.Applications include precise mechanical parts with high dimensional stability, machine components, molds, and refrigeration engineering. Good weldab..
Density 2.84 g/cc
0.103 lb/in³
Aleris Weldural Aluminum Alloy, 700 mm Thickness
Sample treatment not specified for property data.Applications include precise mechanical parts with high dimensional stability, machine components, molds, and refrigeration engineering. Good weldab..