| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Linear Mold Shrinkage, Flow | 0.00 - 0.0010 cm/cm @Thickness 3.20 mm |
0.00 - 0.0010 in/in @Thickness 0.126 in |
SABIC Method |
| SABIC Innovative Plastics Geloy FXTW30PE ASA Pearlescent GELOY ASA resin with copper-look for capstock extrusion. Outstanding weatherability.This data was supplied by SABIC-IP for the Americas region. |
|||
| Linear Mold Shrinkage, Flow | 0.00 cm/cm | 0.00 in/in | Conditioned; ASTM D955 |
| Solvay Specialty Polymers Amodel® AS-1133 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater than 0.. |
|||
| Linear Mold Shrinkage, Flow | 0.00 - 0.0020 cm/cm @Thickness 3.18 mm |
0.00 - 0.0020 in/in @Thickness 0.125 in |
5" x 0.5" x 0.125" bars; ASTM D955 |
| Solvay Specialty Polymers AvaSpire® AV-651 CF30 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-651 CF30 is a 30% carbon fiber reinforced version of AvaSpire AV-651. This formulation offers some advantages relative to 30% carbon fiber reinforced PEEK which include better dimensiona.. |
|||
| Linear Mold Shrinkage, Flow | 0.00 - 0.0020 cm/cm @Thickness 3.18 mm |
0.00 - 0.0020 in/in @Thickness 0.125 in |
5" x 0.5" x 0.125" bars; ASTM D955 |
| Solvay Specialty Polymers AvaSpire® AV-722 CF30 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-722 CF30 is a 30% carbon fiber reinforced version of AvaSpire AV-722. This formulation offers improved part economics relative to 30% carbon fiber reinforced PEEK while retaining most of.. |
|||
| Linear Mold Shrinkage, Flow | 0.00 - 0.0020 cm/cm | 0.00 - 0.0020 in/in | ASTM D955 |
| Solvay Specialty Polymers AvaSpire® AV-848 CF30 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-848 CF30 is a 30% carbon fiber-reinforced, high-temperature, polyaryletherketone (PAEK) that has been specifically formulated to provide several performance advantages over comparable gr.. |
|||
| Linear Mold Shrinkage, Flow | 0.00 - 0.0020 cm/cm @Thickness 3.18 mm |
0.00 - 0.0020 in/in @Thickness 0.125 in |
5" x 0.5" x 0.125" bars; ASTM D955 |
| Solvay Specialty Polymers KetaSpire® KT-820 CF30 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-820 CF30 is the low-flow, 30% carbon-fiber reinforced grade of polyetheretherketone (PEEK). Carbon- fiber reinforcement of KetaSpire PEEK provides the maximum levels of mechanical prope.. |
|||
| Linear Mold Shrinkage, Flow | 0.00 - 0.0020 cm/cm @Thickness 3.18 mm |
0.00 - 0.0020 in/in @Thickness 0.125 in |
5" x 0.5" x 0.125" bars; ASTM D955 |
| Solvay Specialty Polymers KetaSpire® KT-820 SL45 Polyetheretherketone (PEEK)
(Unverified Data**) Ketaspire KT-820 SL45 is a PEEK based compound specifically designed to provide exceptionally low wear rates and good mechanical properties in applications where an external lubricant is provided.In.. |
|||
| Linear Mold Shrinkage, Flow | 0.00 - 0.0010 cm/cm @Thickness 3.20 mm |
0.00 - 0.0010 in/in @Thickness 0.126 in |
SABIC Method |
| SABIC Innovative Plastics Geloy FXTW30CP ASA Pearlescent GELOY ASA resin with copper-look for capstock extrusion. Outstanding weatherability.This data was supplied by SABIC-IP for the Americas region. |
|||
| Linear Mold Shrinkage, Flow | 0.00 cm/cm | 0.00 in/in | 85°C nozzle, 190°C tool; ISO 294-4 |
| Victrex® PEEK 90HMF20 Polyetheretherketone (PEEK), 20% Carbon Fiber Reinforced Product Description: High performance thermoplastic material, 20% carbon fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding, very easy flow, color black.T.. |
|||
| Linear Mold Shrinkage, Flow | 0.00 cm/cm | 0.00 in/in | 380°C nozzle, 190°C tool; ISO 294-4 |
| Victrex® PEEK 90HMF40 Polyetheretherketone (PEEK), 40% Carbon Fiber Reinforced Product Description: High performance thermoplastic material, 40% carbon fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding, easy flow, color black.Typica.. |
|||
| Linear Mold Shrinkage, Flow | 0.00 cm/cm | 0.00 in/in | Compression molding; ISO 2577 |
| Hexion Bakelite™ PF 1107 Phenolic Formaldehyde Resin, Low Shrinkage, Resistant to High Temperatures
(disconti Phenolic molding compound, inorganically filled, glass fiber reinforced, high heat resistance, low heat expansion coefficient, highest resistance to pressure, high dimensional stability.Application .. |
|||
