| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 3.61 g/cc | 0.130 lb/in³ | calculated from bulk density after subtracting pore volume |
|
MarkeTech Repton 314 Mullite
Brand 314 features: Superior hot creep.REPTON setter tiles, kiln furniture, and special fixtures are lightweight, ridge, and high strength ceramics that resist distortion and spalling, even when the..
|
|||
| Density | 3.61 g/cc | 0.130 lb/in³ | |
|
Schott GG395 Long Pass Filter
Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz.Similar glasses include GG385, GG400, GG420, GG435, GG455, GG475, GG495, OG515, OG530, OG550, OG570, OG590, RG610, RG630..
|
|||