Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Particle Size = 5.0 µm Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Particle Size >= 5.0 µm
>= 5.0 µm
10% smaller than
Nyco ASPECT® 4000 Wollastonite
ASPECT 4000 is available untreated or with a surface modification treatment.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive ..
Particle Size 5.0 µm
5.0 µm
Poco Graphite AXF-5F Biomedical Grade Graphite
POCO has developed post synthesis modifications to make our graphites more suitable to specific conditions. As a producer of highly technical, specialty materials, POCO also offers design engineerin..
Particle Size 5.0 µm
5.0 µm
Poco Graphite AXZ-5Q Industrial Grade Graphite
POCO’s specialty graphite materials are used in a wide range of highly technical and industrial applications. Each grade has characteristics and properties that allow the user to match the ideal gr..
Particle Size <= 5.0 µm
<= 5.0 µm
Grade I
Oceanchem Group Decabromodiphenyl Oxide (DECA/DBDPO)
Molecular Formula: C12Br10OCas No.: 1163-19-5Characteristics: White powder, no poison, no smell and noncorrosion. Indissolvable in water, ethyl alcohol, acetone, benzene, arene chloride.Use: It is ..
Particle Size <= 5.0 µm
<= 5.0 µm
84% of particles less than
Old Hickory Dunn Tennessee Ball Clay
Dunn clay is a selection originating from our Gleason, TN processing facility and is characterized by moderately high levels of kaolin interspersed with the presence of some carbon content. It is an..
Particle Size <= 5.0 µm
<= 5.0 µm
89% of particles less than
Old Hickory MCB-11 Tennessee Ball Clay
A clay with excellent kaolin content and virtually no carbon content. It is highly plastic with excellent fired brightness and is an excellent clay for a variety of ceramic glaze and porcelain compo..
Particle Size <= 5.0 µm
<= 5.0 µm
86% of particles less than
Old Hickory No. 5 Kentucky Ball Clay
No. 5 clay is a kaolinitic ball clay containing low levels of carbon. It provides high suspension and plasticity to a variety of ceramic formulations and is an excellent source of Al2O3 content. No...
Particle Size <= 5.0 µm
<= 5.0 µm
PolyOne Aquamix™ 110 Latex
Storage Stability: In excess of 6 months when stored under proper conditions in original sealed container. Keep from freezing. Water lost by evaporation can adversely affect viscosity, dispersabilit..
Particle Size <= 5.0 µm
<= 5.0 µm
PolyOne Aquamix™ 568 Latex
Storage Stability: In excess of 6 months when stored under proper conditions in original sealed container. Keep from freezing. Water lost by evaporation can adversely affect viscosity, dispersabilit..
Particle Size 5.0 µm
5.0 µm
Poco Graphite AXF-5Q Industrial Grade Graphite
POCO’s specialty graphite materials are used in a wide range of highly technical and industrial applications. Each grade has characteristics and properties that allow the user to match the ideal gr..
Particle Size <= 5.0 µm
<= 5.0 µm
79% finer
Malvern Minerals Novakup® L-337 Surface-Treated Lamellar Quartz Filler/Extender
Novakup® is a surface modified or silane treated Novacite®. It has been used its barrier prosperities in chemical and corrosion resistant applications and as a filler/extender/reinforcing agen..
Particle Size 5.0 µm
5.0 µm
97% finer than
Imerys Bardenâ„¢ R Kaolin
Barden is a high surface area kaolin product used a filler in rubber and plastic applications.Information provided by Imerys
Particle Size >= 5.0 µm
>= 5.0 µm
trace
Imerys Minsparâ„¢ 1 Feldspar
Minspar 1 is a minus 30 mesh Feldspar product used in the glass container and ceramic tile markets.Information provided by Imerys
Particle Size 5.0 µm
5.0 µm
mean
Imerys Minsparâ„¢ 7 Ground Feldspar
Minsparâ„¢ 7 is a fine particle size, ground Feldspar with a tightly controlled particle size distribution. Minsparâ„¢ 7 is easily dispersed to a high Hegman grind to produce coatings with hig..
