| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Linear Mold Shrinkage |
0.0060
-
0.0080
cm/cm @Temperature 80.0 °C, Time 3600 sec |
0.0060
-
0.0080
in/in @Temperature 176 °F, Time 1.00 hour |
48 hours after molding; ISO 294-3/4 |
|
Mytex Polymers AS172LW-01US Thermoplastic Polyolefin, Compounded
AS172LW-01US is a compounded thermoplastic polyolefin (TPO) designed for exterior automotive applications requiring cold temperature impact, processability and paintability. Available in natural, g..
|
|||
| Linear Mold Shrinkage | 0.0030 - 0.0080 cm/cm | 0.0030 - 0.0080 in/in | ASTM D955 |
|
Polymer Resources NY66-FRG25 Flame Retardant Nylon 66, 25% Glass Reinforced
Nylon 66, 25% Glass Reinforced, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are..
|
|||
| Linear Mold Shrinkage | 0.0050 - 0.0080 cm/cm | 0.0050 - 0.0080 in/in | 0.125 in; ASTM D955 |
|
Ravago Manufacturing Americas Hylon® N1013STHL Nylon 6/6 (DAM)
Information provided by Ravago.
|
|||
| Linear Mold Shrinkage | 0.0060 - 0.0080 cm/cm | 0.0060 - 0.0080 in/in | DIN 53 464 |
|
Perstorp Compounds AMITEC 751 Melamine
Perstorp dinnerware compression and injection grade. Porcelain like properties suitable for household applications.Information provided by Perstorp Compounds Inc.
|
|||
| Linear Mold Shrinkage | 0.0060 - 0.0080 cm/cm | 0.0060 - 0.0080 in/in | With Flow; ISO 2577 |
|
Polykemi AB POLYabs F30 ABS
Information provided by Polykemi AB
|
|||
| Linear Mold Shrinkage | 0.0060 - 0.0080 cm/cm | 0.0060 - 0.0080 in/in | Across Flow; ISO 2577 |
|
Polykemi AB POLYfill PPH GF8020 PD2 Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled
Information provided by Polykemi AB
|
|||
| Linear Mold Shrinkage | 0.0070 - 0.0080 cm/cm | 0.0070 - 0.0080 in/in | ASTM D955 |
|
PolyOne Lubri-Tech™ AT-15GF/10T Acetal-Copolymer, Glass Filled, PTFE Lubricated
(discontinued **)
Description/Features:Glass Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation.
|
|||
| Linear Mold Shrinkage | 0.0040 - 0.0080 cm/cm | 0.0040 - 0.0080 in/in | |
|
Lehmann & Voss LUVOCOM® 1106-8032/GY Polyether imide, unreinforced, laser markable
Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le..
|
|||
| Linear Mold Shrinkage | 0.0060 - 0.0080 cm/cm | 0.0060 - 0.0080 in/in | |
|
Lehmann & Voss LUVOCOM® 50/TF/15/GY04 Polycarbonate, with PTFE
Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Improved friction and wear behaviour. Emergency running proper..
|
|||
| Linear Mold Shrinkage | 0.0030 - 0.0080 cm/cm | 0.0030 - 0.0080 in/in | |
|
Lehmann & Voss LUVOCOM® 80/CF/10/BK Polyacetal-copolymer, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Electrically conductive, suitable for continuous discharging of statically ..
|
|||
| Linear Mold Shrinkage | 0.0050 - 0.0080 cm/cm | 0.0050 - 0.0080 in/in | 0.125; ASTM D955 |
|
LTL Color Compounds ColorFast® FRPBT150 PBT, 13% Glass-Filled, Flame Retarded
13% glass-filled V-0 rated PBTAll information provided by LTL Color Compounders, Inc.
|
|||
| Linear Mold Shrinkage | 0.0050 - 0.0080 cm/cm | 0.0050 - 0.0080 in/in | ASTM D955 |
|
Mitsubishi Iupilon® H3000R 30 MFI Polycarbonate With Release
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
|
|||
| Linear Mold Shrinkage | 0.0040 - 0.0080 cm/cm | 0.0040 - 0.0080 in/in | |
|
Lucite International Diakon® TD510 Toughened Acrylic Compound
The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness.The grades in the Diakon® series can be processed by..
|
|||
| Linear Mold Shrinkage | 0.0040 - 0.0080 cm/cm | 0.0040 - 0.0080 in/in | |
|
Lucite International Diakon® TD735 Toughened Acrylic Compound
The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness.The grades in the Diakon® series can be processed by..
