| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Linear Mold Shrinkage, Transverse |
0.019
cm/cm <br>@Time 86400 sec
|
0.019
in/in <br>@Time 24.0 hour
|
ASTM D 955 |
|
SABIC Innovative Plastics LNP Lubricomp FX00617 PE
LNP* Lubricomp* FX00617 is a compound based on Polyethylene resin containing Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Amer..
|
|||
| Linear Mold Shrinkage, Transverse |
0.019
cm/cm <br>@Time 86400 sec
|
0.019
in/in <br>@Time 24.0 hour
|
ISO 294 |
|
SABIC Innovative Plastics LNP Lubricomp FX00617 PE
LNP* Lubricomp* FX00617 is a compound based on Polyethylene resin containing Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Amer..
|
|||
| Linear Mold Shrinkage, Transverse |
0.019
cm/cm <br>@Time 86400 sec
|
0.019
in/in <br>@Time 24.0 hour
|
ASTM D 955 |
|
SABIC Innovative Plastics LNP Lubricomp FX00617 PE (Asia Pacific)
LNP* Lubricomp* FX00617 is a compound based on Polyethylene resin containing Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Asia..
|
|||
| Linear Mold Shrinkage, Transverse |
0.019
cm/cm <br>@Time 86400 sec
|
0.019
in/in <br>@Time 24.0 hour
|
ISO 294 |
|
SABIC Innovative Plastics LNP Lubricomp FX00617 PE (Asia Pacific)
LNP* Lubricomp* FX00617 is a compound based on Polyethylene resin containing Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Asia..
|
|||
| Linear Mold Shrinkage, Transverse |
0.019
cm/cm <br>@Time 86400 sec
|
0.019
in/in <br>@Time 24.0 hour
|
ASTM D955 |
|
SABIC Innovative Plastics LNP LUBRICOMP LL004C PEEK
LNP* LUBRICOMP* LL004C is a compound based on Polyetheretherketone resin containing 20% PTFE. Added features of this material include: Wear Resistant, Clean Compounding System.
|
|||
| Linear Mold Shrinkage, Transverse |
0.019
cm/cm <br>@Time 86400 sec
|
0.019
in/in <br>@Time 24.0 hour
|
ASTM D955 |
|
SABIC Innovative Plastics LNP LUBRICOMP LL004C PEEK (Asia Pacific)
LNP* Lubricomp* LL004C is a compound based on Polyetheretherketone resin containing PTFE. Added features of this material include: Internally Lubricated, Clean Compounding System.
|
|||
| Linear Mold Shrinkage, Transverse |
0.019
cm/cm <br>@Time 86400 sec
|
0.019
in/in <br>@Time 24.0 hour
|
ASTM D955 |
|
SABIC Innovative Plastics LNP LUBRICOMP LL004E PEEK (Asia Pacific)
LNP* Lubricomp* LL004E is a compound based on Polyetheretherketone resin containing PTFE. Added features of this material include: Internally Lubricated.
|
|||
| Linear Mold Shrinkage, Transverse |
0.019
cm/cm <br>@Time 86400 sec
|
0.019
in/in <br>@Time 24.0 hour
|
ASTM D955 |
|
SABIC Innovative Plastics LNP LUBRICOMP RFL34 PA 66
LNP* LUBRICOMP* RFL34 is a compound based on Nylon 66 resin containing 20% Glass Fiber, 15% PTFE. Added feature of this material is: Wear Resistant.
|
|||
| Linear Mold Shrinkage, Transverse |
0.019
cm/cm <br>@Time 86400 sec
|
0.019
in/in <br>@Time 24.0 hour
|
ISO 294 |
|
SABIC Innovative Plastics LNP LUBRICOMP RFL34 PA 66
LNP* LUBRICOMP* RFL34 is a compound based on Nylon 66 resin containing 20% Glass Fiber, 15% PTFE. Added feature of this material is: Wear Resistant.
|
|||
| Linear Mold Shrinkage, Transverse |
0.019
cm/cm <br>@Time 86400 sec
|
0.019
in/in <br>@Time 24.0 hour
|
ASTM D955 |
|
SABIC Innovative Plastics LNP LUBRICOMP RFL34 PA 66 (Asia Pacific)
LNP* Lubricomp* RFL34 is a compound based on Nylon 66 resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.
