| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Bulk Density | 0.590 - 0.630 g/cc | 0.0213 - 0.0228 lb/in³ | |
|
Polimeri Europa Extir® CM Galileo Europa 5 AE Expandable Polystyrene - Continuous Mass
Product Description:Extir CM is the new expandable products range produced with the new Continuous Mass technology. All the products have a very low dimensional dispersion and a reduced content of ..
|
|||
| Bulk Density | 0.590 - 0.630 g/cc | 0.0213 - 0.0228 lb/in³ | |
|
Polimeri Europa Extir® CM Galileo Europa 5 Expandable Polystyrene - Continuous Mass
Product Description:Extir CM is the new expandable products range produced with the new Continuous Mass technology. All the products have a very low dimensional dispersion and a reduced content of ..
|
|||
| Bulk Density | 0.590 - 0.630 g/cc | 0.0213 - 0.0228 lb/in³ | |
|
Polimeri Europa Extir® LN 3000 Expandable Polystyrene
Extir LN 3000 belongs to a new expandable product family, the Leonardo Series, with improved processing features: high expandability, high moulding productivity, wide processing area, optimal fusion..
|
|||
| Bulk Density | 0.590 - 0.630 g/cc | 0.0213 - 0.0228 lb/in³ | |
|
Polimeri Europa Extir® LN 5000 Expandable Polystyrene
Extir LN 5000 belongs to the product family, the Leonardo Series, with these features: high expandability, high moulding productivity, wide processing area, optimal fusion and mechanical strength, e..
|
|||
| Bulk Density | 0.590 - 0.630 g/cc | 0.0213 - 0.0228 lb/in³ | |
|
Polimeri Europa Extir® Verdi VR A3000 AE Expandable Polystyrene - Flame Retardant
Product Description:Extir Verdi VR A3000 AE is a flame-retardant expandable polystyrene in the form of spherical beads of medium particle size, containing pentane as blowing agent.Extir does not con..
|
|||
| Bulk Density | 0.590 - 0.630 g/cc | 0.0213 - 0.0228 lb/in³ | |
|
Polimeri Europa Extir® CM Galileo Io 5 AE Expandable Polystyrene - Continuous Mass
Product Description:Extir CM is the new expandable products range produced with the new Continuous Mass technology. All the products have a very low dimensional dispersion and a reduced content of ..
|
|||
| Bulk Density | 0.590 - 0.630 g/cc | 0.0213 - 0.0228 lb/in³ | |
|
Polimeri Europa Extir® CM Galileo Io 5 Expandable Polystyrene - Continuous Mass
Product Description:Extir CM is the new expandable products range produced with the new Continuous Mass technology. All the products have a very low dimensional dispersion and a reduced content of ..
|
|||
| Bulk Density | 0.590 - 0.630 g/cc | 0.0213 - 0.0228 lb/in³ | |
|
Polimeri Europa Extir® CM Giotto 5 AE Expandable Polystyrene - Continuous Mass/Flame Retardant
Product Description:Extir CM is the new expandable products range produced with the new Continuous Mass technology. All the products have a very low dimensional dispersion and a reduced content of ..
|
|||
| Bulk Density | 0.590 - 0.630 g/cc | 0.0213 - 0.0228 lb/in³ | |
|
Polimeri Europa Extir® CM Giotto 5 Expandable Polystyrene - Continuous Mass
Product Description:Extir CM is the new expandable products range produced with the new Continuous Mass technology. All the products have a very low dimensional dispersion and a reduced content of ..
|
|||
| Bulk Density | 0.590 - 0.630 g/cc | 0.0213 - 0.0228 lb/in³ | |
|
Polimeri Europa Extir® D 3000 AE Expandable Polystyrene - Flame Retardant
Product Description:Extir D 3000 AE is a flame-retardant expandable polystyrene in the form of spherical beads of medium particle size, containing pentane as blowing agent.Extir does not contain CFC..
