| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 3.25 g/cc | 0.117 lb/in³ | ISO 1183 |
|
LATI LATAMID 12 H FE85 Nylon 12 Base Magnetizable Compound
(discontinued **)
Description: These are compounds containing a high percentage of magnetizable fillers; compared to traditional techniques for the manufacture of magnets, this allows the molding of complex shapes us..
|
|||
| Density | 3.25 g/cc | 0.117 lb/in³ | ISO 1183 |
|
LATI LATAMID 12 H FE90 Nylon 12 Base Magnetizable Compound
(Unverified Data**)
Description: These are compounds containing a high percentage of magnetizable fillers; compared to traditional techniques for the manufacture of magnets, this allows the molding of complex shapes us..
|
|||
| Density | >= 3.25 g/cc | >= 0.117 lb/in³ | |
|
MarkeTech AN 120 Aluminum Nitride Ceramic Substrate, 98% Purity
Data provided by the supplier, MarkeTech International.Substrate Specs: Maximum dimensions 5.5 x 3.6 in. Thickness 0.12-0.60 in. Surface roughness 0.3 µm as fired; 0.075 µm lapped; 0.025 µ..
|
|||
| Density | >= 3.25 g/cc | >= 0.117 lb/in³ | |
|
MarkeTech AN 160 Aluminum Nitride Ceramic Substrate, 99% Purity
Data provided by the supplier, MarkeTech International.Substrate Specs: Maximum dimensions 5.5 x 3.6 in. Thickness 0.12-0.60 in. Surface roughness 0.3 µm as fired; 0.075 µm lapped; 0.025 µ..
|
|||
| Density | 3.25 - 3.35 g/cc | 0.117 - 0.121 lb/in³ | molded; ASTM D792 |
|
Guarniflon PTFE G420 Polytetrafluoroethylene 50% Steel
PTFE G Special Compound with steelInformation provided by Guarniflon®
|
|||
| Density | 3.25 g/cc | 0.117 lb/in³ | |
|
Ferro EG 2927 Metal Sealing
Glass Type: Sr-B-Al Typical Powder Form: VSD Typical Application: Comp. - Battery Ferro Metal Sealing glasses are formulated for sealing a wide range of metal packages and parts, including matched ..
|
|||
| Density | 3.25 g/cc | 0.117 lb/in³ | Apparent |
|
Gouda Vuurvast AK 99 Dense Refractory Brick
Description: This high purity alumina based brick finds wide application in chemical reactors. The low percentages of SiO2 and Fe2O3 makes this brick very resistant in reducing conditions.Remarks: T..
|
|||
| Density | 3.25 g/cc | 0.117 lb/in³ | ASTM D792 |
|
Techmer ES HiFill® PA6 0325
Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforFeatures: High Specific GravityTPC# 6066102Information provided by TP Composites, Inc.
|
|||
| Density | 3.25 g/cc | 0.117 lb/in³ | DIN EN 623-2 |
|
CeramTec SL 303 Silicon Nitride, SiAION+SiC
SL 303 is a silicon nitride ceramic. Silicon nitrides are ideal for components working under mechanical loads and engine parts, even and especially at elevated temperatures. Their property profile i..
|
|||