|
|||
| Linear Mold Shrinkage, Transverse |
0.019
cm/cm <br>@Time 86400 sec
|
0.019
in/in <br>@Time 24.0 hour
|
ISO 294 |
|
SABIC Innovative Plastics LNP LUBRICOMP RFL34 PA 66 (Asia Pacific)
LNP* Lubricomp* RFL34 is a compound based on Nylon 66 resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.
|
|||
| Linear Mold Shrinkage, Transverse |
0.019
-
0.033
cm/cm <br>@Time 86400 sec
|
0.019
-
0.033
in/in <br>@Time 24.0 hour
|
ASTM D955 |
|
SABIC Innovative Plastics LNP LUBRICOMP RL004S PA 66
LNP LUBRICOMP* RL004S is a compound based on Nylon 66 resin containing 20% PTFE. Added features of this material include: Heat Stabilized, Wear Resistant.
|
|||
| Linear Mold Shrinkage, Transverse |
0.019
cm/cm <br>@Time 86400 sec
|
0.019
in/in <br>@Time 24.0 hour
|
ASTM D955 |
|
SABIC Innovative Plastics LNP LUBRICOMP RP004 PA 66 (Asia Pacific)
LNP* Lubricomp* RP004 is a compound based on Nylon 66 resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated.
|
|||
| Linear Mold Shrinkage, Transverse |
0.019
cm/cm <br>@Time 86400 sec
|
0.019
in/in <br>@Time 24.0 hour
|
ASTM D 955 |
|
SABIC Innovative Plastics LNP Lubricomp RP0049 PA 66
LNP LUBRICOMP* RP0049 is a compound based on Nylon 66 resin containing Flame Retardant, PTFE, Silicone. Added features of this material include: Flame Retardant.This data was supplied by SABIC-IP f..
|
|||
| Linear Mold Shrinkage, Transverse |
0.019
cm/cm <br>@Time 86400 sec
|
0.019
in/in <br>@Time 24.0 hour
|
ISO 294 |
|
SABIC Innovative Plastics LNP LUBRICOMP SP003 PA 12 (Asia Pacific)
LNP* Lubricomp* SP003 is a compound based on Nylon 12 resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated.
|
|||
| Linear Mold Shrinkage, Transverse |
0.019
-
0.022
cm/cm <br>@Time 86400 sec
|
0.019
-
0.022
in/in <br>@Time 24.0 hour
|
ISO 294 |
|
SABIC Innovative Plastics LNP STAT-KON FX98500 PE
LNP* STAT-KON* FX98500 is a compound based on Polyethylene resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive.
|
|||
| Linear Mold Shrinkage, Transverse |
0.019
-
0.024
cm/cm <br>@Time 86400 sec
|
0.019
-
0.024
in/in <br>@Time 24.0 hour
|
ASTM D 955 |
|
SABIC Innovative Plastics LNP Stat-loy K3000 Acetal Copoly
LNP* Stat-loy* K3000 is a compound based on Acetal Copolymer resin containing Anti-Static. Added features of this material include: Antistat.This data was supplied by SABIC-IP for the Americas regi..
|
|||
| Linear Mold Shrinkage, Transverse |
0.019
-
0.024
cm/cm <br>@Time 86400 sec
|
0.019
-
0.024
in/in <br>@Time 24.0 hour
|
ASTM D 955 |
|
SABIC Innovative Plastics LNP Stat-loy K3000 Acetal Copoly (Asia Pacific)
LNP* Stat-loy* K3000 is a compound based on Acetal Copolymer resin containing Anti-Static. Added features of this material include: Antistat.This data was supplied by SABIC-IP for the Asia Pacific ..
|
|||
| Linear Mold Shrinkage, Transverse |
0.019
-
0.024
cm/cm <br>@Time 86400 sec
|
0.019
-
0.024
in/in <br>@Time 24.0 hour
|
ISO 294 |
|
SABIC Innovative Plastics LNP Stat-loy K3000 Acetal Copoly (Asia Pacific)
LNP* Stat-loy* K3000 is a compound based on Acetal Copolymer resin containing Anti-Static. Added features of this material include: Antistat.This data was supplied by SABIC-IP for the Asia Pacific ..
|
|||
| Linear Mold Shrinkage, Transverse |
0.019
-
0.021
cm/cm <br>@Time 86400 sec
|
0.019
-
0.021
in/in <br>@Time 24.0 hour
|
ASTM D 955 |
|
SABIC Innovative Plastics LNP Thermocomp KF003 Acetal Copoly
LNP* Thermocomp* KF003 is a compound based on Acetal Copolymer resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region.
