| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Linear Mold Shrinkage | 0.0070 - 0.0090 cm/cm | 0.0070 - 0.0090 in/in | Across Flow; ISO 2577 |
|
Polykemi AB POLYfill PP CIM9040 Polypropylene, Mineral Reinforced
Information provided by Polykemi AB
|
|||
| Linear Mold Shrinkage | 0.0070 - 0.018 cm/cm | 0.0070 - 0.018 in/in | FRISETTA Test Method |
|
Nilit FRIANYL A63 SG-GV 2010 Nylon 6.6 for injection molding, 20% mineral filled and 10% glass fiber reinforced
Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics
|
|||
| Linear Mold Shrinkage | 0.0070 - 0.016 cm/cm | 0.0070 - 0.016 in/in | FRISETTA Test Method |
|
Nilit FRIANYL B63 KF20 Nylon 6 for injection molding, 20% short glass fiber reinforced
Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics
|
|||
| Linear Mold Shrinkage | 0.0070 - 0.010 cm/cm | 0.0070 - 0.010 in/in | With Flow; ISO 2577 |
|
Polykemi AB POLYlux 3709MLB PC/PBT-Blend, Paintable
Information provided by Polykemi AB
|
|||
| Linear Mold Shrinkage | 0.0070 - 0.010 cm/cm | 0.0070 - 0.010 in/in | Across Flow; ASTM D955 |
|
Polymer Resources PC/TP-GP2 PC/Polyester Alloy
High Impact, Excellent Chemical ResistanceProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided b..
|
|||
| Linear Mold Shrinkage | 0.0070 - 0.010 cm/cm | 0.0070 - 0.010 in/in | ASTM D955 |
|
Polymer Resources PC/TP-GP3-G10 PC/Polyester Alloy, 10% Glass Reinforced
Superior Chemical Resistance, 10% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pr..
|
|||
| Linear Mold Shrinkage | 0.0070 - 0.011 cm/cm | 0.0070 - 0.011 in/in | (longitudinal) Injection; ISO 2257 |
|
Raschig Group MELOPLAS® 182 MF
Wood flour-reinforced and inorganically filled, phenol-modified MF molding compound (MPF) in dark colors. Improved dimensional stability and electrical properties as compared with MP 180, high surf..
|
|||
| Linear Mold Shrinkage | 0.0070 - 0.010 cm/cm | 0.0070 - 0.010 in/in | Injection; ISO 2257 |
|
Raschig Group RALUPOL® 2200 UP Polyester
Organically filled polyester molding compound. Low post-shrinkage, good electrical values and mechanical properties, high surface quality and good color stability (non-yellowing). This product meets..
|
|||
| Linear Mold Shrinkage | 0.0070 cm/cm | 0.0070 in/in | ASTM D955 |
|
LNP Thermocomp® JF-1004 EM M BK905 Polyethersulfone, Milled Glass Fiber
(discontinued **)
Features: Good MoldabilityForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are st..
|
|||
| Linear Mold Shrinkage | 0.0070 - 0.012 cm/cm | 0.0070 - 0.012 in/in | ISO 2577 |
|
Panjin Zhongrun Chemerize 012G High Viscosity CoPEEK
Information provided by Bieglo Gmbh.
|
|||
| Linear Mold Shrinkage | 0.0070 cm/cm | 0.0070 in/in | ASTM D955 |
|
LNP Lubricomp® PDX-E-00548 CCS Polyetherimide, Aramid Fiber Reinforced, PTFE Lubricant
(discontinued **)
Features: Lubricated, Low to None Ion ContentForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however man..
|
|||
| Linear Mold Shrinkage | 0.0070 cm/cm | 0.0070 in/in | ASTM D955 |
|
Solvay Specialty Polymers Supradel® HTS-2600 High Temperature Sulfone Resin
(discontinued **)
SUPRADEL HTS-2600 is a high-temperature, high-performance, amorphous, sulfone polymer. In addition to exceptional thermal performance, this resin has the other performance features and attributes t..
|
|||
| Linear Mold Shrinkage | 0.0070 - 0.012 cm/cm | 0.0070 - 0.012 in/in | |
|
Lehmann & Voss LUVOCOM® 1105-7777 PEEK, lubricant modified
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Isotropic shrinkage characteristics.Emergency running property.Information provided by Leh..
