Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Bulk Density 0.350 g/cc
0.0126 lb/in³
Loose
Nyco NYGLOS® M3 Wollastonite
This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology make..
Bulk Density 0.350 g/cc
0.0126 lb/in³
Nabaltec APYMAG® 60S Magnesium Hydroxide
The demand for halogen free flame retardant plastics for applications in automobile, electrical, and construction industries is stronger than ever. The use of mineral flame retardants within these p..
Bulk Density 0.350 g/cc
0.0126 lb/in³
Pour Density; ASTM D 1513
Orion Engineered Carbons CORAX® N 220 ASTM Carbon Black
Standard grade of furnace black in accordance with the requirements of ASTM D 1765Hard Black - tread grade, reinforcing carbon blackInformation provided by Orion Engineered Carbons.
Bulk Density 0.350 g/cc
0.0126 lb/in³
ASTM D4895
3M Dyneon™ TF 9201 PTFE  (discontinued **)
Low molecular weight virgin PTFE (non-degraded)Agglomerate particlesEasily deagglomerated when incorporated into other matrixesSuitable for use in food contact applications. Complies with FDE specif..
Bulk Density 0.350 - 0.500 g/cc
0.0126 - 0.0181 lb/in³
Magyar Aluminum ALOLT 60DLS Aluminum Hydroxide
Fine Precipitated Type
Bulk Density 0.350 - 0.500 g/cc
0.0126 - 0.0181 lb/in³
Magyar Aluminum ALOLT 60P Aluminum Hydroxide
Fine Precipitated Type
Bulk Density 0.350 g/cc
0.0126 lb/in³
ASTM D1895 method B
Kraton® D1161 E (SIS) Linear Triblock Copolymer
Description: Kraton D1161 E is a clear, linear triblock copolymer based on styrene and isoprene with a polystyrene content of 15%. It is supplied from Europe in the physical form identified: D1161 E..
Bulk Density 0.350 - 0.500 g/cc
0.0126 - 0.0181 lb/in³
Solvay Chemicals NOCOLOK® Cs Flux
Flux for brazing magnesium aluminum alloysHS No.: 38109090/CAS-No.: 60304-36-1 and 138577-01-2Uses: Automotive Sector, Commercial & Residential Air Conditioning, Refrigeration and Household & Elect..
Bulk Density 0.350 - 0.550 g/cc
0.0126 - 0.0199 lb/in³
Solvay Chemicals NOCOLOK® Flux Potassium Fluoroaluminate
A high quality fluxing agent for brazing aluminum components. Classifications: HS No.: 38109090/CAS-No.: 60304-36-1Uses: Automotive Sector, Commercial & Residential Air Conditioning, Refrigeration ..
Bulk Density 0.350 - 0.550 g/cc
0.0126 - 0.0199 lb/in³
ASTM D-4894
Shamrock Technologies Fluoro T® 607 Thermoplastic Grade PTFE Additive
The addition of micronized polytetrafluoroethylene (PTFE) powder to polymeric resins provides greatly increased resistance to surface wear and abrasion. PTFE has a very low coefficient of friction ..
Bulk Density 0.350 - 0.550 g/cc
0.0126 - 0.0199 lb/in³
ASTM D-4894
Shamrock Technologies Fluoro T® 615 Thermoplastic Grade PTFE Additive
The addition of micronized polytetrafluoroethylene (PTFE) powder to polymeric resins provides greatly increased resistance to surface wear and abrasion. PTFE has a very low coefficient of friction ..
Bulk Density 0.350 - 0.550 g/cc
0.0126 - 0.0199 lb/in³
ASTM D-4894
Shamrock Technologies Fluoro T® 707 Thermoplastic Grade PTFE Additive
The addition of micronized polytetrafluoroethylene (PTFE) powder to polymeric resins provides greatly increased resistance to surface wear and abrasion. PTFE has a very low coefficient of friction ..
Bulk Density 0.350 - 0.550 g/cc
0.0126 - 0.0199 lb/in³
ASTM D-4894
Shamrock Technologies Fluoro T® 803 Thermoplastic Grade PTFE Additive
The addition of micronized polytetrafluoroethylene (PTFE) powder to polymeric resins provides greatly increased resistance to surface wear and abrasion. PTFE has a very low coefficient of friction ..
Bulk Density 0.350 - 0.550 g/cc
0.0126 - 0.0199 lb/in³
ASTM D-4894
Shamrock Technologies MicroFLON® 1437 Thermoplastic Grade PTFE Additive
Used in high temperature engineering plastics.The addition of micronized polytetrafluoroethylene (PTFE) powder to polymeric resins provides greatly increased resistance to surface wear and abrasion...
Bulk Density 0.350 - 0.550 g/cc
0.0126 - 0.0199 lb/in³
Shandong Rike Chemical HELIâ„¢ HL-251 PVC Processing Aid Series (PA)
Outline of ACR Processing AidsProducts of processing aid series developed by our company are acrylic copolymers. The basic function of processing aids is to improve processing performance and promo..
Bulk Density 0.350 - 0.550 g/cc
0.0126 - 0.0199 lb/in³
Shandong Rike Chemical HELIâ„¢ HL-750 Weather-resistance Acrylic Impact Modifier (AIM)
Outline of ACR Impact Modifiers:The PVC impact modifiers developed by our company are acrylic copolymers (ACR) with a core-shell structure, their cores are acrylic ester and shells are methacrylic c..
