| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Linear Mold Shrinkage | 0.0030 cm/cm | 0.0030 in/in | Measured on a tensile specimen.; ISO 294-4 |
|
PolyOne OnForce™ LFT PP-40LGF/001 Natural Polypropylene Homopolymer (PP Homopolymer)
PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. ..
|
|||
| Linear Mold Shrinkage | 0.0030 cm/cm | 0.0030 in/in | With Flow; ISO 2577 |
|
Polykemi AB SCANMID 6 B12^ F25 Nylon 6, Glass Fiber Reinforced
Information provided by Polykemi AB
|
|||
| Linear Mold Shrinkage | 0.0030 - 0.0090 cm/cm | 0.0030 - 0.0090 in/in | ASTM D955 |
|
Polymer Resources NY66-G50 Nylon 66, 50% Glass Reinforced
Nylon 66, 50% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are test..
|
|||
| Linear Mold Shrinkage | 0.0030 - 0.0060 cm/cm | 0.0030 - 0.0060 in/in | ASTM D955 |
|
Polymer Resources PC-G10-IM Polycarbonate, 10% Glass Reinforced, Impact Modified
Polycarbonate, 10% Glass Reinforced, Impact ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information ..
|
|||
| Linear Mold Shrinkage | 0.0030 cm/cm | 0.0030 in/in | ASTM Data MD |
|
BASF Capron® SEG6 H1 30% Glass-Filled Nylon 6 (Dry)
(discontinued **)
Capron SEG6 H1 is a 30% glass reinforced nylon 6 injection molding compound. This material is currently under development as XA-2678. It exhibits exceptional surface aesthetics at the slower fill s..
|
|||
| Linear Mold Shrinkage | 0.0030 cm/cm | 0.0030 in/in | ASTM D955 |
|
PolyOne Lubri-Tech™ PS-30GF/15T Polybutylene Terephthalate (PBT), Glass Filled, PTFE Lubricated
(discontinued
Description/Features:Glass Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation.
|
|||
| Linear Mold Shrinkage | 0.0030 cm/cm | 0.0030 in/in | ASTM D955 |
|
LNP Lubricomp® EFL-4034 LE BK8-065 Polyetherimide, Glass Fiber Reinforcement, PTFE Lubricant
(discontinued **
Features: Low Extractables, LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP g..
|
|||
| Linear Mold Shrinkage |
0.0030
-
0.0050
cm/cm @Thickness 3.20 mm |
0.0030
-
0.0050
in/in @Thickness 0.126 in |
ASTM D955 |
|
LNP ULTEM® JD7107 Polyetherimide
(discontinued **)
Forms: PelletsInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names instituted after the SABIC purchase..
|
|||
| Linear Mold Shrinkage | 0.0030 - 0.0050 cm/cm | 0.0030 - 0.0050 in/in | |
|
Lehmann & Voss LUVOCOM® 1-7390 Polyamide 66, with carbon fiber, PTFE, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp..
|
|||
| Linear Mold Shrinkage | 0.0030 - 0.0060 cm/cm | 0.0030 - 0.0060 in/in | |
|
Lehmann & Voss LUVOCOM® 1104-7452 Polyether ketone, with glass fiber, easy flowing
Applications: Automotive industry, mechanical- and precision engineering.Improved strength and stiffnes at elevated temperatures.Improved fatigue properties.Thermic, mechanic and chemical highly str..
|
|||
| Linear Mold Shrinkage | 0.0030 - 0.0070 cm/cm | 0.0030 - 0.0070 in/in | |
|
Lehmann & Voss LUVOCOM® 1105/GF/40/BK-1 PEEK, with glass fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; impact resistance.Dynamic stressed parts at high movement velocity.Ch..
|
|||
| Linear Mold Shrinkage | 0.0030 cm/cm | 0.0030 in/in | ASTM D955 |
|
Sumitomo Bakelite Durez® 23570 Phenolic, Injection Grade
Durez 23570 Black Phenolic is a glass and mineral filled two-stage, special purpose molding material. It is designed for high strength, good dimensional stability, and electrical properties even aft..
|
|||
| Linear Mold Shrinkage | 0.0030 cm/cm | 0.0030 in/in | ASTM D955 |
|
Sumitomo Bakelite Durez® 32633 Glass Filled Phenolic, Injection Grade
Durez 32633 Black Phenolic is a two-stage, glass filled, special purpose molding compound. It is designed for applications requiring high physical strengths, dimensional stability, and heat resista..
|
|||
| Linear Mold Shrinkage | 0.0030 cm/cm | 0.0030 in/in | |
|
Tisan TISLAMID® 66 25% Glass Fiber Reinforced Nylon 66
TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec..
|
|||
| Linear Mold Shrinkage | 0.0030 cm/cm | 0.0030 in/in | ISO 2577 |
|
Polyram RamSter PF305G6 PBT, 30% Glass Fiber
30% Glass fiber reinforced, PBT for injection molding applications.Information provided by Polyram.
