| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Bulk Density | 0.580 - 0.640 g/cc | 0.0210 - 0.0231 lb/in³ | Of unexpanded product |
|
NOVA Chemicals Gedexcel® 25C Expandable Polystyrene
Styrene homopolymer containing pentane, used as a blowing agent. Production of complex and high definition preform for the "lost foam" costing technique used in foundries.Information provided by NOV..
|
|||
| Bulk Density | 0.580 - 0.640 g/cc | 0.0210 - 0.0231 lb/in³ | Of unexpanded product |
|
NOVA Chemicals Gedexcel® 35B Expandable Polystyrene
Styrene homopolymer containing pentane, used as a blowing agent. Production of complex and high definition preforms for the "lost foam" casting technique used in foundries.Information provided by NO..
|
|||
| Bulk Density | 0.580 - 0.640 g/cc | 0.0210 - 0.0231 lb/in³ | Of unexpanded product |
|
NOVA Chemicals Gedexcel® 35C Expandable Polystyrene
Styrene homopolymer containing pentane, used as a blowing agent. Production of complex and high definition preform for the "lost foam" costing technique used in foundries.Information provided by NOV..
|
|||
| Bulk Density | 0.580 - 0.640 g/cc | 0.0210 - 0.0231 lb/in³ | Of unexpanded product |
|
NOVA Chemicals Gedexcel® 44B Expandable Polystyrene
Styrene homopolymer containing pentane, used as a blowing agent. Fast molding cycle product reduced stabilization time in silo. Especially adapted to high density molding and thin thickness, and fr..
|
|||
| Bulk Density | 0.580 - 0.640 g/cc | 0.0210 - 0.0231 lb/in³ | Of unexpanded product |
|
NOVA Chemicals Gedexcel® 44XA Expandable Polystyrene
Styrene homopolymer containing pentane, used as a blowing agent with an additive improving its reaction to fire. Fast molding cycle product allowing to obtain optimum mechanical properties for form ..
|
|||
| Bulk Density | 0.580 - 0.640 g/cc | 0.0210 - 0.0231 lb/in³ | Of unexpanded product |
|
NOVA Chemicals Gedexcel® 45C Expandable Polystyrene
Styrene homopolymer containing pentane, used as a blowing agent. Production of complex and high definition preform for the "lost foam" costing technique used in foundries.Information provided by NOV..
|
|||
| Bulk Density | 0.580 - 0.640 g/cc | 0.0210 - 0.0231 lb/in³ | Of unexpanded product |
|
NOVA Chemicals Gedexcel® 45XA Expandable Polystyrene
Styrene homopolymer containing pentane, used as a blowing agent with an additive improving its reaction to fire. Fast molding cycle product allowing to obtain optimum mechanical properties for from ..
|
|||
| Bulk Density | 0.580 - 0.640 g/cc | 0.0210 - 0.0231 lb/in³ | Of unexpanded product |
|
NOVA Chemicals Gedexcel® 54B Expandable Polystyrene
Styrene homopolymer containing pentane, used as a blowing agent. Fast molding cycle product and reduced stabilization time in silo. Especially adapted to high density molding and thin thickness, an..
|
|||
| Bulk Density | 0.580 - 0.640 g/cc | 0.0210 - 0.0231 lb/in³ | Of unexpanded product |
|
NOVA Chemicals Gedexcel® 54XA Expandable Polystyrene
Styrene homopolymer containing pentane, used as a blowing agent with an additive improving its reaction to fire. Fast molding cycle product to obtain mechanical properties for form molding parts wit..
|
|||
| Bulk Density | 0.580 - 0.640 g/cc | 0.0210 - 0.0231 lb/in³ | Of unexpanded product |
|
NOVA Chemicals Gedexcel® 55B Expandable Polystyrene
Styrene homopolymer containing pentane, used as a blowing agent. Fastmolding cycle product allowing to obtain optimum mechanical properties for form molding parts with a thickness over 10 mm.Inform..
|
|||
| Bulk Density | 0.580 - 0.640 g/cc | 0.0210 - 0.0231 lb/in³ | Of unexpanded product |
|
NOVA Chemicals Gedexcel® 55C Expandable Polystyrene
Styrene homopolymer containing pentane, used as a blowing agent. Fast molding cycle product allowing to obtain optimum mechanical properties for form molding parts with a thickness over 10 mm.Infor..
|
|||
| Bulk Density | 0.580 - 0.640 g/cc | 0.0210 - 0.0231 lb/in³ | Of unexpanded product |
|
NOVA Chemicals Gedexcel® 55XA Expandable Polystyrene
Styrene homopolymer containing pentane, used as a blowing agent with an additive improving its reaction to fire. Fast molding cycle product to obtain mechanical properties for form molding parts wit..
|
|||
| Bulk Density | 0.580 - 0.640 g/cc | 0.0210 - 0.0231 lb/in³ | Of unexpanded product |
|
NOVA Chemicals Gedexcel® 65B Expandable Polystyrene
Styrene homopolymer containing pentane, used as a blowing agent. Production of average to high density blocks and molding of the shape of bulky packaging and parts for the building industry.Informat..
|
|||
| Bulk Density | 0.580 - 0.640 g/cc | 0.0210 - 0.0231 lb/in³ | Of unexpanded product |
|
NOVA Chemicals Gedexcel® 65D Expandable Polystyrene
Styrene homopolymer containing pentane, used as a blowing agent. For the production of blocks of average and low densities.Information provided by NOVA Chemicals.