| Linear Mold Shrinkage, Flow | 0.00 cm/cm | 0.00 in/in | |
| Solvay Specialty Polymers Amodel® AS-1133 HS Polyphthalamide (PPA), 33% Glass Fiber (Conditioned) Amodel® AS-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater th.. |
|||
| Linear Mold Shrinkage, Flow | 0.00 - 0.0020 cm/cm @Thickness 3.18 mm |
0.00 - 0.0020 in/in @Thickness 0.125 in |
|
| Solvay Specialty Polymers AvaSpire® AV-621 CF30 Polyaryletherketone (PAEK), 30% Carbon Fiber AvaSpire® AV-621 CF30 is a 30% carbon fiber reinforced version of AvaSpire® AV-621. It offers better dimensional stability and warp resistance than 30% carbon fiber reinforced PEEK. The AV-621.. |
|||
| Linear Mold Shrinkage, Flow | 0.00 - 0.0020 cm/cm @Thickness 3.18 mm |
0.00 - 0.0020 in/in @Thickness 0.125 in |
|
| Solvay Specialty Polymers AvaSpire® AV-651 CF30 Polyaryletherketone (PAEK), 30% Carbon Fiber AvaSpire® AV-651 CF30 is a 30% carbon fiber reinforced version of AvaSpire® AV-651. This formulation offers some advantages relative to 30% carbon fiber reinforced PEEK which include better di.. |
|||
| Linear Mold Shrinkage, Flow | 0.00 - 0.0020 cm/cm @Thickness 3.18 mm |
0.00 - 0.0020 in/in @Thickness 0.125 in |
|
| Solvay Specialty Polymers AvaSpire® AV-722 CF30 Polyaryletherketone (PAEK), 30% Carbon Fiber AvaSpire® AV-722 CF30 is a 30% carbon fiber reinforced version of AvaSpire® AV-722. This formulation offers improved part economics relative to 30% carbon fiber reinforced PEEK while retaining.. |
|||
| Linear Mold Shrinkage, Flow | 0.00 - 0.0020 cm/cm | 0.00 - 0.0020 in/in | |
| Solvay Specialty Polymers AvaSpire® AV-848 CF30 Polyaryletherketone (PAEK), 30% Carbon Fiber AvaSpire® AV-848 CF30 is a 30% carbon fiber-reinforced, high-temperature, polyaryletherketone (PAEK) that has been specifically formulated to provide several performance advantages over comparabl.. |
|||
| Linear Mold Shrinkage, Flow | 0.00 - 0.0020 cm/cm @Thickness 3.18 mm |
0.00 - 0.0020 in/in @Thickness 0.125 in |
|
| Solvay Specialty Polymers KetaSpire® KT-820 CF30 Polyetheretherketone (PEEK), 30% Carbon Fiber KetaSpire® KT-820 CF30 is the low-flow, 30% carbon-fiber reinforced grade of polyetheretherketone (PEEK). Carbon- fiber reinforcement of KetaSpire® PEEK provides the maximum levels of mechanic.. |
|||
| Linear Mold Shrinkage, Flow | 0.00 - 0.0020 cm/cm @Thickness 3.18 mm |
0.00 - 0.0020 in/in @Thickness 0.125 in |
|
| Solvay Specialty Polymers KetaSpire® KT-820 SL45 Polyetheretherketone (PEEK) KetaSpire® KT-820 SL45 is a PEEK based compound specifically designed to provide exceptionally low wear rates and good mechanical properties in applications where an external lubricant is provide.. |
|||
| Linear Mold Shrinkage, Flow | 0.00 - 0.0020 cm/cm @Thickness 3.18 mm |
0.00 - 0.0020 in/in @Thickness 0.125 in |
|
| Solvay Specialty Polymers KetaSpire® KT-880 CF30 Polyetheretherketone (PEEK), 30% Carbon Fiber KetaSpire® KT-880 CF30 is a high flow, 30% carbon fiber reinforced grade of polyetheretherketone (PEEK). Carbon-fiber reinforcement of KetaSpire® PEEK provides the maximum levels of mechanical.. |
|||
| Linear Mold Shrinkage, Flow | 0.00 - 0.0015 cm/cm | 0.00 - 0.0015 in/in | |
| Solvay Specialty Polymers Torlon® 7130 Polyamide-imide (PAI), 30% Carbon Fiber Torlon® 7130 is an 30% carbon-fiber reinforced grade of polyamide-imide (PAI) resin. It offers high strength and modulus, exceptional creep resistance, and good fatigue resistance. It has thermal.. |
|||
| Linear Mold Shrinkage, Flow | 0.00 - 0.0020 cm/cm @Thickness 3.18 mm |
0.00 - 0.0020 in/in @Thickness 0.125 in |
5" x 0.5" x 0.125" bars; ASTM D955 |
| Solvay Specialty Polymers AvaSpire® AV-621 CF30 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-621 CF30 is a 30% carbon fiber reinforced version of AvaSpire AV-621. It offers better dimensional stability and warp resistance than 30% carbon fiber reinforced PEEK. The AV-621 CF30 gr.. |
|||
| Linear Mold Shrinkage, Flow | 0.00 - 0.0015 cm/cm | 0.00 - 0.0015 in/in | ASTM D955 |
| Solvay Specialty Polymers Torlon® 7130 Polyamide-imide (PAI)
(Unverified Data**) Torlon 7130 is an 30% carbon-fiber reinforced grade of polyamide-imide (PAI) resin. It offers high strength and modulus, exceptional creep resistance, and good fatigue resistance. It has thermal exp.. |
|||