| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Particle Size | <= 40 µm | <= 40 µm | 90% smaller than |
|
Nyco NYAD® 325 Wollastonite
Powdered grade. This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particl..
|
|||
| Particle Size | <= 40 µm | <= 40 µm | 90% smaller than |
|
Nyco NYGLOS® 8 Wollastonite
This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology make..
|
|||
| Particle Size | <= 40 µm | <= 40 µm | 90% smaller than |
|
Nyco NYGLOS® STPO Wollastonite
This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology make..
|
|||
| Particle Size | <= 40 µm | <= 40 µm | 90% smaller than |
|
Nyco RRIMGLOS® II Wollastonite
This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology make..
|
|||
| Particle Size | 40 µm | 40 µm | mesh. |
|
Oceanchem Group Sodium Formate 95-96% powder
Molecular Formula: NaCOOHInformation Provided by Oceanchem Group
|
|||
| Particle Size | 40 µm | 40 µm | Average Diameter |
|
Potters Industries Conduct-O-Fil® SA300S20 Silver-coated Aluminum Granules
Applications:EMI shielding in contact with aluminumConductive adhesivesAerospace and marine applicationsAdvantages:Low density with high conductivityLow galvanic corrosion in contact with aluminumIn..
|
|||
| Particle Size | 40 µm | 40 µm | Average Diameter |
|
Potters Industries Conduct-O-Fil® SC230F9.5 Silver-coated Copper Particles
Applications EMI shielding, conductive adhesives, conductive paints and coatings. Advantages: Most conductive combination of metals; Dendrites give excellent compression set in FIP gaskets; Flakes ..
|
|||
| Particle Size | 40 - 50 µm | 40 - 50 µm | Average; for inner type spray system; Microtrac HRA |
|
NYC YT3WBHQ Y2O3 Powder for Spray Coating
High purity granules produced in clean environment. Uses include semiconductor / LCD industries and electroceramics.Narrow particle size distributionTailorable for each spray coating technologyNo c..
|
|||
| Particle Size | 40 - 70 µm | 40 - 70 µm | d50 |
|
Magyar Aluminum ALO-DFC Alumina
Alumina for Polishing
|
|||
| Particle Size | 40 µm | 40 µm | |
|
Silberline Sparkle Silver® 3624
Sparkle Silver® 3624 is a coarse, brilliant, regular purity, non-leafing aluminum pigment popular for solvent-based general industrial coatings. This pigment can be used with tints to produce a w..
|
|||
| Particle Size | 40 µm | 40 µm | at a density of 2.10 g/cc, pressure 2.5 t/cc |
|
TIMCAL TIMREX® GB99/6 Natural Graphite
TIMREX Natural Flake Graphite is produced in a wide range of products distinguished by particle size distribution, chemistry and carbon content. Timcal mines the graphite from its own source in Lac-..
|
|||
| Particle Size | 40 - 51.5 µm | 40 - 51.5 µm | d90, Guaranteed |
|
TIMCAL TIMREX® KS44 Primary Synthetic Graphite
TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro..
|
|||
| Particle Size | 40 - 55 µm | 40 - 55 µm | d90, Guaranteed |
|
TIMCAL TIMREX® LSG 44 Natural Graphite Flakes
TIMREX Natural Flake Graphite is produced in a wide range of products distinguished by particle size distribution, chemistry and carbon content. Timcal mines the graphite from its own source in Lac-..
|
|||
| Particle Size | 40 µm | 40 µm | Laser Method (Dry) |
|
Daikin POLYFLON M-112 PTFE Molding Powder, Fine Cut
Fine cut powder.Processing Methods: Compression molding.Features: Produces moldings with especially good elasticity, making it ideal for molding diaphragms and bellows. Offers excellent post-moldin..
|
|||
| Particle Size | <= 40 µm | <= 40 µm | |
|
Epoxy Technology EPO-TEK® 337H Graphite-Filled, High Temperature Epoxy
Product Description: EPO-TEK® 377H is a two component, high Tg, graphite filled epoxy designed for ESD/EMI shielding of semiconductor devices and electronics. It can be used in many electronic ind..
|
|||
| Particle Size | <= 40 µm | <= 40 µm | Max |
|
CIMBAR Miti-Wite B10 Chemically Purified White Barite (BaSO4)
Miti-Wite barite products are produced using a proprietary chemical process to enhance the purity of the natural barium sulfate ore. Miti-Wite products are available in a variety of particle sizes ..
|
|||
| Particle Size | 40 µm | 40 µm | D90 |
|
Dandong Taico Minerals TAICOCITE® TC3 Magnesium Hydroxide
Made from local natural brucite minerals, TAICOCITE® is the name of milled magnesium hydroxide products which is produced (micronized/surface treated) by Dandong Taico Minerals Co., Ltd. TAICOCITE®..
|
|||
| Particle Size | <= 40 µm | <= 40 µm | Max |
|
CIMBAR CIMBAR™ 325 Barite Powder (BaSO4)
CIMBAR barite products are made using only the highest quality white, natural barium sulfate ore. CIMBAR barites unique properties of fine grind, high specific gravity, low solubility and chemical ..
|
|||
| Particle Size | 40 µm | 40 µm | Average |
|
Azoty Tarnow™ TARFLEN SM-1 PTFE
Non Free-Flowing suspension powder for standard compression molding and compounding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
|
|||
| Particle Size | 40 µm | 40 µm | Average |
|
Azoty Tarnow™ TARFLEN SM-B30 PTFE
Reinforced with 30% bronze for standard compression molding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
|
|||
| Particle Size | 40 µm | 40 µm | Average |
|
Azoty Tarnow™ TARFLEN SM-G15 PTFE
Tarflen SM1 reinforced with 15% graphite for standard compression molding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
|
|||
| Particle Size | 40 µm | 40 µm | Average |
|
Azoty Tarnow™ TARFLEN SM-G20 PTFE
Reinforced with 20% graphite for standard compression molding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
|
|||
| Particle Size | 40 µm | 40 µm | Average |
|
Azoty Tarnow™ TARFLEN SM-S15 PTFE
15% glass fiber reinforced for standard compression molding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
|
|||
| Particle Size | 40 µm | 40 µm | Average |
|
Azoty Tarnow™ TARFLEN SM-S15G2 PTFE
Tarflen SM1 reinforced with 15% glass fibers and 2% graphite for standard compression molding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
|
|||
| Particle Size | 40 µm | 40 µm | Average |
|
Azoty Tarnow™ TARFLEN SM-S25 PTFE
Tarflen SM1 reinforced with 25% glass fiber for standard compression molding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
|
|||
| Particle Size | 40 µm | 40 µm | Average D50; Laser Diffraction |
|
ALM PA 250 Nylon 12 SLS Prototyping Polymer
Highly Recyclable Nylon 12 Laser Sintering Material.Engineered for excellent mechanical properties, part definition and surface finish. Stabilized against thermal degradation resulting in little or..
|
|||
| Particle Size | 40 µm | 40 µm | Effective Top Size |
|
3M iM16K Glass Bubbles
3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli..
|
|||
| Particle Size | 40 µm | 40 µm | 50th% |
|
3M S35 Glass Bubbles
3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli..
|
|||
| Particle Size | <= 40 µm | <= 40 µm | 90% smaller than |
|
Nyco ULTRAFIBRE® II Wollastonite
Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br..
|
|||
| Particle Size | 40 µm | 40 µm | Average Diameter |
|
Potters Industries Conduct-O-Fil® SM40P20 Silver-coated Magnetic Particles