Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.00050 - 0.00070 cm/cm
0.00050 - 0.00070 in/in
ASTM D955
LG Chemical Lupoy 1200-10 Polycarbonate Resin
Description: LUPOY PC 1200-10 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength...
Linear Mold Shrinkage, Flow 0.00050 - 0.00070 cm/cm
0.00050 - 0.00070 in/in
ASTM D955
LG Chemical Lupoy 1301-10 Polycarbonate Resin
Description: LUPOY PC 1301-10 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength...
Linear Mold Shrinkage, Flow 0.00050 - 0.00070 cm/cm
0.00050 - 0.00070 in/in
ASTM D955
LG Chemical Lupoy 1301EP-22 Polycarbonate Resin
Description: LUPOY PC 1301EP-22 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt..
Linear Mold Shrinkage, Flow 0.00050 - 0.00070 cm/cm
0.00050 - 0.00070 in/in
ASTM D955
LG Chemical Lupoy 1261-03 Polycarbonate Resin
Description: LUPOY PC 1261-03 resin is designed for extrusion blow molding(EBM) and injection stretch blow molding (ISBM) products. It exhibits an excellent physical property balance of heat resista..
Linear Mold Shrinkage, Flow 0.00050 - 0.00070 cm/cm
0.00050 - 0.00070 in/in
ASTM D955
LG Chemical Lupoy 1301V-7 Polycarbonate Resin
Description: LUPOY PC 1301V-07 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength..
Linear Mold Shrinkage, Flow 0.00050 - 0.00070 cm/cm
0.00050 - 0.00070 in/in
ASTM D955
LG Chemical Lupoy 1302-05 Polycarbonate Resin
Description: LUPOY 1302-5 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main..
Linear Mold Shrinkage, Flow 0.00050 - 0.00070 cm/cm
0.00050 - 0.00070 in/in
ASTM D955
LG Chemical Lupoy 1600-03 Polycarbonate Resin
Description: LUPOY PC 1600-03 resin is designed for extrusion products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Characteristics: ..
Linear Mold Shrinkage, Flow 0.00050 - 0.00070 cm/cm
0.00050 - 0.00070 in/in
ASTM D955
LG Chemical Lupoy 1621-02 Polycarbonate Resin
Description: LUPOY PC 1621-02 resin is designed for large injection stretch blow molding and extrusion blow molding parts. It exhibits an excellent physical property balance of heat resistance, tran..
Linear Mold Shrinkage, Flow 0.00050 - 0.00070 cm/cm
0.00050 - 0.00070 in/in
ASTM D955
LG Chemical Lupoy 3010-15 Polycarbonate Resin
Description: LUPOY PC 3010-15 resin is designed for injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Character..
Linear Mold Shrinkage, Flow 0.00050 - 0.00070 cm/cm
0.00050 - 0.00070 in/in
ASTM D955
LG Chemical Lupoy 3030-10 Polycarbonate Resin
Description: LUPOY PC 3030-10 resin is designed for injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Character..
Linear Mold Shrinkage, Flow 0.00050 - 0.00070 cm/cm
0.00050 - 0.00070 in/in
ASTM D955
LG Chemical Lupoy NF1005F 03R Polycarbonate Resin
Description: LUPOY NF 1005F03R, eco-friendly UL94 V0/1.5 mm, is designed for extrusion products. It combines an excellent physical property balance of heat resistance, transparency and impact streng..
Linear Mold Shrinkage, Flow 0.00050 - 0.00070 cm/cm
0.00050 - 0.00070 in/in
ASTM D955
LG Chemical Lupoy NF1009F 15 Polycarbonate Resin
Description: LUPOY NF 1009F15, eco-friendly UL94 V0/2.0 mm, is designed for extrusion and injection molding products. It combines an excellent physical property balance of heat resistance, transpare..
Linear Mold Shrinkage, Flow 0.00050 - 0.00070 cm/cm
0.00050 - 0.00070 in/in
ASTM D955
LG Chemical Lupoy 1300-12 Polycarbonate Resin
Description: LUPOY PC 1300-12 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength...
Linear Mold Shrinkage, Flow 0.00050 - 0.00070 cm/cm
0.00050 - 0.00070 in/in
ASTM D955
LG Chemical Lupoy 1302HP-10 Polycarbonate Resin
Description: LUPOY PC 1302HP-10 resin is designed for extrusion products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Characteristics..
