| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Linear Mold Shrinkage, Transverse |
0.0090
-
0.011
cm/cm @Time 86400 sec |
0.0090
-
0.011
in/in @Time 24.0 hour |
ASTM D955 |
|
SABIC Innovative Plastics LNP LUBRICOMP DBL32 PC
LNP* Lubricomp* DBL32 is a compound based on Polycarbonate resin containing 10% Glass Beads and 15% PTFE. Added features of this material include: Internally Lubricated.
|
|||
| Linear Mold Shrinkage, Transverse |
0.0090
-
0.011
cm/cm @Time 86400 sec |
0.0090
-
0.011
in/in @Time 24.0 hour |
ASTM D955 |
|
SABIC Innovative Plastics LNP LUBRICOMP DL001 PC (Asia Pacific)
LNP* Lubricomp* DL001 is a compound based on Polycarbonate resin containing PTFE. Added features of this material include: Internally Lubricated.
|
|||
| Linear Mold Shrinkage, Transverse |
0.0090
-
0.011
cm/cm @Time 86400 sec |
0.0090
-
0.011
in/in @Time 24.0 hour |
ASTM D955 |
|
SABIC Innovative Plastics LNP LUBRICOMP DL003P PC
LNP LUBRICOMP* DL003P is a compound based on Polycarbonate resin containing 15% PTFE. Added features of this material include: Exceptional Processing, Internally Lubricated.
|
|||
| Linear Mold Shrinkage, Transverse |
0.0090
-
0.011
cm/cm @Time 86400 sec |
0.0090
-
0.011
in/in @Time 24.0 hour |
ISO 294 |
|
SABIC Innovative Plastics LNP LUBRICOMP DL003P PC (Asia Pacific)
LNP LUBRICOMP* DL003P is a compound based on Polycarbonate resin containing PTFE. Added features of this material include: Exceptional Processing.
|
|||
| Linear Mold Shrinkage, Transverse |
0.0080
-
0.011
cm/cm @Time 86400 sec |
0.0080
-
0.011
in/in @Time 24.0 hour |
ISO 294 |
|
SABIC Innovative Plastics LNP LUBRICOMP EL003 PEI
LNP LUBRICOMP* EL003 is a compound based on Polyetherimide resin containing 15% PTFE. Added features of this material include: Internally Lubricated.
|
|||
| Linear Mold Shrinkage, Transverse |
0.0080
-
0.011
cm/cm @Time 86400 sec |
0.0080
-
0.011
in/in @Time 24.0 hour |
ASTM D955 |
|
SABIC Innovative Plastics LNP LUBRICOMP EL003 PEI (Asia Pacific)
LNP LUBRICOMP* EL003 is a compound based on Polyetherimide resin containing PTFE. Added features of this material include: Internally Lubricated.
|
|||
| Linear Mold Shrinkage, Transverse |
0.0080
-
0.011
cm/cm @Time 86400 sec |
0.0080
-
0.011
in/in @Time 24.0 hour |
ISO 294 |
|
SABIC Innovative Plastics LNP LUBRICOMP EL003 PEI (Asia Pacific)
LNP LUBRICOMP* EL003 is a compound based on Polyetherimide resin containing PTFE. Added features of this material include: Internally Lubricated.
|
|||
| Linear Mold Shrinkage, Transverse |
0.0080
-
0.011
cm/cm @Time 86400 sec |
0.0080
-
0.011
in/in @Time 24.0 hour |
ASTM D955 |
|
SABIC Innovative Plastics LNP LUBRICOMP EL003 PEI (Europe-Africa-Middle East)
LNP LUBRICOMP* EL003 is a compound based on Polyetherimide resin containing PTFE. Added features of this material include: Internally Lubricated.
|
|||
| Linear Mold Shrinkage, Transverse |
0.0080
-
0.011
cm/cm @Time 86400 sec |
0.0080
-
0.011
in/in @Time 24.0 hour |
ISO 294 |
|
SABIC Innovative Plastics LNP LUBRICOMP EL003 PEI (Europe-Africa-Middle East)
LNP LUBRICOMP* EL003 is a compound based on Polyetherimide resin containing PTFE. Added features of this material include: Internally Lubricated.
|
|||
| Linear Mold Shrinkage, Transverse |
0.0080
-
0.011
cm/cm @Thickness 3.20 - 4.60 mm |
0.0080
-
0.011
in/in @Thickness 0.126 - 0.181 in |
SABIC Method |
|
SABIC Innovative Plastics Valox® 855 PBT
15% GR PBTP, UL94 V-0 rated. Improved surface appearance. For external housings: steam irons, appliance housings and lighting parts.
