Polymer Property : Linear Mold Shrinkage = 0.0049 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.0032 - 0.0049 cm/cm
0.0032 - 0.0049 in/in
IS 13411-1992
Amity Thermosets ATS 766 Phenolic Molding Chopped cotton fabric Filler, Compression Molded
Characteristics:High impact strengthGlossy surfaceLow shrinkageGood sliding propertiesColor-BrownMedium flowApplications:Cog wheelsCastor wheelsBush bearingsPulleysWelding rod handlesTextile bobbins..