|
|||
| Bulk Density | 0.590 - 0.630 g/cc | 0.0213 - 0.0228 lb/in³ | |
|
Polimeri Europa Extir® EH 2000 Expandable Polystyrene
Extir EH 2000 is an expandable polystyrene in the form of spherical beads of fine particle size, with a low pentane content as blowing agent. Extir does not contain CFC or HCFC. Extir EH 2000 is use..
|
|||
| Bulk Density | 0.590 - 0.630 g/cc | 0.0213 - 0.0228 lb/in³ | |
|
Polimeri Europa Extir® EH 3000 Expandable Polystyrene
Extir EH 3000 is an expandable polystyrene in the form of spherical beads of medium particle size, with a low pentane content as blowing agent. Extir does not contain CFC or HCFC. Extir EH 3000 is u..
|
|||
| Bulk Density | 0.590 - 0.630 g/cc | 0.0213 - 0.0228 lb/in³ | |
|
Polimeri Europa Extir® GEO 3000 AE Expandable Polystyrene - Flame Retardant
Product Description:Extir GEO 3000 AE is a flame-retardant expandable polystyrene in the form of spherical beads of medium particle size, containing pentane as blowing agent.Extir does not contain C..
|
|||
| Bulk Density | 0.589 - 0.630 g/cc | 0.0213 - 0.0228 lb/in³ | |
|
Polimeri Europa Extir® LN 2001 Expandable Polystyrene
Extir LN 2001 belongs to a new expandable product family, the Leonardo Series. Extir LN 2001 is specially coated to be incorporated into bricks, concrete, mortar and plaster, in order to lighten the..
|
|||
| Bulk Density | 0.590 - 0.630 g/cc | 0.0213 - 0.0228 lb/in³ | |
|
Polimeri Europa Extir Leonardo A 3000 AE Expandable Polystyrene
(discontinued **)
Extir A 3000 AE is a flame retardant expandable polystyrene in the form of spherical beads of medium particle size, containing pentane as blowing agent. Extir does not contain CFC or HCFC. Extir A 3..
|
|||
| Bulk Density | 0.590 - 0.630 g/cc | 0.0213 - 0.0228 lb/in³ | |
|
Polimeri Europa Extir Leonardo A 5000 AE Expandable Polystyrene
(discontinued **)
Extir A 5000 AE is a flame retardant expandable polystyrene in the form of spherical beads of medium-large particle size, containing pentane as blowing agent. Extir does not contain CFC or HCFC. Ext..
|
|||
| Bulk Density | 0.590 - 0.630 g/cc | 0.0213 - 0.0228 lb/in³ | |
|
Polimeri Europa Extir Leonardo A 7000 AE Expandable Polystyrene
(discontinued **)
Extir A 7000 AE is a flame retardant expandable polystyrene in the form of spherical beads of large particle size, containing pentane as blowing agent. Extir does not contain CFC or HCFC. Extir A 7..
|
|||
| Bulk Density | 0.590 - 0.630 g/cc | 0.0213 - 0.0228 lb/in³ | |
|
Polimeri Europa Extir Leonardo B 2000 AE Expandable Polystyrene
(discontinued **)
Extir B 2000 AE is a flame retardant expandable polystyrene in the form of spherical beads of fine particle size, containing pentane as blowing agent. Extir does not contain CFC or HCFC. Extir B 200..
|
|||
| Bulk Density | 0.590 - 0.630 g/cc | 0.0213 - 0.0228 lb/in³ | |
|
Polimeri Europa Extir Leonardo B 3000 AE Expandable Polystyrene
(discontinued **)
Extir B 3000 AE is a flame retardant expandable polystyrene in the form of spherical beads of medium particle size, containing pentane as blowing agent. Extir does not contain CFC or HCFC. This grad..
|
|||
| Bulk Density | 0.590 - 0.630 g/cc | 0.0213 - 0.0228 lb/in³ | |
|
Polimeri Europa Extir Leonardo B 5000 AE Expandable Polystyrene
(discontinued **)
Extir B 5000 AE is a flame retardant expandable polystyrene in the form of spherical beads of medium-large particle size, containing pentane as blowing agent. Extir does not contain CFC or HCFC. Ext..
