Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Particle Size 25 - 29 µm
25 - 29 µm
90%
H.C. Starck Amperit® 251 Gas Atomized (NiCr 80-20)
Particle Size 25 - 29 µm
25 - 29 µm
90%
H.C. Starck Amperit® 281 Gas Atomized (NiAl 95-5)