Bulk Density 0.350 - 0.550 g/cc
0.0126 - 0.0199 lb/in³
Shandong Rike Chemical HELIâ„¢ HL-769 Weather-resistance Acrylic Impact Modifier (AIM)
Outline of ACR Impact Modifiers:The PVC impact modifiers developed by our company are acrylic copolymers (ACR) with a core-shell structure, their cores are acrylic ester and shells are methacrylic c..
Bulk Density 0.350 - 0.550 g/cc
0.0126 - 0.0199 lb/in³
Shandong Rike Chemical HELIâ„¢ HPA-220-2 PVC Processing Aid Series (PA)
Outline of ACR Processing AidsProducts of processing aid series developed by our company are acrylic copolymers. The basic function of processing aids is to improve processing performance and promo..
Bulk Density 0.350 - 0.550 g/cc
0.0126 - 0.0199 lb/in³
Shandong Rike Chemical HELIâ„¢ HPA-221 PVC Processing Aid Series (PA)
Outline of ACR Processing AidsProducts of processing aid series developed by our company are acrylic copolymers. The basic function of processing aids is to improve processing performance and promo..
Bulk Density 0.350 - 0.550 g/cc
0.0126 - 0.0199 lb/in³
Shandong Rike Chemical RIKEâ„¢ RK-561 MBS Impact Modifier for PVC Opaque Product
Outline of MBS Impact ModifierRIKEâ„¢ MBS impact modifier for PVC opaque product developed by our R&D Center is the newest PVC impact modifier. Our MBS impact modifier has higher rubber content ..
Bulk Density 0.350 - 0.550 g/cc
0.0126 - 0.0199 lb/in³
Shandong Rike Chemical RIKEâ„¢ RK-564 MBS Impact Modifier for PVC Opaque Product
Outline of MBS Impact ModifierRIKEâ„¢ MBS impact modifier for PVC opaque product developed by our R&D Center is the newest PVC impact modifier. Our MBS impact modifier has higher rubber content ..
Bulk Density 0.350 - 0.550 g/cc
0.0126 - 0.0199 lb/in³
Shandong Rike Chemical HELIâ„¢ HPA-220 PVC Processing Aid Series (PA)
Outline of ACR Processing AidsProducts of processing aid series developed by our company are acrylic copolymers. The basic function of processing aids is to improve processing performance and promo..
Bulk Density 0.350 - 0.450 g/cc
0.0126 - 0.0163 lb/in³
Trelleborg Fillite® 160 Alumino-silicate Cenospheres
Fillite is a glass hard, inert, hollow silicate sphere. Fillite is primarily used to reduce the weight of plastics, rubbers, resins, cement, etc., but also imparts further benefits in many situatio..
Bulk Density 0.350 - 0.450 g/cc
0.0126 - 0.0163 lb/in³
Trelleborg Fillite® 52/7S (355) Alumino-silicate Cenospheres
Fillite is a glass hard, inert, hollow silicate sphere. Fillite is primarily used to reduce the weight of plastics, rubbers, resins, cement, etc., but also imparts further benefits in many situatio..
Bulk Density 0.350 - 0.450 g/cc
0.0126 - 0.0163 lb/in³
Trelleborg Fillite® FG (300) Alumino-silicate Cenospheres
Fillite is a glass hard, inert, hollow silicate sphere. Fillite is primarily used to reduce the weight of plastics, rubbers, resins, cement, etc., but also imparts further benefits in many situatio..
Bulk Density 0.350 - 0.450 g/cc
0.0126 - 0.0163 lb/in³
Trelleborg Fillite® 106 Alumino-silicate Cenospheres
Fillite is a glass hard, inert, hollow silicate sphere. Fillite is primarily used to reduce the weight of plastics, rubbers, resins, cement, etc., but also imparts further benefits in many situatio..
Bulk Density 0.350 g/cc
0.0126 lb/in³
Tapped
Nyco ULTRAFIBRE® 4W Wollastonite
Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br..
Bulk Density 0.350 g/cc
0.0126 lb/in³
ISO 60
Vyncolit Neopreg Kinel® SK4504 S12 Carbon Reinforced Molding Compound
Epoxy based molding compound long carbon fiber reinforced suited for demanding tribologic applications under dry running conditions, exposed to a wide range of temperatures (-100°C up to 150°C)...
Bulk Density 0.350 - 0.550 g/cc
0.0126 - 0.0199 lb/in³
Shandong Rike Chemical HELI™ HL-225 PVC Processing Aid Series (PA)
Outline of ACR Processing AidsProducts of processing aid series developed by our company are acrylic copolymers. The basic function of processing aids is to improve processing performance and promo..
Bulk Density 0.350 - 0.550 g/cc
0.0126 - 0.0199 lb/in³
ASTM D-4894
Shamrock Technologies MicroFLON® 1437FG Thermoplastic Grade PTFE Additive
Used in high temperature engineering plastics; food contactThe addition of micronized polytetrafluoroethylene (PTFE) powder to polymeric resins provides greatly increased resistance to surface wear ..