Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Bulk Density = 0.250 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Bulk Density 0.250 g/cc
0.00903 lb/in³
ISO 1183
Victrex® PEEK 600PF Polyetheretherketone  (discontinued **)
Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, fine powder for compression compounding, low flow, FDA food contact complian..
Bulk Density 0.250 - 0.400 g/cc
0.00903 - 0.0145 lb/in³
Magyar Aluminum ALOLT 120F Aluminum Hydroxide
Fine Precipitated Type
Bulk Density 0.250 - 0.500 g/cc
0.00903 - 0.0181 lb/in³
Magyar Aluminum ALOLT 60F Aluminum Hydroxide
Fine Precipitated Type
Bulk Density 0.250 - 0.450 g/cc
0.00903 - 0.0163 lb/in³
Magyar Aluminum ALOLT 90DLS Aluminum Hydroxide
Fine Precipitated Type
Bulk Density >= 0.250 g/cc
>= 0.00903 lb/in³
Aerated; LSY-QB-KD019
LG Chemical EM500 Impact modifier for Engineering Plastics
Description: LG Chem impact modifiers for Engineering Plastic are developed to enhance the impact strength of Engineering Plastics (PC, PBT, ABS, PC/PBT, PC/ABS, etc). LG Chem has 2 type impact modi..
Bulk Density >= 0.250 g/cc
>= 0.00903 lb/in³
Aerated; LSY-QB-KD019
LG Chemical EM500A Impact modifier for Engineering Plastics
Description: LG Chem impact modifiers for Engineering Plastic are developed to enhance the impact strength of Engineering Plastics (PC, PBT, ABS, PC/PBT, PC/ABS, etc). LG Chem has 2 type impact modi..
Bulk Density >= 0.250 g/cc
>= 0.00903 lb/in³
Aerated; LSY-QB-KD019
LG Chemical EM505 Impact modifier for Engineering Plastics
Description: LG Chem impact modifiers for Engineering Plastic are developed to enhance the impact strength of Engineering Plastics (PC, PBT, ABS, PC/PBT, PC/ABS, etc). LG Chem has 2 type impact modi..
Bulk Density 0.250 g/cc
0.00903 lb/in³
Tap Density
Momentive Performance Materials NX5 Boron Nitride (BN) Powder
Grades NX1, NX5, NX9, and NX10. The NX line makes BN accessible to users of alternate materials, such as aluminum nitride, alumina, and fused silica, who may have previously ruled out BN.NX grades a..
Bulk Density 0.250 - 0.300 g/cc
0.00903 - 0.0108 lb/in³
Sinotek Materials Rigid Graphite Felt Board Heat Insulation Material
Information provided by Sinotek
Bulk Density 0.250 g/cc
0.00903 lb/in³
ASTM D1895
Sumitomo Bakelite North America E 264H Long Glass Fiber Reinforced Epoxy
E 264H is a high strength, long fiberglass reinforced epoxy molding compound, which features improved flow in transfer molding.Information provided by Sumitomo Bak North America, Inc.
Bulk Density 0.250 g/cc
0.00903 lb/in³
Zircar Zirconia ZYBF-5 Zirconia Bulk Fiber Insulation
Zirconia Bulk Fibers Type ZYBF are yttria stabilized zirconia fibers available in five different forms, all having useful properties up to 2200°C. These polycrystalline fibers can be vacuum formed ..
Bulk Density 0.250 g/cc
0.00903 lb/in³
Chosun Refractories 1000BOARD Board
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Bulk Density 0.250 g/cc
0.00903 lb/in³
Chosun Refractories 1260BOARD Board
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Bulk Density 0.250 - 0.300 g/cc
0.00903 - 0.0108 lb/in³
BASF Ultrason® E 2020 P SR PESU
Description: Polyethersulfone flakes, e.g. for membrane applications, coatings and resin modification, containing min. 50% of OH-endgroups. The product is soluble in N-methyl-pyrrolidone (NMP) and N..
Bulk Density 0.250 g/cc
0.00903 lb/in³
ASTM D4895
3M Dyneon™ J14 PTFE Micropowder
3M™ Dyneon™ PTFE Micropowders can be used as additives in many applications and at concentrations typically from 5 to 20%. Homogeneous incorporation is the single most important process and applic..
Bulk Density 0.250 g/cc
0.00903 lb/in³
Zircar Zirconia ZYBF-5 Zirconia Bulk Fiber Insulation
Zirconia Bulk Fibers Type ZYBF are yttria stabilized zirconia fibers available in five different forms, all having useful properties up to 2200°C. These polycrystalline fibers can be vacuum formed ..
Copyright © lookpolymers.com All Rights Reserved