|
|||
| Linear Mold Shrinkage | 0.0030 - 0.0050 cm/cm | 0.0030 - 0.0050 in/in | ASTM D955 |
|
Cheng Yu Plastic VH825 Flame Retardant ABS, Medium Impact |
|||
| Linear Mold Shrinkage | 0.0030 - 0.0060 cm/cm | 0.0030 - 0.0060 in/in | ASTM D 955 |
|
Cossa Polimeri ESTADIENE 1030 HT V0 Flame Retardant ABS
Acrylonitrile Butadiene StyreneFlame retardant class V0, PBDE free, high thermal resistance, good light resistance, good processability and surface appearanceInformation provided by Cossa Polimeri S..
|
|||
| Linear Mold Shrinkage | 0.0030 - 0.0050 cm/cm | 0.0030 - 0.0050 in/in | ASTM D955 |
|
Ecomass® 3800ZD82 Tungsten Filled Polymethylpentene
Nontoxic alternative to Lead (Pb), radiation shielding applicationsModerate Specific GravityTungsten Powder Filled Polymethylpentene (TPX)RigidInformation provided by Technical Polymers
|
|||
| Linear Mold Shrinkage | 0.0030 - 0.0070 cm/cm | 0.0030 - 0.0070 in/in | ASTM D955 |
|
Chi Mei Polylac® PA-709S ABS - Extrusion
Super Impact Extrusion
|
|||
| Linear Mold Shrinkage | 0.0030 cm/cm | 0.0030 in/in | |
|
Eurotec® Tecomid® NA40 GR30 NL PA 6.6 30% glass fiber reinforced
Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good..
|
|||
| Linear Mold Shrinkage | 0.0030 - 0.0070 cm/cm | 0.0030 - 0.0070 in/in | ASTM D955 |
|
Chi Mei Polylac® PA-777E ABS - High Heat
Ultra High Heat
|
|||
| Linear Mold Shrinkage | 0.0030 - 0.012 cm/cm | 0.0030 - 0.012 in/in | ASTM D955 |
|
EPICHEM PA 6 GF 30 Polyamide 6, 30% Glass
Characteristics: medium viscosity, 30% glass fibre filled
|
|||
| Linear Mold Shrinkage | 0.0030 cm/cm | 0.0030 in/in | ASTM D955 |
|
Asahi Kasei Thermylene® P6-20FG-0693 20% Glass Fiber Reinforced, Heat and UV Stabilized
Information provided by Asahi Thermofil
|
|||
| Linear Mold Shrinkage |
<=
0.0030
cm/cm @Temperature 25.0 °C, Time 259000 sec |
<=
0.0030
in/in @Temperature 77.0 °F, Time 72.0 hour |
Cured |
|
ACC QM 100 QSI Quantum Silicones Clear 30 Durometer Condensation Cure Material
QM 100 is a two component, room temperature condensation cure silicone material. The cured rubber is a crystal clear material designed specifically for the special effects market. The materials' cla..
|
|||
| Linear Mold Shrinkage | 0.0030 cm/cm | 0.0030 in/in | ASTM D955 |
|
Ashley Polymers Ashlene® 265 PPO, 20% Glass Reinforced
A general purpose, 20% glass reinforced PPO resin for injection molding applications.Data provided by the manufacturer
|
|||
| Linear Mold Shrinkage | 0.0030 - 0.0050 cm/cm | 0.0030 - 0.0050 in/in | ASTM D955 |
|
Asia International Enterprise (Hong Kong) 60G8-43GF Nylon 66, 43% Filled
Information provided by Asia International Enterprise (Hong Kong) Ltd.
|
|||
| Linear Mold Shrinkage | 0.0030 cm/cm | 0.0030 in/in | ASTM D955 |
|
Asahi Kasei Thermylene® P-25FG-0100 25% Glass Fiber Reinforced, Heat Stabilized
Information provided by Asahi Thermofil
|
|||
| Linear Mold Shrinkage | 0.0030 - 0.0070 cm/cm | 0.0030 - 0.0070 in/in | ASTM D955 |
|
Resirene Resirene® 8450 High Impact Polystyrene (Chemical Resistant)
Features:Low FlowChemical ResistantMechanical StrengthFDA Rating: 21 CFR 177.1640Applications:Extrusion/ThermoformingRegistration LinersExtruded SheetInformation provided by US distributor Calsak Co..
|
|||
| Linear Mold Shrinkage | 0.0030 - 0.0040 cm/cm | 0.0030 - 0.0040 in/in | ASTM D955 |
|
LNP Lubricomp® OCL-4036 Polyphenylene Sulfide, Carbon Fiber Reinforcement, PTFE Lubricant
(discontinued **)&l
Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac..
|
|||
| Linear Mold Shrinkage | 0.0030 - 0.0050 cm/cm | 0.0030 - 0.0050 in/in | ASTM D955 |
|
Sumitomo Bakelite North America Epiall® 1960B-1 Mineral and Glass Filled Electrical Encapsulation Grade Epoxy
Epiall 1960B-1 is a mineral and short fiberglass filled epoxy compound, formulated for the encapsulation of passive electronic devices.Information provided by Sumitomo Bak North America, Inc.
|
|||