| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Linear Mold Shrinkage | 0.0095 cm/cm | 0.0095 in/in | ASTM D955 |
|
RheTech Products FT4802-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black
Applications: Bodyside moldings and claddingsFacia and bumper coversExterior componentsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Linear Mold Shrinkage | 0.0095 cm/cm | 0.0095 in/in | ASTM D955 |
|
RheTech Products FT4802-690UV Thermoplastic Polyolefin, UV Stabilized, HS5 Medium Dark Neutral
Applications: Bodyside moldings and claddingsFacia and bumper coversExterior componentsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Linear Mold Shrinkage | 0.0095 cm/cm | 0.0095 in/in | ASTM D955 |
|
RheTech Products FT4802-690UVA Thermoplastic Polyolefin, UV Stabilized, HS5 Medium Dark Neutral
Applications: Bodyside moldings and claddingsFacia and bumper coversExterior componentsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Linear Mold Shrinkage | 0.0095 cm/cm | 0.0095 in/in | ASTM D955 |
|
RheTech Products FT4802-691UV Thermoplastic Polyolefin, UV Stabilized, RJ3 Dark Grey Green
Applications: Bodyside moldings and claddingsFacia and bumper coversExterior componentsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Linear Mold Shrinkage | 0.0095 cm/cm | 0.0095 in/in | ASTM D955 |
|
RheTech Products FT4802-692UV Thermoplastic Polyolefin, UV Stabilized, RS8 Grey
Applications: Bodyside moldings and claddingsFacia and bumper coversExterior componentsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Linear Mold Shrinkage | 0.0095 cm/cm | 0.0095 in/in | ASTM D955 |
|
RheTech Products FT4802-693UV Thermoplastic Polyolefin, UV Stabilized, SPN Dark Teal
Applications: Bodyside moldings and claddingsFacia and bumper coversExterior componentsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Linear Mold Shrinkage | 0.0095 cm/cm | 0.0095 in/in | ASTM D955 |
|
RheTech Products T40P100-01 40% Talc Reinforced Polypropylene, Black
Applications: Wire troughBracketsConsolesFan shroudsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Linear Mold Shrinkage | 0.0095 cm/cm | 0.0095 in/in | ASTM D955 |
|
RheTech Products T40P100-04 40% Talc Reinforced Polypropylene, White
Applications: Automotive componentsConsumer productsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Linear Mold Shrinkage | 0.0095 cm/cm | 0.0095 in/in | ASTM D955 |
|
RheTech Products T40P105-01 40% Talc Reinforced Polypropylene, Black
Applications: Underhood componentsHVAC ductworkInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Linear Mold Shrinkage | 0.0095 cm/cm | 0.0095 in/in | ASTM D955 |
|
RheTech Products T40P105-04 40% Talc Reinforced Polypropylene, White, 5% Titanium Dioxide
Applications: Instrument cluster masksAutomotive componentsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Linear Mold Shrinkage | 0.0095 cm/cm | 0.0095 in/in | ASTM D955 |
|
RheTech Products T40P106-01 40% Talc Reinforced Polypropylene, Black
Applications: Underhood componentsHVAC ductworkFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Linear Mold Shrinkage | 0.0095 cm/cm | 0.0095 in/in | ASTM D955 |
|
RheTech Products T40P108-01 40% Talc Reinforced Polypropylene, Black
Applications: Wire troughBracketsConsolesFan shroudsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Linear Mold Shrinkage | 0.0095 cm/cm | 0.0095 in/in | |
|
Plastcom SLOVALEN PH 56 T FRD 1 PP, flame retardant
FeaturesModified homopolymer PP for injection moulding with decreased flammability. Contains flame retardant on the halogen basis. Used in the electrical industry - terminals, coil forms, guides, co..
|
|||
| Linear Mold Shrinkage | 0.0095 cm/cm | 0.0095 in/in | mold average;Borealis Method |
|
Borealis Daplen™ EE188HP Polypropylene TPO Compound
Daplen™ EE188HP is a 15% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and g..
|
|||
| Linear Mold Shrinkage | 0.0095 cm/cm | 0.0095 in/in | Borealis Method |
|
Borealis Daplen™ EF040AE TPO Compound
Daplen EF040AE is a elastomer modified polypropylene compound intended for injection molding. Daplen EF040AE is a material with excellent impact/stiffness ratio. Thanks to its low thermal expansio..
|
|||
| Linear Mold Shrinkage | 0.0095 cm/cm | 0.0095 in/in | Borealis Method |
|
Borealis Daplen™ EG102AI Polypropylene Compound 15% Mineral Filled
Daplen EF102AI is a 15% mineral filled polypropylene compound intended injection molding. EG102AI is an easy flow grade, specially developed for the car industry. Daplen EF102AI has been developed..
|
|||
| Linear Mold Shrinkage | 0.0095 cm/cm | 0.0095 in/in | Borealis Method |
|
Borealis Xmod™ GD301FE Polypropylene, Glass Fiber Reinforced
Xmod™ GD301FE is a 30 % chemically coupled high performance glass fiber reinforced polypropylene compound intended for injection molding. This material shows excellent mechanical properties also a..
|
|||
| Linear Mold Shrinkage | 0.0095 - 0.012 cm/cm | 0.0095 - 0.012 in/in | ASTM D955 |
|
Buckeye Polymers BP FLEX D6017 T BLK Thermoplastic Polyolefin
Product Information: TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment.Processing Method: Injection Mold..
|
|||
| Linear Mold Shrinkage | 0.0095 - 0.012 cm/cm | 0.0095 - 0.012 in/in | ASTM D955 |
|
Buckeye Polymers BP FLEX D6020-08 BLK Thermoplastic Polyolefin
Product Information: TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment.Product Features:High tear resist..
|
|||
| Linear Mold Shrinkage | 0.0095 cm/cm | 0.0095 in/in | |
|
Plastcom SLOVALEN PQ 83 T 40 PP, 40% mineral filling
FeaturesModified PP for injection moulding with the content of 40% mineral filling, uv stabilized. Increased rigidity, strength and thermal use up to 130°C depending on the talc content. Decreased ..
|
|||
| Linear Mold Shrinkage | 0.0095 cm/cm | 0.0095 in/in | Injection; ASTM D955 |
|
Chang Chun Plastic Longlite PM T375J Heat Resistant Phenolic Molding Compound
ASTM Grade per ASTM D700 is 13.Information provided by Dowell Trading Company Ltd.
|
|||
| Linear Mold Shrinkage | 0.0095 - 0.015 cm/cm | 0.0095 - 0.015 in/in | ASTM D955 |
|
PolyOne Lubri-Tech™ AT-25GB/5T-2S Acetal-Copolymer, Glass Bead Filled, PTFE/Silicone Lubricated
(discontinued
Description/Features:Glass Bead FilledPTFE/Silicone LubricatedInformation provided by PolyOne Corporation.
|
|||
| Linear Mold Shrinkage | 0.0095 cm/cm | 0.0095 in/in | ASTM D955 |
|
RheTech Products HP507-01 38% Talc Reinforced High Performance Polypropylene, Non-UV Stabilized, Black
Applications: IP structural componentsSpeaker housingsAutomotive interior componentsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||