Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Bulk Density = 0.0289 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Bulk Density 0.600 - 0.800 g/cc
0.0217 - 0.0289 lb/in³
LG Chemical SAP Super Absorbent Polymer
Features: Super Absorbent Polymer absorbs pure water at several-hundred times of its dry weight. They are used extensively as the raw materials for various industries in baby diaper, feminine hygien..
Bulk Density 0.500 - 0.800 g/cc
0.0181 - 0.0289 lb/in³
Shandong Dongyue Polymer DF-21C PTFE Presintered Resin
Usage: The presintered resin is suitable for continuously extruding of all types, pushing and pressing PTFE rod, tube and special shape.Packing: PTFE is packed in double layer PVC bags inside and in..
Bulk Density 0.620 - 0.800 g/cc
0.0224 - 0.0289 lb/in³
RP-0155
Solvay REPEL-O-TEX® PF-594 Surfactant
Description: High active soil release polymer for powder laundry. Prevents adhesion of soils between washes and soil redeposition during wash. Repel-O-Tex PF 594 has been specifically formulated for..
Bulk Density 0.700 - 0.800 g/cc
0.0253 - 0.0289 lb/in³
Solvay RHODICARE T Surfactant
Description: Rhodicare® T is high purity grade specifically designed for thickening and suspension in clear formulations. It has high electrolyte stability over a wide range of pH and fast hydrat..
Bulk Density 0.700 - 0.800 g/cc
0.0253 - 0.0289 lb/in³
Solvay RHODOPOL® T Surfactant
Description: Transparent grade xanthan gum. It is It exhibits high pseudoplastic behavior effective thickening and stabilizing agent.Identification: XANTHAN GUMCAS: 11138 – 66 – 2Available..
Bulk Density 0.600 - 0.800 g/cc
0.0217 - 0.0289 lb/in³
Powder Density; ISO 60
Vyncolit 2530 W Novolac Phenolic
Mineral and organic filled phenolic molding compound with excellent thermal properties.USES: Lamp sockets, special lamp holders, pan handles and knobs.Information provided by Vyncolit, a Sumitomo Ba..
Bulk Density 0.650 - 0.800 g/cc
0.0235 - 0.0289 lb/in³
Addcomp ADD-VANCE® DS 485 Desiccant masterbatch in LLDPE carrier
Fields of application: Highly concentrated desiccant masterbatch for LDPE, LLDPE, HDPE, PP, EVA and other ethylene copolymers.Examples: Elimination of moisture from (recycle) polymers in moisture se..
Bulk Density 0.500 - 0.800 g/cc
0.0181 - 0.0289 lb/in³
BASF Ultramid® A3EG10 50% Glass Filled PA66 (Conditioned)
Description: 50% glass-fiber reinforced injection-molding grade for technical articles of very high stiffness as well as for electric insulating parts.Information provided by BASF
Bulk Density 0.500 - 0.800 g/cc
0.0181 - 0.0289 lb/in³
BASF Ultramid® A3EG10 50% Glass Filled PA66 (Dry)
Description: 50% glass-fiber reinforced injection-molding grade for technical articles of very high stiffness as well as for electric insulating parts.Information provided by BASF
Bulk Density 0.500 - 0.800 g/cc
0.0181 - 0.0289 lb/in³
BASF Ultramid® B3EG5 25% Glass Filled PA6 (Dry)
Description: 25% glass-fiber reinforced injection-molding grade for industrial articles and electrical insulating partsInformation provided by BASF
Bulk Density 0.500 - 0.800 g/cc
0.0181 - 0.0289 lb/in³
BASF Ultramid® B3EG7 35% Glass Filled PA6 (Dry)
Description: 35% Glass fiber reinforced injection molding grade for industrial articles and electrical insulating parts.Information provided by BASF
Bulk Density 0.500 - 0.800 g/cc
0.0181 - 0.0289 lb/in³
BASF Ultramid® KR 4355 G5 25% Glass Filled PA6/6T (Dry)
Description: 25% glass-fiber reinforced product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties r..
Bulk Density 0.500 - 0.800 g/cc
0.0181 - 0.0289 lb/in³
BASF Ultramid® KR 4355 G7 BK 00564 35% Glass Filled PA6/6T (Conditioned)
Description: 35% glass-fiber reinforced product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties r..
Bulk Density 0.500 - 0.800 g/cc
0.0181 - 0.0289 lb/in³
BASF Ultramid® KR 4365 G5 BK 00100 35% Glass Filled PA6/6T FR (Conditioned)
Description: Partially aromatic polyamide; flame retardant based on red phosphorus; low water absorption, high melting point (295°C); low tendency to form deposits on electrical contacts, very resi..
Bulk Density 0.700 - 0.800 g/cc
0.0253 - 0.0289 lb/in³
BASF Ultrason® E 2010 C6 30% Carbon Filled
Carbon fibers and Ultrason® two partners with good properties. The combination of carbon fibers with the amorphous high-temperature plastic Ultrason® guarantees mechanical properties for temperatu..