Particle Size <= 5.0 µm
<= 5.0 µm
Fineness of Grind
Gwent Electronic Materials C2050503D1 Curable Carbon Ink
This product is based on a unique curing process that results in the low temperature formation of a thermosetting conductive coating that combines good adhesion with excellent chemical, solvent and ..
Particle Size 5.0 µm
5.0 µm
mean; 99% -325 mesh
Momentive Performance Materials HCT-S Titanium Diboride (TiB2) Powder
Grade HCT-S powder can be cold-pressed and sintered into high density (98% of theoretical), near-net shapes.Titanium Diboride Powder Titanium Diboride (TiB2) is produced by GE Advanced Ceramics usi..
Particle Size 5.0 µm
5.0 µm
Mean
Momentive Performance Materials PolarTherm® PT132 Boron Nitride (BN) Powder
Boron Nitride powders are produced by GE Advanced Ceramics in more than 50 individual (standard and custom) grades to meet a wide variety of application needs.For use in: Electrically insulating/the..
Particle Size 5.0 - 9.0 µm
5.0 - 9.0 µm
10%
H.C. Starck Amperit® 251 Gas Atomized (NiCr 80-20)
Particle Size 5.0 µm
5.0 µm
Mean Value, Laser diffraction; QSOP-5&amp;75
Shamrock Technologies MicroFLON® 1253 Thermoplastic Grade PTFE Additive
Special grade for fine dispersion.The addition of micronized polytetrafluoroethylene (PTFE) powder to polymeric resins provides greatly increased resistance to surface wear and abrasion. PTFE has a..
Particle Size 5.0 µm
5.0 µm
Shin-Etsu Silicones X-52-1621 Fluid
Information Provided by Shin-Etsu Silicones of America, Inc.
Particle Size 5.0 µm
5.0 µm
at a density of 1.81 g/cc, pressure 2.5 t/cc
TIMCAL TIMREX® KS15 Primary Synthetic Graphite
TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro..
Particle Size 5.0 µm
5.0 µm
at a density of 1.81 g/cc, pressure at 2.5 t/cc
TIMCAL TIMREX® KS5-25 Primary Synthetic Graphite
TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro..
Particle Size 5.0 µm
5.0 µm
at a density of 1.90 g/cc, pressure 2.5 t/cc
TIMCAL TIMREX® SFG150 Primary Synthetic Graphite
TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro..
Particle Size 5.0 µm
5.0 µm
Springback 8%, pressure 0.477 t/cc
TIMCAL TIMREX® SFG44 Primary Synthetic Graphite
TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro..
Particle Size 5.0 µm
5.0 µm
Springback 8%, pressure 0.477 t/cc
TIMCAL TIMREX® SFG6 Primary Synthetic Graphite
TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro..
Particle Size 5.0 - 180 µm
5.0 - 180 µm
Trelleborg Fillite® 160W Alumino-silicate Cenospheres
Fillite is a glass hard, inert, hollow silicate sphere. Fillite is primarily used to reduce the weight of plastics, rubbers, resins, cement, etc., but also imparts further benefits in many situatio..
Particle Size 5.0 µm
5.0 µm
Average Crystal Size - Thin Section Test
CoorsTek Alumina-Zirconia Composite, AZ-25
Information provided by CoorsTek.
Particle Size 5.0 µm
5.0 µm
Average
Daikin POLYFLON L-5 PTFE Low Polymer, White Fine Powder
White fine powder.Major Uses: Extreme pressure additive and lubrication/separation compounding agent for dry lubricants, paints, plastics, rubber, etc.Information provided by Daikin Industries.
Particle Size 5.0 µm
5.0 µm
D90
Dandong Taico Minerals TAICOCITE® TC80 Magnesium Hydroxide
Made from local natural brucite minerals, TAICOCITE® is the name of milled magnesium hydroxide products which is produced (micronized/surface treated) by Dandong Taico Minerals Co., Ltd. TAICOCITE®..
Particle Size 5.0 µm
5.0 µm
Mean, measured using laser light scattering
Potters Industries A-Series Z-CEL® 8054 White Synthetic Sodium Aluminosilicate Microsphere
Fine particle white spheres developed as filler for paints, coatings and films.Information provided by Potters Industries.
Copyright © lookpolymers.com All Rights Reserved