| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 3.70 - 3.80 g/cc | 0.134 - 0.137 lb/in³ | Sintered Density |
|
Nabaltec GRANALOX® NM 9612 Ceramic Bodies
Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum ..
|
|||
| Density | 3.70 - 3.80 g/cc | 0.134 - 0.137 lb/in³ | Sintered Density |
|
Nabaltec GRANALOX® NM 9620 F Ceramic Bodies
Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum ..
|
|||
| Density | 3.76 - 3.80 g/cc | 0.136 - 0.137 lb/in³ | Sintered |
|
Nabaltec GRANALOX® NM 9622 B Ceramic Body, Binder Free
Nabaltec offers ceramic bodies with different alumina content as free-of-binder grades. With the addition of necessary amount of water (approx. 20 %) these grades can be directly used for slip casti..
|
|||
| Density | 3.75 - 3.80 g/cc | 0.135 - 0.137 lb/in³ | Sintered Density |
|
Nabaltec GRANALOX® NM 9622 Ceramic Bodies
Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum ..
|
|||
| Density | 3.75 - 3.80 g/cc | 0.135 - 0.137 lb/in³ | Sintered |
|
Nabaltec GRANALOX® NM 9634 F Ceramic Body
Nabaltec's GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum ..
|
|||
| Density | 1.10 - 3.80 g/cc | 0.0397 - 0.137 lb/in³ | Average value: 1.49 g/cc Grade Count:605 |
|
Overview of materials for Polyphthalamide (PPA)
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide". Each property range of values reported is minimum and maximum values of appropriate Ma..
|
|||
| Density | 1.19 - 3.80 g/cc | 0.0430 - 0.137 lb/in³ | Average value: 1.95 g/cc Grade Count:5 |
|
Overview of materials for Polyphthalamide (PPA), Stainless Fiber, EMI
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Stainless Fiber, EMI". Each property range of values reported is minimum and maximum va..
|
|||
| Density | 1.06 - 3.80 g/cc | 0.0383 - 0.137 lb/in³ | Average value: 1.42 g/cc Grade Count:323 |
|
Overview of materials for Silicone, Molded, Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Silicone, Molded, Glass Fiber Filled". Each property range of values reported is minimum and maximum val..
|
|||
| Density | 0.700 - 3.80 g/cc | 0.0253 - 0.137 lb/in³ | Average value: 1.31 g/cc Grade Count:923 |
|
Overview of materials for Silicone Rubber
This property data is a summary of similar materials in the MatWeb database for the category "Silicone Rubber". Each property range of values reported is minimum and maximum values of appropriate Ma..
|
|||
| Density | 1.03 - 3.80 g/cc | 0.0372 - 0.137 lb/in³ | Average value: 1.30 g/cc Grade Count:215 |
|
Overview of materials for Nylon 610
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610". Each property range of values reported is minimum and maximum values of appropriate MatWeb e..
|
|||
| Density | 0.900 - 3.80 g/cc | 0.0325 - 0.137 lb/in³ | Average value: 1.85 g/cc Grade Count:257 |
|
Overview of materials for Thermoset Fluoroelastomer
This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Fluoroelastomer". Each property range of values reported is minimum and maximum values of appr..
|
|||