|
|||
| Linear Mold Shrinkage | 0.0070 - 0.014 cm/cm | 0.0070 - 0.014 in/in | |
|
Lehmann & Voss LUVOCOM® 20-7796 Polyphthalamide, with aramid reinforcement and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Low influence from moisture an..
|
|||
| Linear Mold Shrinkage | 0.0070 - 0.013 cm/cm | 0.0070 - 0.013 in/in | |
|
Lehmann & Voss LUVOCOM® 1/AR/5/NT Polyamide 66, with aramid reinforcement
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved wear behaviour, low warpage.Isotropic shrinkage characteristics.Control disks, cams, s..
|
|||
| Linear Mold Shrinkage | 0.0070 cm/cm | 0.0070 in/in | |
|
Styron Pulse® 930 ABS + Polycarbonate
PULSE® 930 Engineering resin has been designed to provide excellent processability, high heat resistance, and high impact strength at room temperature. PULSE 930 Engineering resin has been used i..
|
|||
| Linear Mold Shrinkage | 0.0070 - 0.0090 cm/cm | 0.0070 - 0.0090 in/in | ASTM D955 |
|
PlastxWorld CEVIAN® B1500 PBT/ABS Alloy
Unfilled, Excellent ToughnessThese are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc.
|
|||
| Linear Mold Shrinkage | 0.0070 cm/cm | 0.0070 in/in | ASTM D955 |
|
Tipco Tipcolene® SEB 100 - 10% Chemically Coupled Glass Fiber Polypropylene Homopolymer with High Heat Stability
10% Chemically Coupled Glass Reinforced PP HomopolymerApplications: General PurposeProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India.
|
|||
| Linear Mold Shrinkage |
0.0070
cm/cm @Thickness 3.175 mm |
0.0070
in/in @Thickness 0.1250 in |
ASTM D955 |
|
A. Schulman ComAlloy® E-12421 Reinforced High Flow Polyamide
Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line.
|
|||
| Linear Mold Shrinkage | 0.0070 cm/cm | 0.0070 in/in | |
|
E-Polymers TEKAMID® H14HR High Toughness Heat Resistance PA/ABS Alloy
Polyamide (Nylon) Resin. TEKAMID is widely being used in manufacturing of automotive and industrial parts with its outstanding mechanical, thermal and chemical properties.H-series: PA6/ABS, PA66/AB..
|
|||
| Linear Mold Shrinkage | 0.0070 cm/cm | 0.0070 in/in | |
|
E-Polymers TEKAMID® H14HT High Toughness PA/ABS Alloy
Polyamide (Nylon) Resin. TEKAMID is widely being used in manufacturing of automotive and industrial parts with its outstanding mechanical, thermal and chemical properties.H-series: PA6/ABS, PA66/AB..
|
|||
| Linear Mold Shrinkage | 0.0070 cm/cm | 0.0070 in/in | MD; ASTM D955 |
|
Aclo Accutech Polypropylene Copolymer CP0436W30L Wollastonite Reinforced |
|||
| Linear Mold Shrinkage | 0.0070 cm/cm | 0.0070 in/in | MD; ASTM D955 |
|
Aclo Accutech Polypropylene Copolymer CP0437M30L Mica Reinforced |
|||
| Linear Mold Shrinkage | 0.0070 cm/cm | 0.0070 in/in | MD; ASTM D955 |
|
Aclo Accutech Polypropylene Homopolymer HP0334M30CL Mica Reinforced Coupled |
|||
| Linear Mold Shrinkage | 0.0070 cm/cm | 0.0070 in/in | MD; ASTM D955 |
|
Aclo Accutech Polypropylene Copolymer CP0436M20L Mica Reinforced |
|||
| Linear Mold Shrinkage | 0.0070 cm/cm | 0.0070 in/in | ASTM D955 |
|
Plenco 7321 Phenolic, Nodular, Injection Molded
PLENCO 07321 is an organic fiber reinforced phenolic molding compound, offering improved mechanical strength and excellent dimensional stability. Type ASTM 5948 CFI-5, and UL recognized under compon..
|
|||