|
|||
| Linear Mold Shrinkage, Transverse |
0.0080
-
0.011
cm/cm @Thickness 3.20 - 4.60 mm |
0.0080
-
0.011
in/in @Thickness 0.126 - 0.181 in |
SABIC Method |
|
SABIC Innovative Plastics Valox® 855 PBT (Asia Pacific)
15% GR PBTP, UL94 V-0 rated. Improved surface appearance. For external housings: steam irons, appliance housings and lighting parts.
|
|||
| Linear Mold Shrinkage, Transverse |
0.0080
-
0.011
cm/cm @Thickness 3.20 - 4.60 mm |
0.0080
-
0.011
in/in @Thickness 0.126 - 0.181 in |
SABIC Method |
|
SABIC Innovative Plastics Valox® DR48 PBT (Asia Pacific)
17% glass reinforced, flame retardant grade UL-94 rated V-0/5VA.
|
|||
| Linear Mold Shrinkage, Transverse |
0.0080
-
0.011
cm/cm @Thickness 3.20 - 4.60 mm |
0.0080
-
0.011
in/in @Thickness 0.126 - 0.181 in |
SABIC Method |
|
SABIC Innovative Plastics Valox® DR51M PBT (Asia Pacific)
15% GR; exc. mechanical/thermal/electrical performance; nonflame retardant. For spotlights, appliance housings, handles. Easy flow/int. mold release.This data was supplied by SABIC-IP for the Asia ..
|
|||
| Linear Mold Shrinkage, Transverse |
0.0090
-
0.011
cm/cm @Time 86400 sec |
0.0090
-
0.011
in/in @Time 24.0 hour |
ASTM D955 |
|
SABIC Innovative Plastics LNP STAT-KON WE002 PBT
LNP STAT-KON* WE002 is a compound based on PBT resin containing 10% Carbon Fiber. Added features of this material include: Electrically Conductive.
|
|||
| Linear Mold Shrinkage, Transverse |
0.0090
-
0.011
cm/cm @Time 86400 sec |
0.0090
-
0.011
in/in @Time 24.0 hour |
ASTM D955 |
|
SABIC Innovative Plastics LNP STAT-KON WE002 PBT (Asia Pacific)
LNP STAT-KON* WE002 is a compound based on Polybutylene Terephalate resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.
|
|||
| Linear Mold Shrinkage, Transverse |
0.0090
-
0.011
cm/cm @Time 86400 sec |
0.0090
-
0.011
in/in @Time 24.0 hour |
ASTM D955 |
|
SABIC Innovative Plastics LNP THERMOCOMP IX04513C PA 6/12 (Asia Pacific)
LNP THERMOCOMP* IX04513C is a compound based on Nylon 6/12 resin containing Glass Fiber. Added features of this material include: Clean Compounding System.
|
|||
| Linear Mold Shrinkage, Transverse |
0.0090
-
0.011
cm/cm @Time 86400 sec |
0.0090
-
0.011
in/in @Time 24.0 hour |
ISO 294 |
|
SABIC Innovative Plastics LNP THERMOCOMP IX04513C PA 6/12 (Asia Pacific)
LNP THERMOCOMP* IX04513C is a compound based on Nylon 6/12 resin containing Glass Fiber. Added features of this material include: Clean Compounding System.
|
|||
| Linear Mold Shrinkage, Transverse |
0.0090
-
0.011
cm/cm @Time 86400 sec |
0.0090
-
0.011
in/in @Time 24.0 hour |
ASTM D 955 |
|
SABIC Innovative Plastics LNP Thermocomp OF004AER PPS
LNP* Thermocomp* OF004AER is a compound based on Polyphenylene Sulfide resin containing Glass Fiber. Added features of this material include: Easy Molding, Mold Release.This data was supplied by SA..
|
|||
| Linear Mold Shrinkage, Transverse |
0.0090
-
0.011
cm/cm @Time 86400 sec |
0.0090
-
0.011
in/in @Time 24.0 hour |
ASTM D 955 |
|
SABIC Innovative Plastics LNP Thermocomp OF004AER PPS (Asia Pacific)
LNP* Thermocomp* OF004AER is a compound based on Polyphenylene Sulfide resin containing Glass Fiber. Added features of this material include: Easy Molding, Mold Release.This data was supplied by SA..
