Polymer Property : Linear Mold Shrinkage = 0.0060 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.0020 - 0.0060 cm/cm
0.0020 - 0.0060 in/in
ASTM D-955
Plaskolite Optix® CP - 1000 IG High Impact Grade Acrylic Resin
OPTIX® impact-modified grades offer 7 to 10 times the impact resistance of general purpose polymers while maintaining optical clarity.Information provided by Plaskolite, Inc.
Linear Mold Shrinkage 0.0020 - 0.0060 cm/cm
0.0020 - 0.0060 in/in
ASTM D-955
Plaskolite West Optix® CA - 927 High Impact Acrylic Resin
Optix® impact-modified grades exhibit 7 to 10 times the impact strength of general purpose grades and maintaining the superior optical properties. Each grade is offered in a grade(G) that resists g..
Linear Mold Shrinkage 0.0030 - 0.0060 cm/cm
0.0030 - 0.0060 in/in
ASTM D955
Polymer Resources PC-G10-IM Polycarbonate, 10% Glass Reinforced, Impact Modified
Polycarbonate, 10% Glass Reinforced, Impact ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information ..
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm
0.0040 - 0.0060 in/in
ASTM D955
Ineos Nova 474 High Performance Styrenic Enhanced Polystyrene  (discontinued **)
Custom ColorsApplications: Injection molding, Alternative to engineering resinsPerformance grades of polystyrene are engineered to have specific properties. These products can be custom colored. N..
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm

@Thickness 3.17 mm
0.0040 - 0.0060 in/in

@Thickness 0.125 in
ASTM D955
PolyOne Lubri-Tech™ AS-000/10T-2S ABS - 10% PTFE - 2% Silicone  (discontinued **)
Data provided by PolyOne.
Linear Mold Shrinkage 0.0020 - 0.0060 cm/cm
0.0020 - 0.0060 in/in
48 hrs; ASTM D955
Plaskolite Optix® PL-200 Acrylic Resin  (discontinued **)
Injection molding grade pellets.Data provided by the manufacturer, Plaskolite, Inc.
Linear Mold Shrinkage 0.0020 - 0.0060 cm/cm
0.0020 - 0.0060 in/in
ASTM D955
Albis Plastics Cellulose Acetate Butyrate B9024 (UVI, Odor Mask Added), 13% Plasticizer  (discontinued **)
Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T..
Linear Mold Shrinkage 0.0020 - 0.0060 cm/cm
0.0020 - 0.0060 in/in
ASTM D955
Albis Plastics Cellulose Acetate Butyrate B9024 (UVI, Odor Mask Added), 10% Plasticizer  (discontinued **)
Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T..
Linear Mold Shrinkage 0.0020 - 0.0060 cm/cm
0.0020 - 0.0060 in/in
Lehmann & Voss LUVOCOM® 1105-7828/GY PEEK, with glass fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension..
Linear Mold Shrinkage 0.0020 - 0.0060 cm/cm
0.0020 - 0.0060 in/in
Lehmann & Voss LUVOCOM® 1105-8004 PEEK, with carbon fiber, low-warpage, easy flowing
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Dynamic stressed parts.High chemical resistance parts, hydrolysis resi..
Linear Mold Shrinkage 0.0030 - 0.0060 cm/cm
0.0030 - 0.0060 in/in
Lehmann & Voss LUVOCOM® 1-7789/EG Polyamide 66, with carbon fiber, lubricant modified, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Antistatic.High dimensi..
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm

