Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Bulk Density = 0.0231 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Bulk Density 0.608 - 0.640 g/cc
0.0220 - 0.0231 lb/in³
Before expansion
NOVA Chemicals Dylite® F271T Specialty Expandable Polystyrene
Features: Highly consistent bead size; high gloss characteristics; low energy consumption; fast cyclingApplications: Drinking cups -hot and cold, noodle bowls, take-out and ice cream containers, and..
Bulk Density 0.609 - 0.641 g/cc
0.0220 - 0.0231 lb/in³
NOVA Chemicals Dylite® F271TN Expandable Polystyrene Resin
Highly consistent bead size, High gloss characteristics, Low energy consumption, Fast molding cycles, Food contact compliantApplications: Drinking cups (hot and cold), Noodle bowls, Take-out contai..
Bulk Density 0.609 - 0.641 g/cc
0.0220 - 0.0231 lb/in³
NOVA Chemicals Dylite® F271TS Expandable Polystyrene Resin
Highly consistent bead size, High gloss characteristics, Low energy consumption, Fast molding cycles, Food contact compliantApplications: Drinking cups (hot and cold), Noodle bowls, Take-out contai..
Bulk Density 0.580 - 0.640 g/cc
0.0210 - 0.0231 lb/in³
Of unexpanded product
NOVA Chemicals Gedexcel® 25C Expandable Polystyrene
Styrene homopolymer containing pentane, used as a blowing agent. Production of complex and high definition preform for the "lost foam" costing technique used in foundries.Information provided by NOV..
Bulk Density 0.580 - 0.640 g/cc
0.0210 - 0.0231 lb/in³
Of unexpanded product
NOVA Chemicals Gedexcel® 35B Expandable Polystyrene
Styrene homopolymer containing pentane, used as a blowing agent. Production of complex and high definition preforms for the "lost foam" casting technique used in foundries.Information provided by NO..
Bulk Density 0.580 - 0.640 g/cc
0.0210 - 0.0231 lb/in³
Of unexpanded product
NOVA Chemicals Gedexcel® 35C Expandable Polystyrene
Styrene homopolymer containing pentane, used as a blowing agent. Production of complex and high definition preform for the "lost foam" costing technique used in foundries.Information provided by NOV..
Bulk Density 0.580 - 0.640 g/cc
0.0210 - 0.0231 lb/in³
Of unexpanded product
NOVA Chemicals Gedexcel® 44B Expandable Polystyrene
Styrene homopolymer containing pentane, used as a blowing agent. Fast molding cycle product reduced stabilization time in silo. Especially adapted to high density molding and thin thickness, and fr..
Bulk Density 0.580 - 0.640 g/cc
0.0210 - 0.0231 lb/in³
Of unexpanded product
NOVA Chemicals Gedexcel® 44XA Expandable Polystyrene
Styrene homopolymer containing pentane, used as a blowing agent with an additive improving its reaction to fire. Fast molding cycle product allowing to obtain optimum mechanical properties for form ..
Bulk Density 0.580 - 0.640 g/cc
0.0210 - 0.0231 lb/in³
Of unexpanded product
NOVA Chemicals Gedexcel® 45B Expandable Polystyrene
Styrene homopolymer containing pentane, used as a blowing agent. Fast molding cycle product allowing to obtain optimum mechanical properties for form molding of very thin parts (5 mm to 20 mm).Infor..
Bulk Density 0.580 - 0.640 g/cc
0.0210 - 0.0231 lb/in³
Of unexpanded product
NOVA Chemicals Gedexcel® 45C Expandable Polystyrene
Styrene homopolymer containing pentane, used as a blowing agent. Production of complex and high definition preform for the "lost foam" costing technique used in foundries.Information provided by NOV..
Bulk Density 0.580 - 0.640 g/cc
0.0210 - 0.0231 lb/in³
Of unexpanded product
NOVA Chemicals Gedexcel® 45XA Expandable Polystyrene
Styrene homopolymer containing pentane, used as a blowing agent with an additive improving its reaction to fire. Fast molding cycle product allowing to obtain optimum mechanical properties for from ..
Bulk Density 0.580 - 0.640 g/cc
0.0210 - 0.0231 lb/in³
Of unexpanded product
NOVA Chemicals Gedexcel® 54B Expandable Polystyrene
Styrene homopolymer containing pentane, used as a blowing agent. Fast molding cycle product and reduced stabilization time in silo. Especially adapted to high density molding and thin thickness, an..
