| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Particle Size | 25 µm | 25 µm | Median Diameter |
|
Omya TITAN® 200 - LU Calcium Carbonate
An intermediate, dry ground calcium carbonate with a closely controlled particle size distribution.Applications: For use in latex compounds.Information supplied by Omya North America.
|
|||
| Particle Size | 25 µm | 25 µm | D<sub>50</sub>; ISO 13320-1 |
|
Victrex® PEEK 150XF Polyetheretherketone, Unreinforced
Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, fine powder for compression moulding, easy flow, FDA food contact compliant, ..
|
|||
| Particle Size | 25 µm | 25 µm | Geon® DFT 1466; Internal Method |
|
PolyOne Geon™ 210 Series 215 Blending Resin Polyvinyl Chloride Homopolymer (PVC Homopolymer)
Geon® 215 is a low molecular weight particle size homopolymer blending resin intended for use in plastisol formulations. It improves air release performance resulting in reduced scrap rates. It dec..
|
|||
| Particle Size | 25 µm | 25 µm | ASTM D4894 |
|
3M Dyneon™ CCX1029 PTFE, 10% Carbon Fiber Filled
(discontinued **)
Type I, non-free-flowing.Typical Applications: Finished or semi-finished parts: sheets, rods, tubes, billets for skiving of films or machining into complex shapes.Information provided by the Dyneon ..
|
|||
| Particle Size | 25 µm | 25 µm | median |
|
3M Dyneon™ PFA 6503 A EPC Perfluoroalkoxy Fluorothermoplastic
(discontinued **)
Dyneon PFA 6503 A EPC is a fluorothermoplastic powder for powder coating applications, and is designed for thin film applications where target film thickness is 25-40 micrometers per pass.non-stick ..
|
|||
| Particle Size | 25 µm | 25 µm | median |
|
3M Dyneon™ PFA 6503 C EPC Perfluoroalkoxy Fluorothermoplastic
(discontinued **)
Dyneon PFA 6503 C EPC is a fluorothermoplastic powder for powder coating applications, and is designed for thin film applications where target film thickness is 25-40 micrometers per pass.non-stick ..
|
|||
| Particle Size | 25 µm | 25 µm | ASTM D4894 |
|
3M Dyneon™ CC191-HE Custom Fluoropolymer Compound
(discontinued **)
This compound consists of a mixture of high elongation 23% carbon / 2% graphite blended with PTFE.Information provided by Dyneon, A 3M Company
|
|||
| Particle Size | <= 25 µm | <= 25 µm | |
|
Ferro EG 0026 Glaze and Sealant Glass
Glass Type: Ca-B-Al-Si Typical Powder Form: MVG Typical Application: Al2O3 Ferro's electronic and specialty glass group has produced over 3,000 formulations. Many are used as protective and insul..
|
|||
| Particle Size | <= 25 µm | <= 25 µm | MVG Powder |
|
Ferro EG 0225 Specialty Glass
Glass Type: MG-Al-Si (devitrified) Typical Powder Form: MVG, SRRG Typical Application: Sintering Aid / Ceramic Ferro offers a wide range of compositions for specialty applications including sinteri..
|
|||
| Particle Size | <= 25 µm | <= 25 µm | |
|
Ferro EG 2778 Thick Film Glass
Glass Type: Si-Al-Ca Typical Powder Form: MVG Typical Application: Dielectric Ferro produces standard and custom glass products that are used in thick film compositions including resistors, conduct..
|
|||
| Particle Size | <= 25 µm | <= 25 µm | RWG Powder |
|
Ferro IP 780 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates)
Glass Type: Pb-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to a..
|
|||
| Particle Size | <= 25 µm | <= 25 µm | RWG Powder |
|
Ferro IP 820 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates)
Glass Type: Pb-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to a..
|
|||
| Particle Size | <= 25 µm | <= 25 µm | RWG Powder |
|
Ferro IP 830 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates)
Glass Type: Pb-B-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to..
|
|||
| Particle Size | <= 25 µm | <= 25 µm | RWG Powder |
|
Ferro IP 900 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates)
Glass Type: Si-Pb-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to a..
