Polymer Property : Linear Mold Shrinkage = 0.0025 in/in Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.0025 cm/cm
0.0025 in/in
ASTM D955
RheTech Products FRG220-773UB 20% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Flame Retardant, UV Stabilized, Light Grey
Applications: Electrical housingsStructural componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Linear Mold Shrinkage 0.0025 - 0.0045 cm/cm
0.0025 - 0.0045 in/in
Injection and Compression; ISO 2577
Raschig Group 2568 AMC
Glass fiber-reinforced polyester molding compound. Very good mechanical strength, very good electrical properties and dimensional stability, heat resistant up to 500°C for short time - usable for s..
Linear Mold Shrinkage 0.0025 cm/cm
0.0025 in/in
ISO data
BASF Capron® GR20 20% Glass-Filled Nylon 6 (Dry)  (discontinued **)
Capron GR20 is a 20% glass reinforced polyamide 6 injection molding compound possessing a balance of engineering properties combined with excellent processability and surface aesthetics. It is also..
Linear Mold Shrinkage 0.0025 cm/cm
0.0025 in/in
ASTM D955
RheTech Products F32-01 32% Glass Fiber/Mineral Co-Reinforced Polypropylene, Chemically Coupled, Black
Applications: Head lamp housingBracketsUnderhood componentsElectrical housingsFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products.
Linear Mold Shrinkage 0.0025 cm/cm
0.0025 in/in
LATI
LATI LARPEEK 50 G/60 60% Glass Reinforced Polyetheretherketone (PEEK)  (discontinued **)
Larpeek polyetheretherketone (PEEK) is a high performance thermoplastic offering cost effective performance in difficult environments across all industries. PEEK is temperature resistant (up to 250°..
Linear Mold Shrinkage 0.0025 - 0.0035 cm/cm
0.0025 - 0.0035 in/in
With Flow; ISO 2577
Polykemi AB POLYfill PPH GF4030 PD2 Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled
Information provided by Polykemi AB
Linear Mold Shrinkage 0.0025 cm/cm
0.0025 in/in
ASTM D955
Qualchem Danaprop PP2GF-15 Polypropylene, 15% Glass Fiber
Polypropylene (homo-polymer) reinforced with glass fiberInformation provided by Qualchem Zrt.
Linear Mold Shrinkage 0.0025 cm/cm
0.0025 in/in
Cookson Group Plaskon® ULS-12LA Molding Compound  (discontinued **)
Test specimens were transfer molded and post cured 4 hours at 175°C.An ultra low stress, low alpha emission molding compound designed for packaging stress-sensitive memory devices such as TSOPs and..
Linear Mold Shrinkage 0.0025 cm/cm
0.0025 in/in
Haysite 42100 Polyester SMC, 22% Glass Reinforced
Haysite Grade 42100 is a fiber glass reinforced thermoset polyester sheet molding compound exhibiting excellent moldability. It is designed for compression molded parts requiring high strength and g..
Linear Mold Shrinkage 0.0025 cm/cm
0.0025 in/in
ASTM D6289
Sumitomo Bakelite Durez® 32245 Phenolic, Compression Grade
Durez 32245 Black Phenolic is a two-stage glass fiber and mineral filled special purpose molding compound. It is especially designed for applications requiring high strength and dimensional stabilit..
Linear Mold Shrinkage 0.0025 cm/cm
0.0025 in/in
Polyram PB330I8 Nylon 6, 40% Mineral/Glass Filled Heat Stabilized
Information provided by Polymer Technology and Services, LLC (PTS).
Linear Mold Shrinkage 0.0025 cm/cm
0.0025 in/in
ISO 2577
Polyram PlusTek RA301G8 Nylon 6.6 for Injection Molding, 40% Glass Fiber Reinforced, Heat Stabilized
Heat stabilized, 40% glass fiber reinforced Nylon 6.6 for injection molding applications.Information provided by Polyram.
Linear Mold Shrinkage 0.0025 cm/cm
0.0025 in/in
E-Polymers Tekaster® F615G30 , 30% Glass Fiber Reinforced PET
30% Glass Fiber reinforced, High strength, Information provided by E-Polymers Co. Ltd.