Bulk Density 0.580 - 0.640 g/cc
0.0210 - 0.0231 lb/in³
Of unexpanded product
NOVA Chemicals Gedexcel® 54XA Expandable Polystyrene
Styrene homopolymer containing pentane, used as a blowing agent with an additive improving its reaction to fire. Fast molding cycle product to obtain mechanical properties for form molding parts wit..
Bulk Density 0.580 - 0.640 g/cc
0.0210 - 0.0231 lb/in³
Of unexpanded product
NOVA Chemicals Gedexcel® 55B Expandable Polystyrene
Styrene homopolymer containing pentane, used as a blowing agent. Fastmolding cycle product allowing to obtain optimum mechanical properties for form molding parts with a thickness over 10 mm.Inform..
Bulk Density 0.580 - 0.640 g/cc
0.0210 - 0.0231 lb/in³
Of unexpanded product
NOVA Chemicals Gedexcel® 55C Expandable Polystyrene
Styrene homopolymer containing pentane, used as a blowing agent. Fast molding cycle product allowing to obtain optimum mechanical properties for form molding parts with a thickness over 10 mm.Infor..
Bulk Density 0.580 - 0.640 g/cc
0.0210 - 0.0231 lb/in³
Of unexpanded product
NOVA Chemicals Gedexcel® 55XA Expandable Polystyrene
Styrene homopolymer containing pentane, used as a blowing agent with an additive improving its reaction to fire. Fast molding cycle product to obtain mechanical properties for form molding parts wit..
Bulk Density 0.580 - 0.640 g/cc
0.0210 - 0.0231 lb/in³
Of unexpanded product
NOVA Chemicals Gedexcel® 64XA Expandable Polystyrene
Styrene homopolymer containing pentane, used as a blowing agent with an additive improving its reaction to fire. Fast molding cycle product for molding blocks f average and low densities.Information..
Bulk Density 0.580 - 0.640 g/cc
0.0210 - 0.0231 lb/in³
Of unexpanded product
NOVA Chemicals Gedexcel® 65B Expandable Polystyrene
Styrene homopolymer containing pentane, used as a blowing agent. Production of average to high density blocks and molding of the shape of bulky packaging and parts for the building industry.Informat..
Bulk Density 0.580 - 0.640 g/cc
0.0210 - 0.0231 lb/in³
Of unexpanded product
NOVA Chemicals Gedexcel® 65D Expandable Polystyrene
Styrene homopolymer containing pentane, used as a blowing agent. For the production of blocks of average and low densities.Information provided by NOVA Chemicals.
Bulk Density 0.580 - 0.640 g/cc
0.0210 - 0.0231 lb/in³
Of unexpanded product
NOVA Chemicals Gedexcel® 65L Expandable Polystyrene
Styrene homopolymer containing pentane, used as a blowing agent. For the production of blocks of low density. Insulate plasters with low thermal conductivity.Information provided by NOVA Chemicals...
Bulk Density 0.580 - 0.640 g/cc
0.0210 - 0.0231 lb/in³
Of unexpanded product
NOVA Chemicals Gedexcel® 65XA Expandable Polystyrene
Styrene homopolymer containing pentane, used as a blowing agent with an additive improving its reaction to fire. Fast molding cycle product for molding blocks of average and low densities.Informati..
Bulk Density 0.580 - 0.640 g/cc
0.0210 - 0.0231 lb/in³
Of unexpanded product
NOVA Chemicals Gedexcel® 74XA Expandable Polystyrene
Styrene homopolymer containing pentane, sued as a blowing agent with an additive improving its reaction to fire. Fast molding cycle product for molding blocks of average and low densities.Informatio..
Bulk Density 0.580 - 0.640 g/cc
0.0210 - 0.0231 lb/in³
Of unexpanded product
NOVA Chemicals Gedexcel® 76D Expandable Polystyrene
Styrene homopolymer containing pentane, used as a blowing agent. For the production of very low density blocks.Information provided by NOVA Chemicals.
Bulk Density 0.580 - 0.640 g/cc
0.0210 - 0.0231 lb/in³
Of unexpanded product
NOVA Chemicals Gedexcel® 76L Expandable Polystyrene
Styrene homopolymer containing pentane, used as a blowing agent. For the production of blocks of low density. Insulate plates with low thermal conductivity.Information provided by NOVA Chemicals.
Bulk Density 0.580 - 0.640 g/cc
0.0210 - 0.0231 lb/in³
Of unexpanded product
NOVA Chemicals Gedexcel® 76XA Expandable Polystyrene
Styrene homopolymer containing pentane, used as a blowing agent with an additive improving its reaction to fire. Production of low density blocks, recommended for the elastified plates after cutting..
Copyright © lookpolymers.com All Rights Reserved