| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Bulk Density | 0.608 - 0.640 g/cc | 0.0220 - 0.0231 lb/in³ | Before expansion |
|
NOVA Chemicals Dylite® F271T Specialty Expandable Polystyrene
Features: Highly consistent bead size; high gloss characteristics; low energy consumption; fast cyclingApplications: Drinking cups -hot and cold, noodle bowls, take-out and ice cream containers, and..
|
|||
| Bulk Density | 0.609 - 0.641 g/cc | 0.0220 - 0.0231 lb/in³ | |
|
NOVA Chemicals Dylite® F271TN Expandable Polystyrene Resin
Highly consistent bead size, High gloss characteristics, Low energy consumption, Fast molding cycles, Food contact compliantApplications: Drinking cups (hot and cold), Noodle bowls, Take-out contai..
|
|||
| Bulk Density | 0.609 - 0.641 g/cc | 0.0220 - 0.0231 lb/in³ | |
|
NOVA Chemicals Dylite® F271TS Expandable Polystyrene Resin
Highly consistent bead size, High gloss characteristics, Low energy consumption, Fast molding cycles, Food contact compliantApplications: Drinking cups (hot and cold), Noodle bowls, Take-out contai..
|
|||
| Bulk Density | 0.610 g/cc | 0.0220 lb/in³ | Typical; unexpanded product |
|
NOVA Chemicals Gedexcel® 25C Expandable Polystyrene
Styrene homopolymer containing pentane, used as a blowing agent. Production of complex and high definition preform for the "lost foam" costing technique used in foundries.Information provided by NOV..
|
|||
| Bulk Density | 0.610 g/cc | 0.0220 lb/in³ | Typical; unexpanded product |
|
NOVA Chemicals Gedexcel® 35C Expandable Polystyrene
Styrene homopolymer containing pentane, used as a blowing agent. Production of complex and high definition preform for the "lost foam" costing technique used in foundries.Information provided by NOV..
|
|||
| Bulk Density | 0.610 g/cc | 0.0220 lb/in³ | Typical; unexpanded product |
|
NOVA Chemicals Gedexcel® 44XA Expandable Polystyrene
Styrene homopolymer containing pentane, used as a blowing agent with an additive improving its reaction to fire. Fast molding cycle product allowing to obtain optimum mechanical properties for form ..
|
|||
| Bulk Density | 0.610 g/cc | 0.0220 lb/in³ | Typical; unexpanded product |
|
NOVA Chemicals Gedexcel® 45B Expandable Polystyrene
Styrene homopolymer containing pentane, used as a blowing agent. Fast molding cycle product allowing to obtain optimum mechanical properties for form molding of very thin parts (5 mm to 20 mm).Infor..
|
|||
| Bulk Density | 0.610 g/cc | 0.0220 lb/in³ | Typical; unexpanded product |
|
NOVA Chemicals Gedexcel® 45C Expandable Polystyrene
Styrene homopolymer containing pentane, used as a blowing agent. Production of complex and high definition preform for the "lost foam" costing technique used in foundries.Information provided by NOV..
|
|||
| Bulk Density | 0.610 g/cc | 0.0220 lb/in³ | Typical; unexpanded product |
|
NOVA Chemicals Gedexcel® 45XA Expandable Polystyrene
Styrene homopolymer containing pentane, used as a blowing agent with an additive improving its reaction to fire. Fast molding cycle product allowing to obtain optimum mechanical properties for from ..
|
|||
| Bulk Density | 0.610 g/cc | 0.0220 lb/in³ | Typical; unexpanded product |
|
NOVA Chemicals Gedexcel® 54B Expandable Polystyrene
Styrene homopolymer containing pentane, used as a blowing agent. Fast molding cycle product and reduced stabilization time in silo. Especially adapted to high density molding and thin thickness, an..
|
|||
| Bulk Density | 0.610 g/cc | 0.0220 lb/in³ | Typical; unexpanded product |
|
NOVA Chemicals Gedexcel® 54XA Expandable Polystyrene
Styrene homopolymer containing pentane, used as a blowing agent with an additive improving its reaction to fire. Fast molding cycle product to obtain mechanical properties for form molding parts wit..
|
|||
| Bulk Density | 0.610 g/cc | 0.0220 lb/in³ | Typical; unexpanded product |
|
NOVA Chemicals Gedexcel® 55B Expandable Polystyrene
Styrene homopolymer containing pentane, used as a blowing agent. Fastmolding cycle product allowing to obtain optimum mechanical properties for form molding parts with a thickness over 10 mm.Inform..
|
|||
| Bulk Density | 0.610 g/cc | 0.0220 lb/in³ | Typical; unexpanded product |
|
NOVA Chemicals Gedexcel® 55XA Expandable Polystyrene
Styrene homopolymer containing pentane, used as a blowing agent with an additive improving its reaction to fire. Fast molding cycle product to obtain mechanical properties for form molding parts wit..
|
|||
| Bulk Density | 0.610 g/cc | 0.0220 lb/in³ | Typical; unexpanded product |
|
NOVA Chemicals Gedexcel® 64XA Expandable Polystyrene
Styrene homopolymer containing pentane, used as a blowing agent with an additive improving its reaction to fire. Fast molding cycle product for molding blocks f average and low densities.Information..
|
|||
| Bulk Density | 0.610 g/cc | 0.0220 lb/in³ | Typical; unexpanded product |
|
NOVA Chemicals Gedexcel® 65B Expandable Polystyrene
Styrene homopolymer containing pentane, used as a blowing agent. Production of average to high density blocks and molding of the shape of bulky packaging and parts for the building industry.Informat..
