| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Linear Mold Shrinkage | 0.0090 cm/cm | 0.0090 in/in | ASTM D955 |
|
Multibase Multi-Pro® 4518 CUW Polypropylene
Calcium Carbonate Filler, 45% by weight.Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase
|
|||
| Linear Mold Shrinkage | 0.0090 cm/cm | 0.0090 in/in | ASTM D955 |
|
Multibase Nylex™ 2185 FR V0 Polyamide + PP
Features: Crack Resistance, GoodDimensional Stability, GoodImpact Resistance, GoodMoisture ResistantProcessability, GoodFlame RetardantForms:PelletsProcessing Methods:Injection MoldingUses: Electric..
|
|||
| Linear Mold Shrinkage | 0.0090 cm/cm | 0.0090 in/in | ASTM D955 |
|
RheTech Products M25UVP250-01 25% Mica Reinforced Polypropylene Copolymer, UV Stabilized, Black
Applications: BracketsCowl screensRigid exterior componentsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Linear Mold Shrinkage | 0.0090 cm/cm | 0.0090 in/in | ASTM D955 |
|
Nylene® PA6 Homopolymer 201 Nylon 6; Low Viscosity Nucleated
Dry as molded.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation.
|
|||
| Linear Mold Shrinkage | 0.0090 cm/cm | 0.0090 in/in | With Flow; ISO 2577 |
|
Polykemi AB SCANLON A 5005B UV PA/ABS-Blend
Information provided by Polykemi AB
|
|||
| Linear Mold Shrinkage | 0.0090 cm/cm | 0.0090 in/in | Across Flow; ISO 2577 |
|
Polykemi AB SCANMID 6 B22^ E F20 Nylon 6, Glass Fiber Reinforced, Modified
Information provided by Polykemi AB
|
|||
| Linear Mold Shrinkage | 0.0090 - 0.017 cm/cm | 0.0090 - 0.017 in/in | FRISETTA Test Method |
|
Nilit FRIANYL A63 GV 5 Nylon 6.6 for injection molding, 5% glass fiber reinforced
Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics
|
|||
| Linear Mold Shrinkage |
0.0090
-
0.011
cm/cm @Thickness 6.35 mm |
0.0090
-
0.011
in/in @Thickness 0.250 in |
ASTM D955 |
|
Fiberfil® J-60/GB/20 Polypropylene Homopolymer, 20% Glass beads
Information provided by FIBERFIL Engineered Plastics
|
|||
| Linear Mold Shrinkage | 0.0090 - 0.014 cm/cm | 0.0090 - 0.014 in/in | |
|
Lehmann & Voss LUVOCOM® 80-8222 Polyacetal-copolymer, with mineral filler, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri..
|
|||
| Linear Mold Shrinkage | 0.0090 cm/cm | 0.0090 in/in | |
|
Metton LMR M1534 Liquid Molding Resin
Different product numbers represent different formulations for customer specific needs such as liquid freezing point. Metton LMR is a tough and durable engineering plastic material used to produce ..
|
|||
| Linear Mold Shrinkage | 0.0090 cm/cm | 0.0090 in/in | ISO 2577 |
|
LyondellBasell Astryn EPKT25M Polypropylene Copolymer, Mineral Filled
Key Features: conventional melt flow, very high modulus, mineral-filled polypropylene copolymer, high rigidity, good impact resistance, good dimensional stability, low foggingApplications: glove box..
|
|||
| Linear Mold Shrinkage | 0.0090 cm/cm | 0.0090 in/in | Tool, Montell |
|
LyondellBasell Hifaxâ„¢ CB228 Thermoplastic Olefin Resin
Key Features: medium melt flow, medium high modulus, paintable thermoplastic elastomeric olefin resin, excellent impact and stiffness balance, good paintability, good processabilityApplications: aut..
|
|||
| Linear Mold Shrinkage | 0.0090 - 0.011 cm/cm | 0.0090 - 0.011 in/in | |
|
A. Schulman POLYTROPE™ TPP 293 Injection Molding Grade Olefinic Thermoplastic Elastomer
DescriptionPolytrope TPP293 is an injection molding grade olefinic thermoplastic elastomer. This product is recommended for parts requiring excellent low temperature impact properties with good dim..
|
|||
| Linear Mold Shrinkage | 0.0090 - 0.011 cm/cm | 0.0090 - 0.011 in/in | |
|
A. Schulman POLYTROPE™ TPP 504 Injection Molding Grade Olefinic Thermoplastic Elastomer
DescriptionPolytrope TPP 504 is an injection molding grade olefinic thermoplastic elastomer. This product is recommended for parts requiring flexibility and high impact strength at sub-ambient temp..
|
|||
| Linear Mold Shrinkage | 0.0090 cm/cm | 0.0090 in/in | ± 0.1 after 30 min. at 120°C |
|
A. Schulman POLYTROPE™ TPP 530 Injection Molding Grade Olefinic Thermoplastic Elastomer
DescriptionPolytrope TPP 530 is an injection molding grade olefinic thermoplastic elastomer. This mineral filled product is recommended for applications requiring high stiffness and low thermal exp..
|
|||
| Linear Mold Shrinkage | 0.0090 cm/cm | 0.0090 in/in | average process; in flow; 150x80x2mm |
|
Borealis PS65C40 Polypropylene Compound, Mineral Filled
PS65C40 is a 40% mineral filled polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness, gives a good surface quality and..
