Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Linear Mold Shrinkage = 0.0050 in/in Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.0040 - 0.0050 cm/cm
0.0040 - 0.0050 in/in
ASTM D955
Network Polymers PC-1010
Description: Polycarbonate, 10% Glass Filled BlackInformation provided by Network Polymers Inc.
Linear Mold Shrinkage 0.0010 - 0.0050 cm/cm

@Thickness 4.00 mm,
Temperature 23.0 °C
0.0010 - 0.0050 in/in

@Thickness 0.157 in,
Temperature 73.4 °F
Flow Bergmann Method; ISO 294-4
PolyOne Stat-Tech™ NN-20CF/000 Black Polyamide 66 (Nylon 66)
Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound..
Linear Mold Shrinkage 0.0020 - 0.0050 cm/cm

@Thickness 3.20 mm
0.0020 - 0.0050 in/in

@Thickness 0.126 in
ASTM D955
Eastman Eastar GN125 Copolyester, Natural  (discontinued **)
Eastar Copolyester GN125 is a glycol modified polyethylene terephthalate (PET) that contains an ultraviolet light inhibitor. This product is recommended for indoor applications requiring enhanced co..
Linear Mold Shrinkage 0.0020 - 0.0050 cm/cm
0.0020 - 0.0050 in/in
ASTM D955
PolyOne Lubri-Tech™ AT-10CF/15T-2S Acetal-Copolymer, Carbon Fiber Reinforced, PTFE/Silicone Lubricated  (disco
Description/Features:Carbon Fiber ReinforcedPTFE/Silicone LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Linear Mold Shrinkage 0.0030 - 0.0050 cm/cm

@Thickness 3.20 mm
0.0030 - 0.0050 in/in

@Thickness 0.126 in
ASTM D955
LNP ULTEM® JD7902 Polyetherimide  (discontinued **)
Forms: PelletsInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names instituted after the SABIC purchase..
Linear Mold Shrinkage 0.0030 - 0.0050 cm/cm
0.0030 - 0.0050 in/in
Lehmann & Voss LUVOCOM® 1-7390 Polyamide 66, with carbon fiber, PTFE, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp..
Linear Mold Shrinkage 0.0020 - 0.0050 cm/cm
0.0020 - 0.0050 in/in
Lehmann & Voss LUVOCOM® 1850/GF/30/TF/13/SI/2 PBT, with glass fiber, PTFE, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec..
Linear Mold Shrinkage 0.0020 - 0.0050 cm/cm
0.0020 - 0.0050 in/in
Lehmann & Voss LUVOCOM® 1850/GF/30/TF/15/BK PBT, with glass fiber and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec..
Linear Mold Shrinkage 0.0020 - 0.0050 cm/cm
0.0020 - 0.0050 in/in
Lehmann & Voss LUVOCOM® 3-8351 Polyamide 6, with carbon fiber
Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Strong, stiff parts.Electrically conductive, suitable for continuous discharging of statically generated el..
Linear Mold Shrinkage 0.0030 - 0.0050 cm/cm

@Temperature 23.0 °C
0.0030 - 0.0050 in/in

@Temperature 73.4 °F
ASTM D955
Kingfa JH-R2G10 P60 10% Glass Fiber Reinforced PC/ABS Alloy
Features:UL HB @ 1.6-3.2mmExcellent balance propertiesHigh stiffnessGood size stabilityGood surface adhesionExcellent processing properties, large partsApplications:Injection moldingAutomobile instr..
Linear Mold Shrinkage 0.0020 - 0.0050 cm/cm
0.0020 - 0.0050 in/in
Lehmann & Voss LUVOCOM® 1/CF/10/TF/20/GY Polyamide 66, with carbon fiber and PTFE, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Electrically conductive, suita..
Linear Mold Shrinkage 0.0020 - 0.0050 cm/cm
0.0020 - 0.0050 in/in
Lehmann & Voss LUVOCOM® 1105/GF/30/NAT-2 PEEK, with glass fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension..
Linear Mold Shrinkage 0.0030 - 0.0050 cm/cm
0.0030 - 0.0050 in/in
Lehmann & Voss LUVOCOM® 1301-8060 PPS, linear, with glass fiber and PTFE, high viscosity
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Strong, stiff parts.Low warpage, isotropic shrinkage characteristics.Improved friction and wear be..
Linear Mold Shrinkage 0.0020 - 0.0050 cm/cm
0.0020 - 0.0050 in/in
ASTM D955
Eastman Eastar DN010 Copolyester
Eastar Copolyester DN010 is a brilliantly clear polymer having excellent impact strength, chemical resistance, and low shrinkage rates. Eastar Copolyester DN010 contains no mold release.Applications..
Linear Mold Shrinkage 0.0020 - 0.0050 cm/cm

