| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Particle Size | 4.0 - 9.0 µm | 4.0 - 9.0 µm | d50 |
|
Magyar Aluminum ALO-EL-7P Alumina
Ground Alumina
|
|||
| Particle Size | 6.0 - 9.0 µm | 6.0 - 9.0 µm | Mean |
|
Momentive Performance Materials HCPH Boron Nitride (BN) Powder
GE Advanced Ceramics boron nitride (BN) powders of grades HCP, HCPH, HCPL, and AC6004 are generally single-crystal hexagonal platelets with very high purity. The mean particle sizes for these ultra-..
|
|||
| Particle Size | 5.0 - 9.0 µm | 5.0 - 9.0 µm | 10% |
|
H.C. Starck Amperit® 251 Gas Atomized (NiCr 80-20) |
|||
| Particle Size | 5.0 - 9.0 µm | 5.0 - 9.0 µm | 10% |
|
H.C. Starck Amperit® 281 Gas Atomized (NiAl 95-5) |
|||
| Particle Size | 5.0 - 9.0 µm | 5.0 - 9.0 µm | Laser Diffraction D50 |
|
H.C. Starck Grade A Zirconium Carbide, ZrC
Additive for hard metalsAdditive for powder metallurgyModerator in solid fuel propellant
|
|||
| Particle Size | 7.0 - 9.0 µm | 7.0 - 9.0 µm | 10% |
|
H.C. Starck Amperit® 554.071 Tungsten Carbide-Cobalt-Chromium 86-10-4 (WC-Co-Cr) |
|||
| Particle Size | 6.0 - 9.0 µm | 6.0 - 9.0 µm | D(0.5) |
|
Akzo Nobel Expancel® 461 DU 20 Dry unexpanded microspheres
Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the..
|
|||
| Particle Size | 6.0 - 9.0 µm | 6.0 - 9.0 µm | D(0.5) |
|
Akzo Nobel Expancel® 461 WU 20 Wet unexpanded microspheres
Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the..
|
|||
| Particle Size | 6.0 - 9.0 µm | 6.0 - 9.0 µm | D(0.5) |
|
Akzo Nobel Expancel® 551 DU 20 Dry unexpanded microspheres
Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the..
|
|||
| Particle Size | 6.0 - 9.0 µm | 6.0 - 9.0 µm | D(0.5) |
|
Akzo Nobel Expancel® 551 WU 20 Wet unexpanded microspheres
Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the..
|
|||