|
|||
| Linear Mold Shrinkage | 0.0090 cm/cm | 0.0090 in/in | ASTM D955 |
|
Plenco 2571 Phenolic, Granular, Injection Molded
PLENCO 02571 is a general purpose, organic filled phenolic molding compound offering optimum cure characteristics while maintaining excellent mechanical and electrical properties. UL recognized unde..
|
|||
| Linear Mold Shrinkage | 0.0090 - 0.012 cm/cm | 0.0090 - 0.012 in/in | ASTM D955 |
|
A. Schulman POLYFLAM™ RPP 1174 Talc Filled, Homopolymer Polypropylene
DescriptionPolyflam® RPP 1174 is a high performance talc filled homopolymer polypropylene product with UL V0 flammability and 105°C temperature index at 0.81 mm. RPP 1174 is non-dripping and has ..
|
|||
| Linear Mold Shrinkage | 0.0090 cm/cm | 0.0090 in/in | |
|
Tisan TISOPLEN® 30% Calcite Filled Heat Stabilized Homopolymer Polypropylene
TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois..
|
|||
| Linear Mold Shrinkage | 0.0090 - 0.011 cm/cm | 0.0090 - 0.011 in/in | |
|
A. Schulman POLYTROPE™ TPP 503 Injection Molding Grade Olefinic Thermoplastic Elastomer
DescriptionPolytrope TPP 503 is an injection molding grade olefinic thermoplastic elastomer. This product is recommended for parts requiring flexibility and high impact strength at sub-ambient temp..
|
|||
| Linear Mold Shrinkage |
0.0090
cm/cm @Thickness 3.175 mm |
0.0090
in/in @Thickness 0.1250 in |
ASTM D955 |
|
A. Schulman ComAlloy® E-12812 Easy Flow Glass Reinforced Nylon 66
Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line.
|
|||
| Linear Mold Shrinkage | 0.0090 cm/cm | 0.0090 in/in | ASTM D955 |
|
Buckeye Polymers BP RPP 2020T Polypropylene, 20% Mineral Filled
This Talc-filled product exhibits excellent properties such as high stiffness, surface aesthetics, low coefficient of thermal expansion, low shrinkage, improved scratch and mar resistance, and resis..
|
|||
| Linear Mold Shrinkage | 0.0090 cm/cm | 0.0090 in/in | ASTM Data; MD |
|
BASF Ultramid® 8202C HS BK-102 PA6 (Conditioned)
Ultramid 8202C HS BK-102 is a heat stabilized, low viscosity, pigmented black, PA6, injection molding homopolymer possessing a modified crystalline structure for increased property performance and f..
|
|||
| Linear Mold Shrinkage | 0.0090 cm/cm | 0.0090 in/in | ASTM Data; MD |
|
BASF Ultramid® 8260 HS BK-102 40% Mineral Filled PA6 (Conditioned)
Ultramid 8260 HS BK-102 is a heat stabilized, pigmented black, 40% mineral reinforced PA6 injection molding resin. It possesses high stiffness, dimensional stability and heat resistance combined wi..
|
|||
| Linear Mold Shrinkage | 0.0090 cm/cm | 0.0090 in/in | Transfer; ASTM D955 |
|
Chang Chun Plastic Longlite PM T357 Electrical Phenolic Molding Compound
ASTM Grades per ASTM D700 are 2, 3.Information provided by Dowell Trading Company Ltd.
|
|||
| Linear Mold Shrinkage | 0.0090 - 0.011 cm/cm | 0.0090 - 0.011 in/in | With Flow; ISO 2577 |
|
Polykemi AB POLYfill PPH TS8038 Polypropylene Homopolymer, Mineral Reinforced
Information provided by Polykemi AB
|
|||
| Linear Mold Shrinkage | 0.0090 - 0.011 cm/cm | 0.0090 - 0.011 in/in | |
|
A. Schulman POLYTROPE™ TPP 504 Injection Molding Grade Olefinic Thermoplastic Elastomer
DescriptionPolytrope TPP 504 is an injection molding grade olefinic thermoplastic elastomer. This product is recommended for parts requiring flexibility and high impact strength at sub-ambient temp..
|
|||
| Linear Mold Shrinkage | 0.0090 - 0.012 cm/cm | 0.0090 - 0.012 in/in | after bake; ISO 294 |
|
Solvay Engineered Polymers DEXFLEX® 930 TPO
(discontinued **)
Description: DEXFLEX® 930 is a thermoplastic olefinic elastomer (TPO) designed for large automotive exterior applications that require high flow for excellent processability, ductile impact propert..
|
|||
| Linear Mold Shrinkage | 0.0090 - 0.012 cm/cm | 0.0090 - 0.012 in/in | as molded; ISO 294 |
|
Solvay Engineered Polymers DEXFLEX® 980HF TPO
(discontinued **)
Description: DEXFLEX® 980HF is a thermoplastic olefinic elastomer (TPO) designed for large automotive exterior applications that require high flow for excellent processability, ductile impact prope..
|
|||
| Linear Mold Shrinkage | 0.0090 cm/cm | 0.0090 in/in | ASTM D955 |
|
Teknor Apex Sinpolene CPP2030 Polypropylene
Availability: Africa & Middle East; Latin America; Asia Pacific; South America Calcium Carbonate Filler, 30% Filler by Weight Features: Copolymer Uses: Automotive Applications; Industrial Applicati..
|
|||