@Temperature 23.0 °C
0.0040 - 0.0060 in/in

@Temperature 73.4 °F
ASTM D955
Kingfa JH950-402 Flame Retardant PC/ABS Alloy
Features:UL V-0 @ 3.2mmExcellent balance propertiesHigh heat resistanceGood normal/low temperature impact strengthGood surfaceApplications:Small household appliance cabinetControllerSocketShell of a..
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm
0.0040 - 0.0060 in/in
ASTM-D955
Ineos ABS Lustran® 633 ABS, Injection Molding Grade
Lustran® ABS 633 is a general-purpose injection molding grade of ABS (Acrylonitrile Butadiene Styrene). It offers a good balance of physical properties, high gloss, and good moldability. Typical ..
Linear Mold Shrinkage 0.0030 - 0.0060 cm/cm
0.0030 - 0.0060 in/in
ASTM D955
Ineos Styrenics Polystyrene 147F (NAFTA)
An easy flow, general purpose polystyrene. Has moderate heat resistance and strength for general molding and extrusion applications.Information provided by BASF.Ineos Styrenics purchased this produ..
Linear Mold Shrinkage 0.0030 - 0.0060 cm/cm
0.0030 - 0.0060 in/in
0.125; ASTM D955
LTL Color Compounds ColorFast® FRA202 General Purpose ABS
General purpose V0/5VA-rated ABSAll information provided by LTL Color Compounders, Inc.
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm
0.0040 - 0.0060 in/in
ASTM D955
LTL Color Compounds ColorRxâ„¢ ABS-0501A Antimicrobial ABS
A high gloss, injection molding grade of ABS containing antimicrobial protection. Ingredients are not approved for biocompatibility or food contact applications.All information provided by LTL Color..
Linear Mold Shrinkage 0.0030 - 0.0060 cm/cm
0.0030 - 0.0060 in/in
ASTM D955
KKPC Kuhmo HFH 403 Flame Retarded HIPS
Key features: Low flammable V-2 grade. Common Uses: TV and VCR housing.HIPS is a functional resin made by copolymerization of styrene monomer and PBR. It shows excellent balance between impact-resis..
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm
0.0040 - 0.0060 in/in
ASTM D1299
Loxim 230 01V0 Polybutylene Terephthalate
Information provided by Loxim Industries
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm
0.0040 - 0.0060 in/in
ASTM D955
PlastxWorld CEVIAN® LMW48 Laser Markable Grade ABS
White MarkingThese are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc.
Linear Mold Shrinkage 0.0020 - 0.0060 cm/cm

@Thickness 3.20 mm
0.0020 - 0.0060 in/in

@Thickness 0.126 in
72 hr; ISO 294
A. Schulman FORMION™ FI 330 Ionomer
Information provided by A. Schulman.
Linear Mold Shrinkage 0.0020 - 0.0060 cm/cm
0.0020 - 0.0060 in/in
ASTM D955
Eastman Tenite 307A4000018 Propionate Clear, Trsp
Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi..
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm
0.0040 - 0.0060 in/in
ASTM D955
Ecomass® 4703ZD88 Tungsten Filled Polyurethane
Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applicationsModerate Specific GravityTungsten Filled Polyurethane (TPU)FlexibleInformation provided by Technical Polym..
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm
0.0040 - 0.0060 in/in
ASTM D955
Diamond Polymers ABS 1000
Description: Injection Molding Grade, Extra High GlossInformation provided by Diamond Polymers, Inc.
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm
0.0040 - 0.0060 in/in
ASTM D955
Diamond Polymers ABS 3501E Natural 1002 ESCR Extrusion Grade, Environmental Stress Crack Resistant
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm
0.0040 - 0.0060 in/in
ASTM D-955
Bhansali Engineering Abstron IM-29 ABS Injection Molding Grade
High Impact, Medium, High Flow, General PurposeInformation provided by Bhansali
Linear Mold Shrinkage 0.0010 - 0.0060 cm/cm
0.0010 - 0.0060 in/in
ASTM D955
Cheng Yu Plastic E2350 Flame Retardant PET, 50% Glass Fiber
Linear Mold Shrinkage 0.0020 - 0.0060 cm/cm
0.0020 - 0.0060 in/in
ASTM D955
Ineos Nova Zylar® 530 Clear Impact Modified Acrylic Copolymer  (discontinued **)
Features:High clarityStyrenic processing advantagesExcellent property retention after ETO and gamma sterilizationMeets USP XXIII specifications for Class VI plasticsUL94 HB @ 1.5 mm for uncolored ma..
Linear Mold Shrinkage 0.0020 - 0.0060 cm/cm
0.0020 - 0.0060 in/in
ASTM D955
Albis Plastics Cellulose Acetate Butyrate B9024 (UVI, Odor Mask Added), 13% Plasticizer  (discontinued **)
Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T..
Linear Mold Shrinkage 0.0020 - 0.0060 cm/cm
0.0020 - 0.0060 in/in
ASTM D955
Albis Plastics Cellulose Acetate Butyrate B9086 (FDA Odor Mask), 10% Plasticizer  (discontinued **)
Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T..