|
|||
| Bulk Density | 0.580 - 0.640 g/cc | 0.0210 - 0.0231 lb/in³ | Of unexpanded product |
|
NOVA Chemicals Gedexcel® 65XA Expandable Polystyrene
Styrene homopolymer containing pentane, used as a blowing agent with an additive improving its reaction to fire. Fast molding cycle product for molding blocks of average and low densities.Informati..
|
|||
| Bulk Density | 0.580 - 0.640 g/cc | 0.0210 - 0.0231 lb/in³ | Of unexpanded product |
|
NOVA Chemicals Gedexcel® 74XA Expandable Polystyrene
Styrene homopolymer containing pentane, sued as a blowing agent with an additive improving its reaction to fire. Fast molding cycle product for molding blocks of average and low densities.Informatio..
|
|||
| Bulk Density | 0.580 - 0.640 g/cc | 0.0210 - 0.0231 lb/in³ | Of unexpanded product |
|
NOVA Chemicals Gedexcel® 76D Expandable Polystyrene
Styrene homopolymer containing pentane, used as a blowing agent. For the production of very low density blocks.Information provided by NOVA Chemicals.
|
|||
| Bulk Density | 0.580 g/cc | 0.0210 lb/in³ | |
|
NOVA Chemicals Sclair® 2714 HDPE Injection Molding Resin
Features: Excellent processability for applications requiring good stiffness and toughness, good cold temperature impact properties.Applications: Food containers and lids, frozen food containers.Dat..
|
|||
| Bulk Density | 0.580 - 0.640 g/cc | 0.0210 - 0.0231 lb/in³ | Of unexpanded product |
|
NOVA Chemicals Gedexcel® 76L Expandable Polystyrene
Styrene homopolymer containing pentane, used as a blowing agent. For the production of blocks of low density. Insulate plates with low thermal conductivity.Information provided by NOVA Chemicals.
|
|||
| Bulk Density | 0.580 - 0.640 g/cc | 0.0210 - 0.0231 lb/in³ | Of unexpanded product |
|
NOVA Chemicals Gedexcel® 76XA Expandable Polystyrene
Styrene homopolymer containing pentane, used as a blowing agent with an additive improving its reaction to fire. Production of low density blocks, recommended for the elastified plates after cutting..
|
|||
| Bulk Density | 0.580 g/cc | 0.0210 lb/in³ | ASTM D4745 |
|
3M Dyneon™ CC105 Custom Fluoropolymer Compound
(discontinued **)
This compound consists of a mixture of 25% fiberglass blended with PTFEInformation provided by Dyneon, A 3M Company
|
|||
| Bulk Density | 0.580 g/cc | 0.0210 lb/in³ | DIN-53466 |
|
Iran Petrochemical (PCC) PVC-S6058 Poly Vinyl Chloride
Grade S6058 has low porosity & very high bulk density. Therefore it is most suitable for rigid applications, high machine throughput, and specific applications as additive polymer.Applications: ex..
|
|||
| Bulk Density | 0.580 g/cc | 0.0210 lb/in³ | ISO 60 |
|
SolVin 267RC Polyvinyl Chloride Homopolymer Extrusion Grade
Polyvinyl chloride made by suspension polymerization. Uses: Sewage pipes, pressure pipes, rigid profiles, window frames, electrical ductsInformation provided by SolVin.
|
|||
| Bulk Density | 0.580 g/cc | 0.0210 lb/in³ | ASTM D1895 |
|
Sumitomo Bakelite Durez® 32962 Phenolic Molding Compound, Injection Grade
Durez 32962 Black Phenolic is a medium impact, molding compound. It is designed for applications where additional mechanical strength is required. Typical applications include appliance housings whe..
|
|||
| Bulk Density | 0.580 g/cc | 0.0210 lb/in³ | ASTM D1895 |
|
Plenco 2567 Phenolic, Granular, Injection Molded
PLENCO 02567 is a general purpose, organic filled phenolic molding compound offering excellent cosmetic characteristics as typically required for vacuum metalized closures. UL recognized under compo..
|
|||
| Bulk Density | 0.580 g/cc | 0.0210 lb/in³ | ASTM D1895 |
|
Plenco 3554 Phenolic, Granular, Compression Molded
PLENCO 03554 is an organic reinforced phenolic molding compound modified with PTFE to offer improved coefficient of friction values. 03554 is available in black. It is UL listed. 03554 is a re-numbe..
|
|||
| Bulk Density | 0.580 g/cc | 0.0210 lb/in³ | ASTM D1895 |
|
Plenco 7203 Phenolic, Granular, Transfer Molded
PLENCO 07203 is an organic fiber reinforced phenolic molding compound, offering improved mechanical strength and an industrial finish. UL recognized under component file E40654. 07203 is available i..
|
|||
| Bulk Density | 0.580 g/cc | 0.0210 lb/in³ | ISO 1183 |
|
Polyram RamClean™ 203 Purging Agent
Purging agent for blow molding machines.Information provided by Polyram.
|
|||
| Bulk Density | 0.580 g/cc | 0.0210 lb/in³ | ASTM D1895 |
|
Formosa Plastics Formolon® 622S PVC
Homopolymer Siding Grade Resin F622S is a medium-low molecular weight PVC homopolymer designed primarily for rigid extrusion applications, but it is also suitable for many flexible applications. Thi..
|
|||