| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 2.85 g/cc | 0.103 lb/in³ | Apparent |
|
Gouda Vuurvast AK 85 P1 Dense Refractory Brick
Description: A phosphate bonded bauxite brick with outstanding erosion resistance and resistance against liquid aluminum. In order to optimized the resistance against aluminum attack the sum of Al2O..
|
|||
| Density | 2.85 g/cc | 0.103 lb/in³ | Apparent |
|
Gouda Vuurvast LP 80 A Dense Refractory Brick
Description: LP 80 is a low porosity brick based on sintered bauxite with an extremely high abrasion resistance and therefore very well suited for application in rotary cement furnaces.Remarks: This..
|
|||
| Density | 2.85 g/cc | 0.103 lb/in³ | |
|
Momentive Performance Materials BNC2 Boron Nitride (BN) Refractory Composite
Boron Nitride is a unique engineering material. It is a soft, machinable ceramic which can be combined with other refractory ceramics including Aluminum Oxide, Silicon Nitride, Aluminum Nitride, Mu..
|
|||
| Density | 2.85 g/cc | 0.103 lb/in³ | |
|
Kaiser 7068 T6, T651 Rod & Bar
Alloy 7068 offers some of the highest strength mechanical properties available in an extruded product. Intended for aerospace, ordnance and light weight recreational applications where extremely hig..
|
|||
| Density | 2.85 g/cc | 0.103 lb/in³ | |
|
Kaiser 7068 T6, T6511 Rod & Bar
Alloy 7068 offers some of the highest strength mechanical properties available in an extruded product. Intended for aerospace, ordnance and light weight recreational applications where extremely hig..
|
|||
| Density | 2.85 g/cc | 0.103 lb/in³ | |
|
Kaiser 7068 T76, T76511 Rod & Bar
Alloy 7068 offers some of the highest strength mechanical properties available in an extruded product. Intended for aerospace, ordnance and light weight recreational applications where extremely hig..
|
|||
| Density | 2.85 g/cc | 0.103 lb/in³ | Apparent |
|
Gouda Vuurvast AK 85 M Dense Refractory Brick
Description: A bauxite based brick with a mullite bond. Application: torpedo ladles, electric arc furnace roofs, cement kilns.Remarks: This data represents average values, obtained from samples that..
|
|||
| Density | 2.85 g/cc | 0.103 lb/in³ | Apparent |
|
Gouda Vuurvast AK 85 PW Dense Refractory Brick
Description: A phosphate bonded bauxite brick with outstanding erosion resistance and resistance against liquid aluminum. Application: aluminum holding furnaces.Remarks: This data represents average..
|
|||
| Density | 2.85 g/cc | 0.103 lb/in³ | |
|
Schott UG5 Band Pass Filter
Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz.
|
|||
| Density | 2.85 g/cc | 0.103 lb/in³ | |
|
Goodfellow Aluminum-Copper/SiC Metal Matrix Composite
Information provided by Goodfellow.
|
|||
| Density | 2.85 g/cc | 0.103 lb/in³ | |
|
Alcoa QC-10® Aluminum Mold Alloy
Specifically designed for high production injection and blow mold applications, QC-10 offers outstanding strength, stability, and durability. Its improved alloy composition provides outstanding, 1"-..
|
|||