Polymer Property : Bulk Density = 3.21 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Bulk Density 3.21 g/cc
0.116 lb/in³
Chosun Refractories AB10H Alumina Magnesia Carbon Bricks for Ladle Wall And Bottom
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).