|
|||
| Linear Mold Shrinkage | 0.0050 - 0.0080 cm/cm | 0.0050 - 0.0080 in/in | ASTM D955 |
|
Star Plastics ABSFR1 Molding Grade ABSFR
Information provided by Star Plastics, Inc.
|
|||
| Linear Mold Shrinkage | 0.0060 - 0.0080 cm/cm | 0.0060 - 0.0080 in/in | as molded |
|
A. Schulman POLYTROPE™ TPP 530 Injection Molding Grade Olefinic Thermoplastic Elastomer
DescriptionPolytrope TPP 530 is an injection molding grade olefinic thermoplastic elastomer. This mineral filled product is recommended for applications requiring high stiffness and low thermal exp..
|
|||
| Linear Mold Shrinkage | 0.0040 - 0.0080 cm/cm | 0.0040 - 0.0080 in/in | ISO 294-4 |
|
Wellman Wellamid® GF14-60 XE-N 14% Glass Fiber Reinforced Nylon 6, Lubricated & Heat Stabilized
Typical Applications: Radio and TV components, dishwasher roller carriages, chain saw oil reservoirs, gears, housings, door & window latches, power hand tool housings, high temperature devices.Data ..
|
|||
| Linear Mold Shrinkage | 0.0040 - 0.0080 cm/cm | 0.0040 - 0.0080 in/in | D955 |
|
Zhejiang Juner 201-G30 30% Glass Fibre Reinforced
Applications: Electrons and Electricity: TV Components, Plugs of Computers, Exhaust Fans of Computers, Plugs, Sockets, Shells of Electronics, Framework of Level Output Transformers, Pipe Pedestals, ..
|
|||
| Linear Mold Shrinkage | 0.0040 - 0.0080 cm/cm | 0.0040 - 0.0080 in/in | D955 |
|
Zhejiang Juner 301-G20 20% Glass Fibre Reinforced and Flammable Resistant
Applications: Electrons and Electricity: TV Components, Plugs of Computers, Exhaust Fans of Computers, Plugs, Sockets, Shells of Electronics, Framework of Level Output Transformers, Pipe Pedestals, ..
|
|||
| Linear Mold Shrinkage | 0.0060 - 0.0080 cm/cm | 0.0060 - 0.0080 in/in | ASTM D 955 |
|
Cossa Polimeri ESTAPROP H 0560 GFCTG Polypropylene, 30% Mixed Filler
PP homopolymer 30% mixed fillerGood physical and mechanical characteristicsInformation provided by Cossa Polimeri S.r.l.
|
|||
| Linear Mold Shrinkage | 0.0060 - 0.0080 cm/cm | 0.0060 - 0.0080 in/in | ASTM D955 |
|
Covestro Makrolon® 3103 Polycarbonate
Injection molding and extrusion grade with high viscosity, UV stabilized, special grade for sheets.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Baye..
|
|||
| Linear Mold Shrinkage | 0.0040 - 0.0080 cm/cm | 0.0040 - 0.0080 in/in | ASTM D955 |
|
Diamond Polymers DIAMALOY 761 ABS/PC Alloy, Non-Halogen Flame Retardant with 5% PTFE
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
|
|||
| Linear Mold Shrinkage | 0.0060 - 0.0080 cm/cm | 0.0060 - 0.0080 in/in | ASTM D955 |
|
Covestro Makroblend® EL 703 Polycarbonate + Polyester-based Blend, Impact Modified, Flame-Retardant, UV Stabilized
Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.
|
|||
| Linear Mold Shrinkage | 0.0060 - 0.0080 cm/cm | 0.0060 - 0.0080 in/in | ASTM D955 |
|
Asahi Kasei Xyron® X05516 Modified Polyphenylene Ether
AutomotiveInformation provided by Asahi Kasei
|
|||
| Linear Mold Shrinkage | 0.0040 - 0.0080 cm/cm | 0.0040 - 0.0080 in/in | ASTM D955 |
|
Beijing Ranger Chem PBT-201-G30 291 Flame Retarding FR PBT
Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin..
|
|||
| Linear Mold Shrinkage | 0.0050 - 0.0080 cm/cm | 0.0050 - 0.0080 in/in | 0.125; ASTM D955 |
|
LTL Color Compounds ColorFast® GPA300 ABS
Super-tough ABS with our highest impact strength, injection moldingAll information provided by LTL Color Compounders, Inc.
|
|||
| Linear Mold Shrinkage | 0.0040 - 0.0080 cm/cm | 0.0040 - 0.0080 in/in | ASTM D955 |
|
LG Chemical HI835H PMMA, Impact Resistant Grade
Molding granule designed for greater impact strength combined with the outstanding properties of conventional acrylic materialsFeatures: Excellent transparency and eleganceWeather resistance and che..
|
|||