|
|||
| Bulk Density | 0.610 g/cc | 0.0220 lb/in³ | Typical; unexpanded product |
|
NOVA Chemicals Gedexcel® 65D Expandable Polystyrene
Styrene homopolymer containing pentane, used as a blowing agent. For the production of blocks of average and low densities.Information provided by NOVA Chemicals.
|
|||
| Bulk Density | 0.610 g/cc | 0.0220 lb/in³ | Typical; unexpanded product |
|
NOVA Chemicals Gedexcel® 65L Expandable Polystyrene
Styrene homopolymer containing pentane, used as a blowing agent. For the production of blocks of low density. Insulate plasters with low thermal conductivity.Information provided by NOVA Chemicals...
|
|||
| Bulk Density | 0.610 g/cc | 0.0220 lb/in³ | Typical; unexpanded product |
|
NOVA Chemicals Gedexcel® 76D Expandable Polystyrene
Styrene homopolymer containing pentane, used as a blowing agent. For the production of very low density blocks.Information provided by NOVA Chemicals.
|
|||
| Bulk Density | 0.610 g/cc | 0.0220 lb/in³ | |
|
NOVA Chemicals Sclair® 19C (High Gloss) HDPE Blow Molding Resin
19C complies with the U.S. FDA specifications for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food, without te..
|
|||
| Bulk Density | 0.609 - 0.673 g/cc | 0.0220 - 0.0243 lb/in³ | |
|
Chevron Phillips EA3350 Crystal Polystyrene
(discontinued **)
High heat crystal polystyrene.Applications:Medical containersBlends with clear SB-copolymersClam-shell containersBi-axially oriented sheetFeatures:High molecular weight homopolymerHigh Vicat softeni..
|
|||
| Bulk Density | 0.609 - 0.673 g/cc | 0.0220 - 0.0243 lb/in³ | |
|
Chevron Phillips MC3200 Crystal Polystyrene
(discontinued **)
High heat crystal polystyrene.Applications:Medical partsConsumer containers, vials, jars, etc.Clock lensesAudio cassettesFeatures:Fast cycling due to high heat distortionHigh Vicat softening tempera..
|
|||
| Bulk Density | 0.609 - 0.673 g/cc | 0.0220 - 0.0243 lb/in³ | |
|
Chevron Phillips MC3600 Crystal Polystyrene
(discontinued **)
General purpose crystal polystyrene.Applications:HousewaresConsumer containers, vials, jars, etc.Disposable cutleryInjection molded drink cupsFeatures:Easy filling of thin-walled partsExceptional mo..
|
|||
| Bulk Density | 0.610 g/cc | 0.0220 lb/in³ | Typical; unexpanded product |
|
NOVA Chemicals Gedexcel® 76L Expandable Polystyrene
Styrene homopolymer containing pentane, used as a blowing agent. For the production of blocks of low density. Insulate plates with low thermal conductivity.Information provided by NOVA Chemicals.
|
|||
| Bulk Density | 0.610 g/cc | 0.0220 lb/in³ | Typical; unexpanded product |
|
NOVA Chemicals Gedexcel® 76XA Expandable Polystyrene
Styrene homopolymer containing pentane, used as a blowing agent with an additive improving its reaction to fire. Production of low density blocks, recommended for the elastified plates after cutting..
|
|||
| Bulk Density | 0.610 g/cc | 0.0220 lb/in³ | ASTM D1895 |
|
Plenco 00757 Melamine-Phenolic, Granular, Injection Molded
PLENCO 00757 is a melamine-phenolic, copolymer molding compound, offering excellent arc resistance and comparative track index values. It is formulated to provide improved mechanical strength proper..
|
|||
| Bulk Density | 0.610 g/cc | 0.0220 lb/in³ | ASTM D1895 |
|
Plenco 00757 Melamine-Phenolic, Granular, Transfer Molded
PLENCO 00757 is a melamine-phenolic, copolymer molding compound, offering excellent arc resistance and comparative track index values. It is formulated to provide improved mechanical strength proper..
|
|||
| Bulk Density | 0.610 g/cc | 0.0220 lb/in³ | ASTM D1895 |
|
Plenco 2535 Phenolic, Granular, Injection Molded
PLENCO 02535 is a general purpose, organic filled phenolic molding compound offering optimized cure characteristics and excellent electrical properties. Type ASTM 5948 CFG, and UL recognized under c..
|
|||
| Bulk Density | 0.610 g/cc | 0.0220 lb/in³ | ASTM D1895 |
|
Plenco 4466 Phenolic, Granular, Transfer Molded
PLENCO 04466 is a heat resistant, mineral and flock filled phenolic molding compound, offering excellent mechanical strength and cosmetic properties. UL recognized under component file E40654. 04466..
|
|||
| Bulk Density | 0.609 - 0.673 g/cc | 0.0220 - 0.0243 lb/in³ | |
|
Chevron Phillips EB6400 HIPS - High Impact Polystyrene
Rubber modified high impact polystyrene.Applications:Packaging and one-time use itemsPrinted toys and gamesPoint of purchase displaysSilk screen printingFeatures:Very good printabilityMatte surface ..
|
|||
| Bulk Density | 0.610 g/cc | 0.0220 lb/in³ | Pour Density; ASTM D 1513 |
|
Orion Engineered Carbons PUREX® LS 35 Carbon Black
Carbon black grade for manufacture of mechanical rubber goods such as extruded profiles and sealsInformation provided by Orion Engineered Carbons.
|
|||