| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Particle Size | 18 µm | 18 µm | median; Microtrac |
|
Nyco NYGLOS® 12 Wollastonite
High aspect ratio grade. This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctiv..
|
|||
| Particle Size | 18 µm | 18 µm | d50 |
|
Magyar Aluminum ALOLT 730 Aluminum Hydroxide
Viscosity Optimized Type
|
|||
| Particle Size | 18 µm | 18 µm | D50 |
|
Malvern Minerals Wollastokup® FF Silane Treated Wollastonite
Wollastokup® is a custom, silane treated calcium metasilicate (wollastonite) which is used as a functional filler in coatings, plastics, rubber and others due in part to its acicular or “too..
|
|||
| Particle Size | 18 - 22 µm | 18 - 22 µm | 10% |
|
H.C. Starck Amperit® 105.074 Agglomerated Sintered Molybdenum (Mo) |
|||
| Particle Size | 18 - 22 µm | 18 - 22 µm | 10% |
|
H.C. Starck Amperit® 526.074 Agglomerated, Sintered Tungsten Carbide-Cobalt (WC-Co) 83-17 |
|||
| Particle Size | 18 - 22 µm | 18 - 22 µm | 10% for WC-Co 83-17 |
|
H.C. Starck Amperit® 560.062 Tungsten Carbide-Cobalt(83-17)-Nickel-SF RC 60 50-50 (Wc-Co / NiSF RC 60)
Composition is of NiSF RC 60 only
|
|||
| Particle Size | 18 - 24 µm | 18 - 24 µm | 50% |
|
H.C. Starck Amperit® 588.059 Chromium Carbide-Nickel Chromium 75-25 (Cr3C2-NiCr) |
|||
| Particle Size | 18 µm | 18 µm | |
|
Silberline 4-Allâ„¢ E2778
The 4-Allâ„¢ series of passivated aluminum pigments is designed for use in waterborne automotive and industrial coatings. In the 4-Allâ„¢ system, the aluminum pigment is passivated using a pr..
|
|||
| Particle Size | 18 µm | 18 µm | |
|
Silberline Aquasil® "BP" 5745
Silberline has specifically created Aquasil® BP grades for aqueous architectural and industrial maintenance coatings. This family offers a cost-effective alternative for achieving stability and ..
|
|||
| Particle Size | 18 µm | 18 µm | |
|
Silberline Sparkle Silver® 5251-AR
Sparkle Silver® 5251-AR is a medium particle size, bright, non-leafing aluminum pigment with a smooth patina. It provides exceptional brightness and is acid resistant.Applications: Automotive
|
|||
| Particle Size | 18 µm | 18 µm | |
|
Silberline Sparkle Silver® Premier 331AR
Sparkle Silver® Premier flakes provide more uniform surfaces than Sparkle Silver® products, and also sharper edges and controlled particle size distribution. "Sparkle Silver® Premier or Sil..
|
|||
| Particle Size | 18 µm | 18 µm | |
|
Silberline Sparkle Silver® Premier 404AR
Sparkle Silver® Premier flakes provide more uniform surfaces than Sparkle Silver® products, and also sharper edges and controlled particle size distribution. "Sparkle Silver® Premier or Sil..
|
|||
| Particle Size | 18 µm | 18 µm | |
|
Silberline Tufflake® 3620
Tufflake® aluminum pigments are circulation-resistant, specifically designed to withstand mechanical forces and maintain their target appearance. They are primarily used in automotive coating app..
|
|||
| Particle Size | 18 µm | 18 µm | d90 |
|
TIMCAL TIMREX® MB15 Primary Synthetic Graphite
TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro..
|
|||
| Particle Size | 18 - 22 µm | 18 - 22 µm | Average; ATO 40-41-0 (Coulter Counter) |
|
Arkema Group ORGASOL® 2002 D Nat 1 Polyamide 12, Food Contact Approved
Information provided by Arkema Group
|
|||
| Particle Size | 18 - 24 µm | 18 - 24 µm | D(0.5) |
|
Akzo Nobel Expancel® 009 DU 80 Dry unexpanded microspheres
Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the..
|
|||
| Particle Size | 18 - 24 µm | 18 - 24 µm | D(0.5) |
|
Akzo Nobel Expancel® 091 DU 80 Dry unexpanded microspheres
Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the..
|
|||
| Particle Size | 18 - 28 µm | 18 - 28 µm | D(0.5) |
|
Akzo Nobel Expancel® 551 DE 20 d60 Dry expanded microspheres
Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the..
|
|||
| Particle Size | 18 - 24 µm | 18 - 24 µm | D(0.5) |
|
Akzo Nobel Expancel® 551 DU 80 Dry unexpanded microspheres
Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the..
|
|||
| Particle Size | 18 - 24 µm | 18 - 24 µm | D(0.5) |
|
Akzo Nobel Expancel® 551 WU 80 Wet unexpanded microspheres
Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the..
|
|||
| Particle Size | 18 - 24 µm | 18 - 24 µm | D(0.5) |
|
Akzo Nobel Expancel® 950 DU 80 Dry unexpanded microspheres
Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the..
|
|||
| Particle Size | 18 - 24 µm | 18 - 24 µm | D(0.5) |
|
Akzo Nobel Expancel® 092 DU 80 Dry unexpanded microspheres
Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the..
|
|||
| Particle Size | 18 - 24 µm | 18 - 24 µm | D(0.5) |
|
Akzo Nobel Expancel® 091 WU 80 Wet unexpanded microspheres
Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the..
|
|||
| Particle Size | 18 - 24 µm | 18 - 24 µm | 50% |
|
H.C. Starck Amperit® 529.053 Tungsten Carbide - Hastalloy C 85-15 (NiMoCrFeCo) |
|||