@Thickness 3.20 mm
0.0020 - 0.0050 in/in

@Thickness 0.126 in
ASTM D955
Eastman Eastar MN210 Copolyester, Natural
Eastar copolyesters are brilliantly clear polymers that have excellent impact strength, chemical resistance, dimensional stability, and low shrinkage rates.Applications/UsesMedical
Linear Mold Shrinkage 0.0030 - 0.0050 cm/cm
0.0030 - 0.0050 in/in
ASTM D 955
Cossa Polimeri ESTACARB 0820 GF V0-5V Flame Retardant Polycarbonate
Polycarbonate with 10% glass fiber reinforcementFlame retardant class V0, PBDE free, high stiffness, high dimensional stability, good melt flow, good processability, good light resistanceInformation..
Linear Mold Shrinkage 0.0020 - 0.0050 cm/cm
0.0020 - 0.0050 in/in
ASTM D955
EPICHEM Epilac R ABS 10% GF Acrylonitrile Butadiene Styrene, 10% Glass Fiber
Characteristics: 10% glass fibre filled
Linear Mold Shrinkage 0.0020 - 0.0050 cm/cm
0.0020 - 0.0050 in/in
ISO 2577
Cossa Polimeri ESTABLEND PA 1050 GF HI ABS / Nylon 6 Blend, 25% Glass Filled
ESTABLEND PA is a blend of acrylonitrile butadiene styrene and polyamide 6.25% glass fiber reinforcedHigh impact strength, high chemical resistance, excellent heat resistance, high dimensional stabi..
Linear Mold Shrinkage 0.0030 - 0.0050 cm/cm
0.0030 - 0.0050 in/in
Internal
Ecomass® 705ZC75 Stainless Steel Filled ABS
Nontoxic Alternative to traditional metals, weighting and balancing applicationsModerate Specific GravityStainless Steel Powder Filled ABSInformation provided by Technical Polymers
Linear Mold Shrinkage 0.0040 - 0.0050 cm/cm
0.0040 - 0.0050 in/in
ASTM D-955
Bhansali Engineering Abstron IM-14G ABS Very High Rigidity Injection Molding Grade
Very High Rigidity, High Gloss, Medium Impact with excellent other mechanical propertiesInformation provided by Bhansali
Linear Mold Shrinkage 0.0030 - 0.0050 cm/cm
0.0030 - 0.0050 in/in
Bulk Molding Compounds BMC 3001H Mineral Filled Alkyd
BMC 3001H molding compound is a mineral filled, glass-fiber reinforced alkyd compound suitable for compression and transfer molding. Because of its soft flow, it is also used extensively in cold spu..
Linear Mold Shrinkage 0.0040 - 0.0050 cm/cm
0.0040 - 0.0050 in/in
ASTM D-955
Bhansali Engineering Abstron SE-22 ABS Sheet Extrusion Grade
Sheet Extrusion grade for profile & DoorsInformation provided by Bhansali
Linear Mold Shrinkage 0.0030 - 0.0050 cm/cm

@Thickness 4.00 mm
0.0030 - 0.0050 in/in

@Thickness 0.157 in
Teijin Panlite® GS-3410 Friction and Abrasion Resistant, Glass Fiber Reinforced Polycarbonate Resin
GF 10% reinforced grade, meeting UL 94 V-2. It is compounded with fluorine powder to improve friction and abrasion resistance, maintaining excellent characteristics of polycarbonate resin.Applicatio..
Linear Mold Shrinkage 0.0030 - 0.0050 cm/cm
0.0030 - 0.0050 in/in
ASTM D-955
Bhansali Engineering Abstron HR-105 ABS Super Heat Resistant
High Heat Resistant Grades with Better Flow characteristicInformation provided by Bhansali