|
|||
| Linear Mold Shrinkage, Transverse |
0.0090
-
0.011
cm/cm @Time 86400 sec |
0.0090
-
0.011
in/in @Time 24.0 hour |
ISO 294 |
|
SABIC Innovative Plastics LNP THERMOCOMP RF006EXZ PA 66
LNP THERMOCOMP* RF006EXZ is a compound based on Nylon 66 resin containing 30% Glass Fiber. Added features of this material include: Easy Molding.
|
|||
| Linear Mold Shrinkage, Transverse |
0.0090
-
0.011
cm/cm @Time 86400 sec |
0.0090
-
0.011
in/in @Time 24.0 hour |
ISO 294 |
|
SABIC Innovative Plastics LNP THERMOTUF QX01581H PA6.10
LNP THERMOTUF* QX01581H is a compound based on Nylon 6/10 resin containing Glass Fiber. Added features of this material include: High Impact.
|
|||
| Linear Mold Shrinkage, Transverse |
0.0080
-
0.011
cm/cm @Thickness 3.20 - 4.60 mm |
0.0080
-
0.011
in/in @Thickness 0.126 - 0.181 in |
SABIC Method |
|
SABIC Innovative Plastics Valox® 451E PBT
20% GR. Easy flow version of VALOX 451.
|
|||
| Linear Mold Shrinkage, Transverse |
0.0080
-
0.011
cm/cm @Thickness 3.20 - 4.60 mm |
0.0080
-
0.011
in/in @Thickness 0.126 - 0.181 in |
SABIC Method |
|
SABIC Innovative Plastics Valox® 451E PBT (Asia Pacific)
20% GR. Easy flow version of VALOX 451.
|
|||
| Linear Mold Shrinkage, Transverse |
0.0090
-
0.011
cm/cm @Time 86400 sec |
0.0090
-
0.011
in/in @Time 24.0 hour |
ASTM D 955 |
|
SABIC Innovative Plastics LNP Thermocomp MF006S PP (Asia Pacific)
LNP* Thermocomp* MF006S is a compound based on Polypropylene resin containing Glass Fiber. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for the Asia P..
|
|||
| Linear Mold Shrinkage, Transverse |
0.0090
-
0.011
cm/cm @Time 86400 sec |
0.0090
-
0.011
in/in @Time 24.0 hour |
ASTM D955 |
|
SABIC Innovative Plastics LNP THERMOCOMP MF006SU PP
LNP* THERMOCOMP* MF006SU is a compound based on Polypropylene containing 30% lass Fiber. Characteristics of this grade are: Heat Stabilized, Chemically Coupled, UV Stabilized.
|
|||
| Linear Mold Shrinkage, Transverse |
0.0090
-
0.011
cm/cm @Time 86400 sec |
0.0090
-
0.011
in/in @Time 24.0 hour |
ASTM D 955 |
|
SABIC Innovative Plastics LNP Thermocomp OF002A PPS
LNP* Thermocomp* OF002A is a compound based on Polyphenylene Sulfide resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region.
|
|||
| Linear Mold Shrinkage, Transverse |
0.0090
-
0.011
cm/cm @Time 86400 sec |
0.0090
-
0.011
in/in @Time 24.0 hour |
ASTM D955 |
|
SABIC Innovative Plastics LNP THERMOCOMP RF006ESZ PA 66
LNP THERMOCOMP* RF006ESZ is a compound based on Nylon 66 resin containing 30% Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized.
|
|||
| Linear Mold Shrinkage, Transverse |
0.0090
-
0.011
cm/cm @Time 86400 sec |
0.0090
-
0.011
in/in @Time 24.0 hour |
ASTM D955 |
|
SABIC Innovative Plastics LNP THERMOTUF QX01581H PA 6/10 (Asia Pacific)
LNP* THERMOTUF* QX01581H is a compound based on Nylon 6/10 resin containing Glass Fiber. Added features of this material include: High Impact.
|
|||
| Linear Mold Shrinkage, Transverse |
0.0090
-
0.011
cm/cm @Time 86400 sec |
0.0090
-
0.011
in/in @Time 24.0 hour |
ISO 294 |
|
SABIC Innovative Plastics LNP THERMOTUF QX01581H PA 6/10 (Asia Pacific)
LNP* THERMOTUF* QX01581H is a compound based on Nylon 6/10 resin containing Glass Fiber. Added features of this material include: High Impact.
|
|||
| Linear Mold Shrinkage, Transverse |
0.0090
-
0.011
cm/cm @Time 86400 sec |
0.0090
-
0.011
in/in @Time 24.0 hour |
ASTM D955 |
|
SABIC Innovative Plastics LNP LUBRICOMP DBL32 PC (Asia Pacific)
LNP* Lubricomp* DBL32 is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive, Internally Lubricated.
|
|||