| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Molecular Weight | 60000 - 150000 g/mol | 60000 - 150000 g/mol | Average value: 105000 g/mol Grade Count:19 |
|
Overview of materials for PVC, Uncompounded
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Uncompounded". Each property range of values reported is minimum and maximum values of appropriate ..
|
|||
| Molecular Weight | 60000 - 150000 g/mol | 60000 - 150000 g/mol | |
|
LG Chemical LB100M PVC
General Description: LB100M, blend resin exhibits the following characteristics. Reduced viscosity, aging of plastisol, low gloss at the top layers and improved deaeration of plasticallyMain Applica..
|
|||
| Molecular Weight | 60000 - 150000 g/mol | 60000 - 150000 g/mol | |
|
LG Chemical LB110 PVC
General Description: LB110 is a homopolymer blending resin, which can be characterized with its fine particle size, medium molecular weight . It is used in plastically for viscosity , air released a..
|
|||
| Molecular Weight | 60000 - 150000 g/mol | 60000 - 150000 g/mol | |
|
LG Chemical LP090 PVC
General Description: LP090 ,Homopolymer made from micro-suspension polymerization ,is a medium-viscosity PVC resin with a pseudo plastic flow property in processing range. LP090 can be used for wall..
|
|||
| Molecular Weight | 60000 - 150000 g/mol | 60000 - 150000 g/mol | |
|
LG Chemical LP170 PVC
General Description: LP170, homopolymer made from micro- suspension polymerization, is a medium- viscosity PVC resin with a pseudo plastic flow property in processing range. LP170 can be used for sy..
|
|||
| Molecular Weight | 60000 - 150000 g/mol | 60000 - 150000 g/mol | |
|
LG Chemical LP170G PVC
General Description: LP170G, homopolymer made from micro- suspension polymerization, is a low viscosity PVC resin with an good deaeration and stable viscosity at high temperature. Products made from..
|
|||
| Molecular Weight | 60000 - 150000 g/mol | 60000 - 150000 g/mol | |
|
LG Chemical LP170L PVC
General Description: LP170L, homopolymer made from micro- suspension polymerization, is a medium- viscosity PVC resin with a pseudo plastic flow property in processing range. LP170L can be used for ..
|
|||
| Molecular Weight | 60000 - 150000 g/mol | 60000 - 150000 g/mol | |
|
LG Chemical LS080S PVC
General Description: LS080S, homopolymer made by suspension polymerization, can be applied to hard or semi-hard products.Main Applications: Hard sheets, films, fittings, injection molded products, b..
|
|||
| Molecular Weight | 60000 - 150000 g/mol | 60000 - 150000 g/mol | |
|
LG Chemical LS100 PVC
General Description: LS100 is a general-purpose product used for soft and hard products and is most widely used in PVC grade.Main Applications: Pipe, power cable jacket, leather, sheets, hoses, soft..
|
|||
| Molecular Weight | 60000 - 150000 g/mol | 60000 - 150000 g/mol | |
|
LG Chemical LS100E PVC
General Description: LS100E, homopolymer by mass polymerization, can be applied to various applications, such as semi rigid and rigid products.Main Applications: Pipe, profiles, sashCAS No: 9002-86-..
|
|||
| Molecular Weight | 60000 - 150000 g/mol | 60000 - 150000 g/mol | |
|
LG Chemical LS100S PVC
General Description: LS100S, homopolymer made by suspension polymerization, can be applied to soft or semi-hard products. Products made from LS100S have excellent surface, bright color and transpare..
|
|||
| Molecular Weight | 60000 - 150000 g/mol | 60000 - 150000 g/mol | |
|
LG Chemical LS130S PVC
General Description: LS130S, homopolymer made by suspension polymerization, is mainly used in PVC wire extrusion and calendar processing, well known for giving clean surfaces and bright color to the..
|
|||
| Molecular Weight | 60000 - 150000 g/mol | 60000 - 150000 g/mol | |
|
LG Chemical LS170 PVC
General Description: LS170, homopolymer made by suspension polymerization, is applied for value added products such as matted sheeting, super heat resistant wire ,high pressure hose, packing and gas..
|
|||
| Molecular Weight | 60000 - 150000 g/mol | 60000 - 150000 g/mol | |
|
LG Chemical LS300 PVC
General Description: LS300, a homopolymer made by suspension polymerization, is applied for value added special products such as matted sheeting ,super heat resistant wire, high pressure hose, packi..
|
|||
| Molecular Weight | 60000 - 150000 g/mol | 60000 - 150000 g/mol | |
|
LG Chemical PB1120 PVC
General Description: PB1120, homopolymer made by micro-suspension seeded polymerization, is medium-viscosity PVC resin with pseudo plastic flow property. It can be used for foam flooring layer and w..
|
|||
| Molecular Weight | 60000 - 150000 g/mol | 60000 - 150000 g/mol | |
|
LG Chemical PB1202 PVC
General Description: PB1202, homopolymer made by micro-suspension seeded polymerization, PVC Resin has a fluid property similar to Newtonian fluidity (low-viscosity) It is mainly used for non-foamin..
|
|||
| Molecular Weight | 60000 - 150000 g/mol | 60000 - 150000 g/mol | |
|
LG Chemical PB1302 PVC
General Description: PB1302, homopolymer made from micro-suspension seeded polymerization, is a low-viscosity PVC resin with a pseudo-plastic flow property in processing range. It can be used for ca..
|
|||
| Molecular Weight | 60000 - 150000 g/mol | 60000 - 150000 g/mol | |
|
LG Chemical PB1752 PVC
General Description: PB1752, homopolymer made from micro-suspension seeded polymerization, is a low-viscosity PVC resin with a pseudo-plastic flow property in processing range. It can be used for sk..
|
|||
| Molecular Weight | 60000 - 150000 g/mol | 60000 - 150000 g/mol | |
|
LG Chemical PB900 PVC
General Description: PB900, homopolymer made by micro-suspension seeded polymerization, is PVC resin with pseudo plastic flow property. PB900 can be used for wall paper made by knife coating/rotary ..
|
|||
| Molecular Weight | 60000 - 150000 g/mol | 60000 - 150000 g/mol | |
|
LG Chemical PE1311 PVC
General Description: PE1311, homopolymer made by emulsion polymerization, is a high-viscosity PVC resin with pseudo-plastic flow property PE1311 has an good chemical foaming with low density and fin..
|
|||