Linear Mold Shrinkage 0.0025 cm/cm
0.0025 in/in
ASTM D955
Adell BR-38 Nylon 6, 40% Glass Reinforced
Data provided by Adell Plastics, Inc.
Linear Mold Shrinkage 0.0025 - 0.0040 cm/cm
0.0025 - 0.0040 in/in
IS 13411-1992
Amity Thermosets ATO 156 Phenolic Molding Glass Filler, Compression Molded
Characteristics:High electrical insulationHigh mechanical strengthDimensional stabilityLow water absorptionColor-black Medium flow Applications: High electric insulation componentsHigh voltage swit..
Linear Mold Shrinkage 0.0025 - 0.0035 cm/cm
0.0025 - 0.0035 in/in
Bulk Molding Compounds BMC 2270 Mineral Filled, Glass Reinforced Polyester
BMC 2270 molding compound is a mineral filled, glass-fiber-reinforced polyester compound suitable for compression and transfer molding. It is a general purpose material with medium impact strength a..
Linear Mold Shrinkage 0.0025 - 0.00345 cm/cm
0.0025 - 0.00345 in/in
Bulk Molding Compounds BMC 620X Mineral Filled, Glass Fiber Reinforced Polyester Compound
BMC 620X molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is a high impact material produced in ex..
Linear Mold Shrinkage 0.0025 - 0.0030 cm/cm
0.0025 - 0.0030 in/in
Bulk Molding Compounds BMC T14 General Purpose Molding Compound
BMC T14 is a general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T14 is well suited for injection, transfer or compression molding of intricate parts. Typica..
Linear Mold Shrinkage 0.0025 cm/cm
0.0025 in/in
BCC Products BC 8160 Urethane Casting
BC8160 is a low viscosity two-component urethane casting compound that is specifically formulated for its flexural and impact strength. It is recommended for use for the production casting of highly..
Linear Mold Shrinkage 0.0025 - 0.0030 cm/cm
0.0025 - 0.0030 in/in
Bulk Molding Compounds BMC A50-MS General Purpose Molding Compound
BMC A50-MS is a medium strength, high appearance, general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC A50-MS is well suited for injection, transfer or compres..
Linear Mold Shrinkage 0.0025 cm/cm
0.0025 in/in
LATI
LATI LASTIROL TR G/10-V1 10% Glass Fiber Reinforced Polystyrene (PS) (UL94 V-1)  (discontinued **)
Description: Lastirol thermoplastics are polystyrene (PS) products. The Lastirols feature excellent dimensional stability, good flowability, and can be molded without any particular problem. Glass f..
Linear Mold Shrinkage 0.0025 cm/cm
0.0025 in/in
LATI
LATI LARIL 13 G/30 30% Glass Fiber Reinforced Polyphenylene Oxide (PPOm)  (Unverified Data**)
Description: Laril thermoplastics are polyphenylene oxide (PPOm) products. They exhibit excellent toughness, even at low temperatures, good thermal resistance and dimensional stability are the most ..
Linear Mold Shrinkage 0.0025 cm/cm
0.0025 in/in
ASTM D955
Oxford Polymers 20GF 20% Glass Fiber Filled Polycarbonate for Injection Molding
20% Glass Fiber Filled Polycarbonate for Injection MoldingInformation provided by Oxford Polymers.
Linear Mold Shrinkage 0.0025 cm/cm
0.0025 in/in
ASTM D955
RheTech Products G20P252-00 20% Glass Fiber Reinforced Polypropylene Copolymer, Natural
Applications: Interior trimArm rest insertConsolesDome light housingInjection molding conditions reported in table.Information provided by RheTech Products.
Linear Mold Shrinkage 0.0025 cm/cm
0.0025 in/in
ISO 294-4
LNP Thermocomp® UFM-3249 HS BK8-115 Polyphthalamide, Glass Mineral Reinforcement  (discontinued **)
Features: Heat StabilizedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are sti..