| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Linear Mold Shrinkage | 0.0090 - 0.017 cm/cm | 0.0090 - 0.017 in/in | FRISETTA Test Method |
|
Nilit FRIANYL A63 SG40 Nylon 6.6 for injection molding, 40% mineral filled
Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics
|
|||
| Linear Mold Shrinkage | 0.0080 - 0.017 cm/cm | 0.0080 - 0.017 in/in | FRISETTA Test Method |
|
Nilit FRIANYL B63 H-KV30 Nylon 6 for injection molding, 30% glass ball reinforced
Nylon 6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics
|
|||
| Linear Mold Shrinkage | 0.0080 - 0.017 cm/cm | 0.0080 - 0.017 in/in | FRISETTA Test Method |
|
Nilit FRIANYL B63 KV30 Nylon 6 for injection molding, 30% glass ball reinforced
Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics
|
|||
| Linear Mold Shrinkage | 0.0060 - 0.017 cm/cm | 0.0060 - 0.017 in/in | FRISETTA Test Method |
|
Nilit RECONYL B GV30 Recycled nylon 6 for injection molding, 30% glass fiber reinforced
Recycled nylon 6 for injection molding (available only in black).Information provided by Frisetta Polymer, which merged into Nilit Plastics
|
|||
| Linear Mold Shrinkage | 0.014 - 0.017 cm/cm | 0.014 - 0.017 in/in | as molded; ISO 294 |
|
Solvay Engineered Polymers DEXFLEX® 810HSF TPO
(discontinued **)
Description: DEXFLEX® 810HSF is a thermoplastic olefinic elastomer (TPO) designed for large molded-in-color automotive exterior applications that require high flow characteristics for excellent pro..
|
|||
| Linear Mold Shrinkage | 0.0090 - 0.017 cm/cm | 0.0090 - 0.017 in/in | FRISETTA Test Method |
|
Nilit FRIANYL A63 GV 5 Nylon 6.6 for injection molding, 5% glass fiber reinforced
Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics
|
|||
| Linear Mold Shrinkage | 0.0080 - 0.017 cm/cm | 0.0080 - 0.017 in/in | FRISETTA Test Method |
|
Nilit RECONYL A SG30 Recycled nylon 6.6 for injection molding, 30% mineral filled
Recycled nylon 6.6 for injection molding (available only in black).Information provided by Frisetta Polymer, which merged into Nilit Plastics
|
|||
| Linear Mold Shrinkage | 0.012 - 0.017 cm/cm | 0.012 - 0.017 in/in | |
|
Lehmann & Voss LUVOCOM® 1/TF/18/SI/2/BK Polyamide 66, with PTFE, lubricant modified, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri..
|
|||
| Linear Mold Shrinkage | 0.012 - 0.017 cm/cm | 0.012 - 0.017 in/in | ASTM D955 |
|
Kolon KOPA® KN133HR Heat Resistant Nylon 6
KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr..
|
|||
| Linear Mold Shrinkage | 0.015 - 0.017 cm/cm | 0.015 - 0.017 in/in | ASTM D955 |
|
Samyang Triel® 5301SP Thermoplastics Polyetherester Elastomer, Double Extrusion
Excellent mechanical characteristics, elasticity, thermal resistance and chemical resistance.5301SP is intended for double extrusion.Information provided by Samyang.
|
|||
| Linear Mold Shrinkage | 0.015 - 0.017 cm/cm | 0.015 - 0.017 in/in | ASTM D955 |
|
Samyang Triel® 5350 Thermoplastics Polyetherester Elastomer, General Extrusion
Excellent mechanical characteristics, elasticity, thermal resistance and chemical resistance.5350 is an extrusion grade.Applications: Elastic threadInformation provided by Samyang.
|
|||
| Linear Mold Shrinkage | 0.015 - 0.017 cm/cm | 0.015 - 0.017 in/in | ASTM D955 |
|
Samyang Triel® 5401BM Thermoplastics Polyetherester Elastomer, Blow Molding
Excellent mechanical characteristics, elasticity, thermal resistance and chemical resistance.5401BM is for blow molding applications.Applications: Automotive - CVJB and BellowsInformation provided ..
|
|||
| Linear Mold Shrinkage | 0.013 - 0.017 cm/cm | 0.013 - 0.017 in/in | aged 48 hrs at 80; ISO 294 |
|
A. Schulman FORMION™ FI 391 Ionomer
DescriptionFormion® FI 391 is a non-reinforced, injection molding grade Ionomer, which has been formulated for scratch resistance, low temperature ductility, and medium stiffness. Formion F1 391U i..
|
|||
| Linear Mold Shrinkage | 0.013 - 0.017 cm/cm | 0.013 - 0.017 in/in | aged 48 hrs at 80; ISO 294 |
|
A. Schulman FORMION™ FI 391 Ionomer
DescriptionFormion® FI 391 is a non-reinforced, injection molding grade Ionomer, which has been formulated for scratch resistance, low temperature ductility, and medium stiffness. Formion F1 391U i..
|
|||
| Linear Mold Shrinkage | 0.013 - 0.017 cm/cm | 0.013 - 0.017 in/in | ISO 2577 |
|
Polyram PlusTek PB200 Nylon 6 for Extrusion
High viscosity Nylon 6, formulated for extrusion application.Information provided by Polyram.
|
|||
| Linear Mold Shrinkage | 0.012 - 0.017 cm/cm | 0.012 - 0.017 in/in | ASTM D955 |
|
Clariant BRU2000 Nylon 66, Lubricated, Nucleated, Weather Resistant, Black
Data provided by Clariant Masterbatches
|
|||
| Linear Mold Shrinkage | 0.014 - 0.017 cm/cm | 0.014 - 0.017 in/in | after bake; ISO 294 |
|
Solvay Engineered Polymers DEXFLEX® 930HS TPO
(discontinued **)
Description: DEXFLEX® 930HS is a thermoplastic olefinic elastomer (TPO) designed for large automotive exterior applications that require high flow for excellent processability, ductile impact prope..
|
|||
| Linear Mold Shrinkage | 0.015 - 0.017 cm/cm | 0.015 - 0.017 in/in | ASTM D955 |
|
Samyang Triel® 5206SP Thermoplastics Polyetherester Elastomer, Double Extrusion
Excellent mechanical characteristics, elasticity, thermal resistance and chemical resistance.5206SP is intended for double extrusion.Information provided by Samyang.
|
|||
| Linear Mold Shrinkage | 0.015 - 0.017 cm/cm | 0.015 - 0.017 in/in | ASTM D955 |
|
Samyang Triel® 5500 Thermoplastics Polyetherester Elastomer, General Extrusion
Excellent mechanical characteristics, elasticity, thermal resistance and chemical resistance.5500 is an extrusion grade.Information provided by Samyang.
|
|||