Polymer Property : Linear Mold Shrinkage = 0.0025 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.0025 cm/cm
0.0025 in/in
ASTM D955
RheTech Products FRG220-773UB 20% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Flame Retardant, UV Stabilized, Light Grey
Applications: Electrical housingsStructural componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Linear Mold Shrinkage 0.0025 - 0.0035 cm/cm
0.0025 - 0.0035 in/in
With Flow; ISO 2577
Polykemi AB POLYfill PPH GF12030 PD2 Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled
Information provided by Polykemi AB
Linear Mold Shrinkage 0.0025 cm/cm
0.0025 in/in
Positive Mold; ASTM D955
Resinoid 2002-C5 Phenolic Molding, Fabric Reinforced
Data provided by the manufacturer.The Resinoid 2000 organic fiber reinforced series compounds feature mechanical strength, dimensional stability, and shock resistance
Linear Mold Shrinkage 0.0025 - 0.0040 cm/cm
0.0025 - 0.0040 in/in
ASTM D955
PolyOne Stat-Tech™ PS-NX 102902 CM Black Polybutylene Terephthalate (PBT)  (discontinued **)
Preliminary Data SheetPolyOne First ChoiceInformation provided by PolyOne Corporation.
Linear Mold Shrinkage 0.0025 - 0.0035 cm/cm
0.0025 - 0.0035 in/in
With Flow; ISO 2577
Polykemi AB POLYfill PPH GF3030 PD2 PP, Glass Fiber-Reinforced, Chemically Coupled
Information provided by Polykemi AB
Linear Mold Shrinkage 0.0025 - 0.0035 cm/cm
0.0025 - 0.0035 in/in
With Flow; ISO 2577
Polykemi AB POLYfill PPH GF5030 PD2 Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled
Information provided by Polykemi AB
Linear Mold Shrinkage 0.0025 cm/cm
0.0025 in/in
LATI
LATI LASTANE 50 G/25 25% Glass Fiber Reinforced Polyurethane (PUR)  (Unverified Data**)
Description: Lastane thermoplastics are polyurethane (PUR) products. They exhibit good wear and impact resistance, even at low temperatures, noise inertness and excellent mould release. These proper..
Linear Mold Shrinkage 0.0025 - 0.0045 cm/cm
0.0025 - 0.0045 in/in
(longitudinal); ISO 2577
Raschig Group 3572 Epoxy
Glass-fiber reinforced epoxy molding compound. Good mechanical strength and electrical strength, enhanced elasticity for ensuring good sealing under extreme heat and/or humidity, good chemical resis..
Linear Mold Shrinkage 0.0025 cm/cm
0.0025 in/in
ASTM D955
Mitsui AURUM® JCL3030 Thermoplastic Polyimide Resin, Amorphous, Wear/Friction Grade  (discontinued **)
AURUM® is an easy melt, processable and recyclable thermoplastic polyimide resin that provides continuous service temperatures to 465° F in its amorphous state and up to 550° F when annealed to i..
Linear Mold Shrinkage 0.0025 cm/cm
0.0025 in/in
Cookson Group Plaskon® ULS-12HLG Epoxy Encapsulant  (discontinued **)
Test specimens were transfer molded and post cured 4 hours at 175°C.A state-of-the-art, ultra low stress epoxy encapsulant designed for packaging large, stress-sensitive DIPs, PLCCs and QFPs. It i..
Linear Mold Shrinkage 0.0025 cm/cm
0.0025 in/in
ASTM D6289
Sumitomo Bakelite Durez® 32245 Phenolic, Compression Grade
Durez 32245 Black Phenolic is a two-stage glass fiber and mineral filled special purpose molding compound. It is especially designed for applications requiring high strength and dimensional stabilit..
Linear Mold Shrinkage 0.0025 cm/cm
0.0025 in/in
ASTM D955
Sumitomo Bakelite North America XB-22 Fiberglass Reinforced Phenolic Novolac
XB-22 is a fiberglass reinforced phenolic novolac molding compound, with excellent dimensional stability and good strength at elevated temperatures. This material is formulated for low thermal condu..
Linear Mold Shrinkage 0.0025 - 0.0035 cm/cm
0.0025 - 0.0035 in/in
Polyram PlusTek PA325G5 Nylon 6.6, 25% Glass Fiber, Flame Retardant
25% glass fiber reinforced, flame retardant, halogen free polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind.
Linear Mold Shrinkage 0.0025 - 0.015 cm/cm
0.0025 - 0.015 in/in
ASTM D955
EPICHEM Epiter PBT GF 20 Polybutylene Terephthalate, 20% Glass
Characteristics: 20% glass fibre filled
Linear Mold Shrinkage 0.0025 cm/cm
0.0025 in/in
ASTM D955
Adell AR-38 Nylon 66, 40% Glass Reinforced
Data provided by Adell Plastics, Inc.
Linear Mold Shrinkage 0.0025 cm/cm
0.0025 in/in
ASTM D955
Adell BR-38 Nylon 6, 40% Glass Reinforced
Data provided by Adell Plastics, Inc.
Linear Mold Shrinkage 0.0025 cm/cm
0.0025 in/in
ASTM D2566
BCC Products BC 8400 Urethane Casting
BC8400 is an unfilled, low viscosity, quick setting two component urethane system. When properly cured, BC 8400 will exhibit high impact strength and yield thermoplastic-like parts. Some features i..
Linear Mold Shrinkage 0.0025 cm/cm
0.0025 in/in
BCC Products BC 8690E Polyurethane Elastomer
BC 8690E is a two-component urethane elastomer compound specifically designed for casting applications. This product is a safe, easy-to-handle, room temperature mixing and curing system that contain..
Linear Mold Shrinkage 0.0025 - 0.0035 cm/cm
0.0025 - 0.0035 in/in
Across Flow; ISO 2577
Polykemi AB POLYfill PPH GF5035 PD2 VT Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled/Heat Resistant
Information provided by Polykemi AB
Linear Mold Shrinkage 0.0025 cm/cm
0.0025 in/in
E-Polymers SEPAZ® LB40 PA6 LFT Resin
Long Fiber Thermoplastics: SEPAZ LFT products, injection moldable long fiber-reinforced thermoplastics (LFT), are made using a unique pultrusion that thoroughly wets out the glass fibers and deliver..
Linear Mold Shrinkage 0.0025 cm/cm
0.0025 in/in
LATI
LATI LASTIROL TR G/10-V1 10% Glass Fiber Reinforced Polystyrene (PS) (UL94 V-1)  (discontinued **)
Description: Lastirol thermoplastics are polystyrene (PS) products. The Lastirols feature excellent dimensional stability, good flowability, and can be molded without any particular problem. Glass f..
Linear Mold Shrinkage 0.0025 cm/cm
0.0025 in/in
LATI
LATI LASULF G/30 30% Glass Reinforced Polysulfone (PSU)  (Unverified Data**)
Description: Lasulf products are composed of polysulfone (PSU). They feature good thermal and mechanical properties such as excellent toughness, even at low temperatures, excellent dimensional stabi..
Linear Mold Shrinkage 0.0025 cm/cm
0.0025 in/in
ASTM D955
RheTech Products G20P252-00 20% Glass Fiber Reinforced Polypropylene Copolymer, Natural
Applications: Interior trimArm rest insertConsolesDome light housingInjection molding conditions reported in table.Information provided by RheTech Products.