|
|||
| Linear Mold Shrinkage, Transverse |
0.019
-
0.021
cm/cm <br>@Time 86400 sec
|
0.019
-
0.021
in/in <br>@Time 24.0 hour
|
ASTM D 955 |
|
SABIC Innovative Plastics LNP Thermocomp KF003 Acetal Copoly (Asia Pacific)
LNP* Thermocomp* KF003 is a compound based on Acetal Copolymer resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region.
|
|||
| Linear Mold Shrinkage, Transverse |
0.019
-
0.021
cm/cm <br>@Time 86400 sec
|
0.019
-
0.021
in/in <br>@Time 24.0 hour
|
ASTM D955 |
|
SABIC Innovative Plastics LNP THERMOCOMP RB008 PA 66 (Asia Pacific)
LNP THERMOCOMP* RB008 is a compound based on Nylon 66 resin containing Glass Bead.
|
|||
| Linear Mold Shrinkage, Transverse |
0.019
cm/cm <br>@Time 86400 sec
|
0.019
in/in <br>@Time 24.0 hour
|
ASTM D955 |
|
SABIC Innovative Plastics LNP LUBRICOMP LL004 PEEK
LNP LUBRICOMP* LL004 is a compound based on Polyetheretherketone resin containing 20% PTFE. Added feature of this material is: Wear Resistant.
|
|||
| Linear Mold Shrinkage, Transverse |
0.019
cm/cm <br>@Time 86400 sec
|
0.019
in/in <br>@Time 24.0 hour
|
ASTM D955 |
|
SABIC Innovative Plastics LNP LUBRICOMP LL004 PEEK (Asia Pacific)
LNP LUBRICOMP* LL004 is a compound based on Polyetheretherketone resin containing PTFE. Added features of this material include: Internally Lubricated.
|
|||
| Linear Mold Shrinkage, Transverse |
0.019
cm/cm <br>@Time 86400 sec
|
0.019
in/in <br>@Time 24.0 hour
|
ASTM D955 |
|
SABIC Innovative Plastics LNP LUBRICOMP LL004 PEEK (Europe-Africa-Middle East)
LNP LUBRICOMP* LL004 is a compound based on Polyetheretherketone resin containing PTFE. Added features of this material include: Internally Lubricated.
|
|||
| Linear Mold Shrinkage, Transverse |
0.019
cm/cm <br>@Time 86400 sec
|
0.019
in/in <br>@Time 24.0 hour
|
ISO 294 |
|
SABIC Innovative Plastics LNP LUBRICOMP WBL36L PBT
LNP* LUBRICOMP* WBL36L is a compound based on PBT resin containing 30% Glass Bead, 15% PTFE. Added features of this material include: Wear Resistant, Low Extractible.
|
|||
| Linear Mold Shrinkage, Transverse |
0.019
-
0.022
cm/cm <br>@Time 86400 sec
|
0.019
-
0.022
in/in <br>@Time 24.0 hour
|
ASTM D955 |
|
SABIC Innovative Plastics LNP STAT-KON FX98500C PE
LNP* STAT-KON* FX98500C is a compound based on Polyethylene resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive.
|
|||
| Linear Mold Shrinkage, Transverse |
0.019
-
0.022
cm/cm <br>@Time 86400 sec
|
0.019
-
0.022
in/in <br>@Time 24.0 hour
|
ISO 294 |
|
SABIC Innovative Plastics LNP STAT-KON FX98500C PE
LNP* STAT-KON* FX98500C is a compound based on Polyethylene resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive.
|
|||
| Linear Mold Shrinkage, Transverse |
0.019
-
0.021
cm/cm <br>@Time 86400 sec
|
0.019
-
0.021
in/in <br>@Time 24.0 hour
|
ASTM D955 |
|
SABIC Innovative Plastics LNP THERMOCOMP RB008 PA 66
LNP THERMOCOMP* RB008 is a compound based on Nylon 66 resin containing 40% Glass Bead.
|
|||
| Linear Mold Shrinkage, Transverse |
0.019
cm/cm <br>@Thickness 2.00 mm
|
0.019
in/in <br>@Thickness 0.0787 in
|
ISO 294-4 |
|
DuPont Performance Polymers Delrin® 111P NC010 Acetal Homopolymer
Delrin® 111P is a high viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage, fewer voids). It has higher tensile strength and mod..
|
|||