Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Bulk Density = 0.641 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Bulk Density 0.641 g/cc
0.0231 lb/in³
packed
Imerys Minsparâ„¢ 10 Ground Feldspar
Minsparâ„¢ 10 is a fine particle size, ground Feldspar with a tightly controlled particle size distribution. Minsparâ„¢ 10 is easily dispersed to a high Hegman grind to produce coatings finish..
Bulk Density 0.641 g/cc
0.0231 lb/in³
loose
Imerys Minsparâ„¢ 4 Ground Feldspar
Minsparâ„¢ 4 is a medium particle size, ground Feldspar with a tightly controlled particle size distribution. The small amount of material retained on a 325 mesh screen, in conjunction with excel..
Bulk Density 0.641 g/cc
0.0231 lb/in³
loose
Imerys Minsparâ„¢ 7 Ground Feldspar
Minsparâ„¢ 7 is a fine particle size, ground Feldspar with a tightly controlled particle size distribution. Minsparâ„¢ 7 is easily dispersed to a high Hegman grind to produce coatings with hig..
Bulk Density 0.641 - 0.721 g/cc
0.0231 - 0.0260 lb/in³
Green Dot Terratek® SC 50 Polypropylene - Wheat Starch Biocomposite
Terratek® SC 50 is a proprietary blend of wheat starch and polypropylene for injection molding applications. SC 50 contains 50% wheat starch by weight, however, a range of properties can be achie..
Bulk Density 0.641 - 0.721 g/cc
0.0231 - 0.0260 lb/in³
Green Dot Terratek® SC 65 Polypropylene - Wheat Starch Biocomposite
Terratek® SC 65 is a proprietary blend of wheat starch and polypropylene for injection molding applications. SC 65 contains 65% wheat starch by weight, however, a range of properties can be achie..
Bulk Density 0.641 - 0.721 g/cc
0.0231 - 0.0260 lb/in³
Loose
KaMin Polyplate® HMT Kaolin Clay - Delaminated
Polyplate® HMT is a high brightness, very high aspect ratio, delaminated kaolin, intended for use in water-borne coatings, adhesives, and sealants. The large, platy structure of Polyplate® HMT..
Bulk Density 0.641 - 0.753 g/cc
0.0231 - 0.0272 lb/in³
Loose
KaMin Polyplate® P Kaolin Clay - Delaminated
Polyplate® P is a high brightness, delaminated clay intended for use in latex paints, water flexography inks, water-based adhesives or water-based systems where increased hiding, tinting strength..
Bulk Density 0.641 - 0.753 g/cc
0.0231 - 0.0272 lb/in³
Loose
KaMin Polyfil® DL Kaolin Clay - Delaminated
Large, platy delaminated clay that reduces gas/vapor permeability, spray dried bead form.Industry: Rubber & PlasticUses: Non-Black Rubber, Tire, General Rubber Goods, Butyl Rubber, MasterBatchInform..
Bulk Density 0.641 - 0.721 g/cc
0.0231 - 0.0260 lb/in³
Loose
KaMin Polyfil® DLX Kaolin Clay - Delaminated
Polyfil DLX is a large particle size, very high aspect ratio, delaminated clay that reduces gas and vapor permeability. It is a type of water washed clay which is processed to have a high aspect rat..
Bulk Density 0.641 - 0.705 g/cc
0.0231 - 0.0255 lb/in³
loose
CIMBAR CAL-BEN™ Calcium Bentonite
Selectively mined calcium bentonite, specially blended and processed for general industrial use. It is tan to yellowish in color and comes in the form of a fine powder.Incorporation:Can be base exc..
Bulk Density 0.641 g/cc
0.0231 lb/in³
Loose
CIMBAR NANO-FLEX® Talc - D for TPO Applications
NANO-FLEX® Talc is designed for use in high performance TPO applications that require high brightness and an high balance of stiffness and toughens. NANO-FLEX® Talc is made by a proprietary proces..