|
|||
| Particle Size | 25 - 35 µm | 25 - 35 µm | d50 |
|
Magyar Aluminum ALOLT 21AF Aluminum Hydroxide
Ground type
|
|||
| Particle Size | 25 - 35 µm | 25 - 35 µm | 90% |
|
H.C. Starck Amperit® 250.071 Water Atomized (NiCr 80-20) |
|||
| Particle Size | 25 - 29 µm | 25 - 29 µm | 90% |
|
H.C. Starck Amperit® 281 Gas Atomized (NiAl 95-5) |
|||
| Particle Size | 25 - 35 µm | 25 - 35 µm | |
|
Lucite International Colacryl ® B611 Acrylic Dental Resin
Cold-curing denture repair resin with Methyl Methacrylate based copolymers. Features fast polymerisation, easy mixing, good clarity, short hydroflask cure cycles, and excellent pigment acceptance.I..
|
|||
| Particle Size | <= 25 µm | <= 25 µm | |
|
Ferro EG 0002 Glazes and Sealants
Glass Type: Si-Al-Ba Typical Powder Form: VWG Typical Application: SiC Ferro's electronic and specialty glass group has produced over 3,000 formulations. Many are used as protective and insulatin..
|
|||
| Particle Size | <= 25 µm | <= 25 µm | |
|
Ferro IP 530 Thick Film Glass
Glass Type: Pb-Si-B-Al Typical Powder Form: RWG Typical Application: General Ferro produces standard and custom glass products that are used in thick film compositions including resistors, conducto..
|
|||
| Particle Size | <= 25 µm | <= 25 µm | RWG Powder |
|
Ferro IP 730 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates)
Glass Type: Pb-B-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to..
|
|||
| Particle Size | 25 - 30 µm | 25 - 30 µm | Violet |
|
Solvay Chemicals Blue pigment
Information provided by Solvay
|
|||
| Particle Size | 25 µm | 25 µm | |
|
Silberline Sparkle Silvex® Premier 860-20-C
Sparkle Silvex® C grades are aluminum pigment flakes dampened with a plasticizer to help prevent the individual flakes from becoming airborne during handling and processing. They are well suited ..
|
|||
| Particle Size | 25 µm | 25 µm | |
|
UCAR Carbon UCAR® ATA Isostatic Molded Graphite
Economical grade ATA is the lowest density version of isostatically molded, fine grain grade ATJ family of graphite materials.Typical Applications: ATA is used in general purpose applications where ..
|
|||
| Particle Size | 25 µm | 25 µm | d90 |
|
TIMCAL TIMREX® MX25 Primary Synthetic Graphite
TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro..
|
|||
| Particle Size | 25 µm | 25 µm | 10th% |
|
3M S15 Glass Bubbles
3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli..
|
|||
| Particle Size | 25 µm | 25 µm | ASTM D4894 |
|
3M Dyneon™ TFM™ 1700 Modified PTFE Powder
Type III, gr. 1 PTFE. Dyneon™ TFM™ 1700 PTFE is a second-generation modified polytetrafluoro-ethylene (PTFE) that maintains the exceptional chemical and heat resistance properties of first-genera..
|
|||
| Particle Size | 25 µm | 25 µm | |
|
Asahi Glass Fluon® G190 PTFE Granular Powder
Fluon®PTFE granular powders (molding powders) are used for the production of sheets, rods, billets and other general moldings.Information provided by Asahi Glass Company, Inc.
|
|||
| Particle Size | <= 25 µm | <= 25 µm | |
|
Chesterton 785 FG Parting Lubricant
Description: Chesterton® 785 FG Parting Lubricant represents the newest generation of food and pharmaceutical anti-seize compounds. A white soft-paste, formulated with proprietary blend of ultra-fi..
|
|||
| Particle Size | 25 µm | 25 µm | 95%, Laser diffraction; QSOP-5&75 |
|
Shamrock Technologies MicroFLON® 1437FG Thermoplastic Grade PTFE Additive
Used in high temperature engineering plastics; food contactThe addition of micronized polytetrafluoroethylene (PTFE) powder to polymeric resins provides greatly increased resistance to surface wear ..
|
|||