Physical Properties Metric English Comments
Particle Size 4.0 µm
4.0 µm
median; Microtrac
Nyco 10 WOLLASTOCOAT® Wollastonite
Chemically treated grade. This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctiv..
Particle Size 4.0 µm
4.0 µm
median; Microtrac
Nyco M1250 AS WOLLASTOCOAT® Wollastonite
Chemically treated grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal per..
Particle Size >= 4.0 µm
>= 4.0 µm
10% smaller than
Nyco M200 WOLLASTOCOAT® Wollastonite
Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br..
Particle Size 4.0 µm
4.0 µm
median; Microtrac
Nyco MD1250 WOLLASTOCOAT® Wollastonite
Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br..
Particle Size >= 4.0 µm
>= 4.0 µm
10% smaller than
Nyco NYAD® MD200 Wollastonite
Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br..
Particle Size >= 4.0 µm
>= 4.0 µm
10% smaller than
Nyco NYGLOS® 8 Wollastonite
This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology make..
Particle Size 4.0 µm
4.0 µm
mean aggregate size
NanoScale NanoActive® Calcium Oxide
NanoActive CaO is produced using proprietary processes to obtain high specific surface area (over 20 m²/g vs. 1-2 m²/g for standard CaO) with strong affinity towards carbon dioxide and hydrogen su..
Particle Size 4.0 µm
4.0 µm
mean aggregate size
NanoScale NanoActive® Calcium Oxide Plus
NanoActive CaO Plus is produced using proprietary processes to obtain high specific surface area (over 90 m²/g vs. 1-2 m²/g for standard CaO), small crystallite size material possessing high chemi..
Particle Size 4.0 µm
4.0 µm
mean aggregate size
NanoScale NanoActive® Zinc Oxide
NanoActive ZnO is produced using proprietary processes to obtain high specific surface area, small crystallite size material that can be dispersed in various carrier fluids with significantly reduce..
Particle Size <= 4.0 µm
<= 4.0 µm
Poco Graphite EDM-4 EDM Graphite
POCO's EDM-4 is our premier offering in the Ultrafine classification. This highly isotropic grade combines strength with moderate hardness, yielding superior electrode fabrication characteristics. T..
Particle Size 4.0 µm
4.0 µm
50% of particles, (RWG Powder)
Ferro IX 2443 Passivation Glasses - High Voltage (Zn-B-Silicates)
Typical Powder Form: RWG, DSD Zinc-Boro-Silicate passivation glasses are used for hermetic passivation of high voltage diodes, thyristors, and transistors. They provide high junction temperatures a..
Particle Size 4.0 - 7.0 µm
4.0 - 7.0 µm
d50
Magyar Aluminum ALO-DN-4S Alumina
Ground Alumina
Particle Size 4.0 - 7.0 µm
4.0 - 7.0 µm
d50
Magyar Aluminum ALO-G4-4G Alumina
Ground Alumina
Particle Size 4.0 µm
4.0 µm
average
Inhance Fluoro-Seal INHANCE® Si-8900 Polymer Alloy
Product Description: INHANCE S i-8000 series polymer alloy consists of black, medium density, silicon carbide chemically modified for greater adhesion. This product was designed for alloying with v..
Particle Size <= 4.0 µm
<= 4.0 µm
Main Break; Fineness of Grind
Gwent Electronic Materials C2010829D2 Silver Ink
Silver Ink C2010829D2 is a high definition silver ink for LTCC tape. It is compatible with other members of the GEM range of Silver LTCC Inks and most LTCC tape systems on the market.The ink has be..
Particle Size <= 4.0 µm
<= 4.0 µm
Average Particle Size/Laser Diffraction D50
H.C. Starck Grade A Yttrium Oxide
Sintering additive for Si3N4 and AlNStabilizer for zirconias (PSZ) and insulating coatings (TBC`s)Catalyst carrierYttria stabilized zirconias electrolytes for solid oxide fuel cellsLuminescent mater..
Particle Size <= 4.0 µm
<= 4.0 µm
Average Particle Size/Laser Diffraction D50
H.C. Starck Grade AT Yttrium Oxide
Sintering additive for Si3N4 and ALNStabilizer for zirconias (PSZ) and insulating coatings (TBC`s)Catalyst carrierYttria stabilized zirconias electrolytes for solid oxide fuel cellsLuminescent mater..
Particle Size 4.0 - 8.0 µm
4.0 - 8.0 µm
D 50%; Laser Light Diffraction per ASTM C1070
H.C. Starck Type I Pure Molybdenum MIMP Powder
Description of Product: Highly deagglomerated high purity molybdenum powder for any applications requiring the most finely deagglomerated powders like paste or metal injection molding applications...
Particle Size 4.0 µm
4.0 µm
Solvay Chemicals Blanc fixe G
Blanc Fixe G is an extender for almost all applications in the production of paints and coatings and plasticInformation provided by Solvay
Particle Size 4.0 - 5.0 µm
4.0 - 5.0 µm
Median Grain (d50)
CeramTec Alunit® Aluminum Nitride
Alunit® offers an extremely high thermal conductivity of 180 W/mK and outstanding electrical insulation properties. The thermal expansion coefficient of this material is comparable to silicon. Its ..
Particle Size 4.0 - 5.0 µm
4.0 - 5.0 µm
Medium Grain (d50)
CeramTec Alunit® HS Aluminum Nitride
Alunit® HS offers an extremely high thermal conductivity of 170 W/mK and outstanding electrical insulation properties. The thermal expansion coefficient of this material is comparable to silicon. I..
Particle Size 4.0 - 7.0 µm
4.0 - 7.0 µm
Grain Size; Intercept Method
CoorsTek ADS-96R 96% Alumina Thick Film Substrate
This high-purity material ensures strong, reliable performance for ceramic substrate application. Applications: thick films and lasers
Particle Size 4.0 µm
4.0 µm
Median
Excalibar ExBar™ W 4 Barite BaSO4 Powder
ExBar™ W high-purity white barytes are manufactured using only the highest quality white, natural barium sulfate ore. Strict quality control results in consistent products that are used in paints, ..
Particle Size 4.0 µm
4.0 µm
China Tungsten YG15 Tungsten Carbide Powder
Information provided by China Tungsten
Particle Size 4.0 - 7.0 µm
4.0 - 7.0 µm
Chesterton 725 Nickel Anti-Seize Compound
Description: Chesterton® 725 Nickel Anti-Seize Compound is an assembly lubricant combining the extreme pressure, corrosion resistant anti-seize abilities of colloidal nickel, aluminum and graphite ..
Particle Size 4.0 - 7.0 µm
4.0 - 7.0 µm
Chesterton 772 Premium Nickel Anti-Seize Compound
Description: Chesterton® 772 Premium Nickel Anti-Seize Compound is formulated with ultra pure raw materials. This permits 772 Premium Nickel Anti-Seize Compound to conform to most applicable equipm..
Particle Size 4.0 - 6.0 µm
4.0 - 6.0 µm
Mean particle size
Carborundum CarboTherm™ CTUF Boron Nitride Powder
Boron Nitride powders have high thermal conductivity, low dielectric loss, and low thermal expansion. They are non-abrading to electronic components, lubricious, non-toxic, and retain their dielect..
Particle Size 4.0 µm
4.0 µm
50&quot; Percentile
3M W-410 Ceramic Microspheres
3M™ White Ceramic Microspheres are unique, semi-transparent, white-colored, fine particle size, high-strength microspheres. These products are typically used to reduce VOC levels; increase filler l..