Polymer Property : Density = 3.76 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Density 3.76 - 3.80 g/cc
0.136 - 0.137 lb/in³
Sintered
Nabaltec GRANALOX® NM 9622 B Ceramic Body, Binder Free
Nabaltec offers ceramic bodies with different alumina content as free-of-binder grades. With the addition of necessary amount of water (approx. 20 %) these grades can be directly used for slip casti..
Density 3.76 g/cc
0.136 lb/in³
Ferro EG 2807 Metal Sealing
Glass Type: Zn-B-Si (devit) Typical Powder Form: VSD Typical Application: Kovar Mo, W Ferro Metal Sealing glasses are formulated for sealing a wide range of metal packages and parts, including matc..