|
|||
| Bulk Density | 0.590 - 0.630 g/cc | 0.0213 - 0.0228 lb/in³ | |
|
Polimeri Europa Extir® D 3000 AE Expandable Polystyrene
(discontinued **)
Extir D 3000 AE is a flame-retardant expandable polystyrene in the form of spherical beads of medium particle size, containing pentane as blowing agent. Extir does not contain CFC or CFC. Extir D 30..
|
|||
| Bulk Density | 0.590 - 0.630 g/cc | 0.0213 - 0.0228 lb/in³ | |
|
Polimeri Europa Extir® E 3000 AE Expandable Polystyrene
(discontinued **)
Extir E 3000 AE is a flame-retardant expandable polystyrene in the form of spherical beads of medium particle size, with a low pentane content as blowing agent. Extir does not contain CFC or HCFC. T..
|
|||
| Bulk Density | 0.590 - 0.630 g/cc | 0.0213 - 0.0228 lb/in³ | |
|
Polimeri Europa Extir® E 5000 AE Expandable Polystyrene
(discontinued **)
Extir E 5000 AE is a flame-retardant expandable polystyrene in the form of spherical beads of medium-large particle size, with a low pentane content as blowing agent. Extir does not contain CFC or H..
|
|||
| Bulk Density | 0.590 - 0.630 g/cc | 0.0213 - 0.0228 lb/in³ | |
|
Polimeri Europa Extir® F 1111 Expandable Polystyrene
(discontinued **)
Extir F 1111 is an expandable polystyrene in the form of spherical beads of very fine particle size and a narrow particle size distribution, containing pentane as blowing agent. Extir does not cont..
|
|||
| Bulk Density | 0.590 - 0.630 g/cc | 0.0213 - 0.0228 lb/in³ | |
|
Polimeri Europa Extir® P 1212 Expandable Polystyrene
(discontinued **)
Extir P 1212 is an expandable polystyrene in the form of spherical beads of very fine particle size and narrow distribution, containing pentane as blowing agent. Extir does not contain CFC or HCFC. ..
|
|||
| Bulk Density | 0.570 - 0.630 g/cc | 0.0206 - 0.0228 lb/in³ | After drying at 110°C |
|
Gouda Vuurvast GOLITE 1.0.6. Mix Refractory Insulating Castable
Description: This castable is composed of a high quality alumina cement and vermiculite and is applied as a backlining. Special additives are responsible for the low shrinkage. This castable can be ..
|
|||
| Bulk Density | 0.590 - 0.630 g/cc | 0.0213 - 0.0228 lb/in³ | |
|
Polimeri Europa Extir® D 5000 AE Expandable Polystyrene - Flame Retardant
Product Description:Extir D 5000 AE is a flame-retardant expandable polystyrene in the form of spherical beads of medium-large particle size, containing pentane as blowing agent.Extir does not conta..
|
|||
| Bulk Density | 0.590 - 0.630 g/cc | 0.0213 - 0.0228 lb/in³ | |
|
Polimeri Europa Extir® EH 5000 Expandable Polystyrene
Extir EH 5000 is an expandable polystyrene in the form of spherical beads of medium-large particle size, with a low pentane content as blowing agent. Extir does not contain CFC or HCFC. This grade i..
|
|||
| Bulk Density | 0.590 - 0.630 g/cc | 0.0213 - 0.0228 lb/in³ | |
|
Polimeri Europa Extir® LN 2000 Expandable Polystyrene
Extir LN 2000 belongs to a new expandable product family, the Leonardo Series, with improved processing features: high expandability, high moulding productivity, wide processing area, optimal fusion..
|
|||
| Bulk Density | 0.590 - 0.630 g/cc | 0.0213 - 0.0228 lb/in³ | |
|
Polimeri Europa Extir Leonardo A 2000 AE Expandable Polystyrene
(discontinued **)
Extir A 2000 AE is a flame retardant expandable polystyrene in the form of spherical beads of fine particle size, containing pentane as blowing agent. Extir does not contain CFC or HCFC. Extir A 200..
|
|||