| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Particle Size | 27 µm | 27 µm | Mean |
|
Potters Industries Sphericel® 45P25 Hollow Engineered Glass Microspheres
Sphericel® hollow glass microspheres are alternatives to conventional fillers and additives such as silicas, calcium carbonates, talc, clay, etc. A variety of particle sizes, densities and strength..
|
|||
| Particle Size | 27 - 31 µm | 27 - 31 µm | 90% |
|
H.C. Starck Amperit® 554.071 Tungsten Carbide-Cobalt-Chromium 86-10-4 (WC-Co-Cr) |
|||
| Particle Size | 27 µm | 27 µm | |
|
Silberline 4-Allâ„¢ LEP 20061
The 4-Allâ„¢ series of passivated aluminum pigments is designed for use in waterborne automotive and industrial coatings. In the 4-Allâ„¢ system, the aluminum pigment is passivated using a pr..
|
|||
| Particle Size | 27 µm | 27 µm | |
|
Silberline Aquasil® "BP" 3500
Silberline has specifically created Aquasil® BP grades for aqueous architectural and industrial maintenance coatings. This family offers a cost-effective alternative for achieving stability and ..
|
|||
| Particle Size | 27 µm | 27 µm | |
|
Silberline Aquavet® 3500nl-136M
Aquavet® grades are aluminum pigment pellets designed for use in aqueous inks for flexographic and gravure printing. The pellets are composed of 80% aluminum pigment and 20% of a proprietary poly..
|
|||
| Particle Size | 27 µm | 27 µm | |
|
Silberline Dedusted Flake Series DF-3500 Aluminum Flake
DF-3500 Dedusted Aluminum Flake is manufactured by incorporating a small amount of Teflonâ„¢ with an uncoated aluminum pigment, and then, through further processing, is provided in a dry, non-dus..
|
|||
| Particle Size | 27 µm | 27 µm | Before Conversion |
|
Silberline Silvet® 880-20-P
Silvet® P grades are recommended for use with engineering resins or transparent polymers where compatibility, maintenance of polymer clarity and distinctiveness of image (D.O.I.) observed from th..
|
|||
| Particle Size | 27 µm | 27 µm | Before Conversion |
|
Silberline Sparkle Silvet® 880-30-E1
Sparkle Silvet® E1 grades are easy to disperse and are compatible with a variety of polymers, particularly polyolefins. They are typically used to make concentrates or compounds for use in final ..
|
|||
| Particle Size | 27 µm | 27 µm | |
|
Silberline Sparkle Silvex® 883-20-C
Sparkle Silvex® C grades are aluminum pigment flakes dampened with a plasticizer to help prevent the individual flakes from becoming airborne during handling and processing. They are well suited ..
|
|||
| Particle Size | 27 µm | 27 µm | |
|
Silberline Sparkle Silvex® 885-20-D
Sparkle Silvex® D grades are aluminum pigment flakes dampened with a plasticizer to help prevent the individual flakes from becoming airborne during handling and processing. They are well suited ..
|
|||
| Particle Size | 27 µm | 27 µm | |
|
Silberline Sparkle Silver® 3500
Sparkle Silver® 3500 is a medium, non-leafing aluminum pigment. It was developed to provide formulators of industrial finishes with an economical source of sparkling aluminum flake. It is widely ..
|
|||
| Particle Size | 27 µm | 27 µm | d90 |
|
TIMCAL TIMREX® MB25 Primary Synthetic Graphite
TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro..
|
|||
| Particle Size | 27 µm | 27 µm | @ 98% |
|
CIMBAR Gel Talc for Polyester Filler
Gel Talc and Body Filler talc products are produced from high purity ore. Gel Talc and Body Filler products provide an excellent balance of color and mechanical properties for primary use in polyes..
|
|||
| Particle Size | 27 µm | 27 µm | @ 98%; Micrometrics Sedigraph 5100 |
|
CIMBAR RP 9305 Talc
RP 9300 Series talcs are produced from high purity ores, which provide an excellent balance of color and mechanical properties, for primary use in commodity polypropylene and polyester compounds. R..
|
|||
| Particle Size | 27 µm | 27 µm | Before Conversion |
|
Silberline Sparkle Silvet® 880-20-E
Sparkle Silvet® E grades are economical aluminum pigments provided in pellet form for easy handling and incorporation. They are composed of 80% aluminum pigment and 20% polyolefin and are compatibl..
|
|||