Bulk Density 0.500 - 0.800 g/cc
0.0181 - 0.0289 lb/in³
BASF Ultramid® A3XZG5 BK 23187 25% Glass Filled PA66 FR (Conditioned)
Description: Impact-modified, 25% glass-fiber reinforced injection-molding grade with improved flame retardance and enhanced long-term stability. Flame retardant based on red phosphorus; for compone..
Bulk Density 0.500 - 0.800 g/cc
0.0181 - 0.0289 lb/in³
BASF Ultramid® A3Z BK 30464 PA66 (Conditioned)
Description: Impact-modified and stabilized injection- molding grade for components and housings with good low temperature impact resistance.Information provided by BASF
Bulk Density 0.500 - 0.800 g/cc
0.0181 - 0.0289 lb/in³
BASF Ultramid® A4H PA66 (Dry)
Description: Highly heat aging resistant, medium-viscosity injection-molding grade for highly stressed parts such as bearing cages, gearwheels, spool bodies and chain drive tensioners.Information pr..
Bulk Density 0.500 - 0.800 g/cc
0.0181 - 0.0289 lb/in³
BASF Ultramid® B35EG3 15% Glass Filled PA6 (Conditioned)
Description: 15% glass-fiber reinforced injection-molding grade for gIT applications such as, for example, steering column switches, vehicle mirror housings and the wheels of mountain bikes.Informat..
Bulk Density 0.500 - 0.800 g/cc
0.0181 - 0.0289 lb/in³
BASF Ultramid® B35G3 BK 00564 15% Glass Filled PA6 (Conditioned)
Description: 15% glass fiber reinforced injection molding grade e.g. for internal gas pressure applications such as flashing direction switch gears, automobile mirror housings and wheels of mountain..
Bulk Density 0.500 - 0.800 g/cc
0.0181 - 0.0289 lb/in³
BASF Ultramid® B3EG5 25% Glass Filled PA6 (Conditioned)
Description: 25% glass-fiber reinforced injection-molding grade for industrial articles and electrical insulating partsInformation provided by BASF
Bulk Density 0.500 - 0.800 g/cc
0.0181 - 0.0289 lb/in³
BASF Ultramid® B3GK24 BK 00564 10/20% Glass/Glass Bead Filled PA6 (Conditioned)
Description: combined 10% glass-fiber and 20% glass-bead reinforced injection-molding grade for technical articles of very good dimensional stability, for instance, vehicle ash tray housings and ele..
Bulk Density 0.700 - 0.800 g/cc
0.0253 - 0.0289 lb/in³
BASF Ultrason® E 2010 HC PESU
Information provided by BASF
Bulk Density 0.700 - 0.800 g/cc
0.0253 - 0.0289 lb/in³
BASF Ultrason® S 3010 MR UN PSU
Description: Unreinforced, higher viscosity injection molding and extrusion grade, tougher, with improved chemical resistance and demolding optimized. Abbreviated designation according to ISO 1043-1..
Bulk Density 0.500 - 0.800 g/cc
0.0181 - 0.0289 lb/in³
BASF Ultramid® A3HG5 LS BK 23189 25% Glass Filled PA66 (Dry)
Description: 25% glass fiber reinforced injection molding grade for machinery components and housings of high stiffness and dimensional stability such as coil formers and bearing cages. Also used fo..
Bulk Density 0.500 - 0.800 g/cc
0.0181 - 0.0289 lb/in³
BASF Ultramid® B3UG4 Grey 22975 20% Glass Filled PA66 FR (Dry)
Description: Halogen-free and phosphorus free flame retardant injection-molding grade with outstanding free-flow properties, good electrical properties and low smoke density; resistant to glow wire..
Bulk Density 0.500 - 0.800 g/cc
0.0181 - 0.0289 lb/in³
BASF Ultramid® B3UG4 LS BK 23215 20% Glass Filled PA66 FR (Conditioned)
Description: Halogen-free and phosphorus free flame retardant injection-molding grade with outstanding free-flow properties, good electrical properties and low smoke density; resistant to glow wire..
Bulk Density 0.500 - 0.800 g/cc
0.0181 - 0.0289 lb/in³
BASF Ultramid® B3WG6 GP BK 23210 30% Glass Filled PA6 (Dry)
Description: 30% Glass fiber reinforced and heat aging resistant injection molding grade used e.g. for automobile manifold.Information provided by BASF
Bulk Density 0.500 - 0.800 g/cc
0.0181 - 0.0289 lb/in³
BASF Ultramid® Seal-Fit PA6/66 (Conditioned)
Description: Transparent, tough, amorphous copolyamide for injection molding, specially developed for tight overmoulding of metal inlays.Information provided by BASF
Bulk Density 0.500 - 0.800 g/cc
0.0181 - 0.0289 lb/in³
BASF Ultramid® B3UG4 LS Grey22985 20% Glass Filled PA66 FR (Dry)
Description: Halogen-free and phosphorus free flame retardant injection-molding grade with outstanding free-flow properties, good electrical properties and low smoke density; resistant to glow wire..