Linear Mold Shrinkage, Flow 0.00050 - 0.00070 cm/cm
0.00050 - 0.00070 in/in
ASTM D955
LG Chemical Lupoy 1303AH-15 Polycarbonate Resin
Description: LUPOY PC 1303AH-15 Tint Polycarbonate Resin is designed for injection molding of auto-headlamps. It exhibits an excellent physical property balance of heat resistance, transparency and ..
Linear Mold Shrinkage, Flow 0.00050 cm/cm
0.00050 in/in
Post-shrinkage, 60x60x2; 120°C; 4 hour; ISO 294-4
Lanxess Durethan® AKV 40 H2.0 901510 Nylon 66, Glass Fiber Reinforced
PA 66, 40% glass fibers, injection molding, heat-aging stabilizedInformation provided by LANXESS.
Linear Mold Shrinkage, Flow 0.00050 cm/cm
0.00050 in/in
Post-shrinkage, 60x60x2; 120°C; 4 hour; ISO 294-4
Lanxess Durethan® BKV 30 H2.0 EF DUS029 901510 Nylon 6, Glass Fiber Reinforced
PA 6, 30% glass fibers, injection molding, improved flowability, heat-aging stabilizedInformation provided by LANXESS.
Linear Mold Shrinkage, Flow 0.00050 - 0.0020 cm/cm
0.00050 - 0.0020 in/in
LATI Laramid K/40 HM PPA, 40% Carbon Fiber Reinforced
Semi-aromatic polyamide (PPA) based compound. Carbon fiber. High tensile modulus. Very good thermal properties. Good chemical resistance. Low moisture absorption.Availability: Africa & Middle East; ..
Linear Mold Shrinkage, Flow 0.00050 - 0.0025 cm/cm
0.00050 - 0.0025 in/in
on Tensile Bar; SABIC Method
SABIC Innovative Plastics LNP LUBRICOMP OCL13XXP PPS - LINEAR (Europe-Africa-Middle East)
LNP* Stat-kon* OCL13XXP is a compound based on PPS - LINEAR resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive.
Linear Mold Shrinkage, Flow 0.00050 - 0.0015 cm/cm
0.00050 - 0.0015 in/in
SABIC Method
SABIC Innovative Plastics LNP Lubricomp UCL36AS PPA (Europe-Africa-Middle East)
LNP* LUBRICOMP* UCL36AS is a compound based on Polyphthalamide resin containing Carbon Fiber, PTFE. Added features include; Internally Lubricated, Electrically Conductive, Heat Stabilized.This data ..
Linear Mold Shrinkage, Flow 0.00050 - 0.0015 cm/cm
<br>@Time 86400 sec
0.00050 - 0.0015 in/in
<br>@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP STAT-KON DX13320C PC COPOLYMER (Asia Pacific)
LNP* Statkon DX13320C is ultra clean polycarbonate/carbon fiber compound with high modulus, good flow ability, easy mold release, and high level of cleanliness for the most demanding application. A ..
Linear Mold Shrinkage, Flow 0.00050 - 0.0015 cm/cm
<br>@Thickness 3.20 mm
0.00050 - 0.0015 in/in
<br>@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics LNP STAT-KON Lexan_LCF1506 PC (Europe-Africa-Middle East)
LNP* Stat-kon* Lexan_LCF1506 is a 15% carbon fiber, 6% PTFE reinforced polycarbonate.
Linear Mold Shrinkage, Flow 0.00050 - 0.0015 cm/cm
<br>@Thickness 3.20 mm
0.00050 - 0.0015 in/in
<br>@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics LNP STAT-KON Noryl_HMC3008A PPE+PS
LNP* Stat-kon* Noryl_HMC3008A compound is a 30% glass/mineral/carbon fiber reinforced resin; static dissipative; 250F (120C) HDT. Tight tolerance molding.
Linear Mold Shrinkage, Flow 0.00050 - 0.0020 cm/cm
<br>@Time 86400 sec
0.00050 - 0.0020 in/in
<br>@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP THERMOCOMP DF00A8P PC (Asia Pacific)
LNP* Thermocomp* DF00A8P is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: High modulus, good flatness, good impact perform..
Linear Mold Shrinkage, Flow 0.00050 - 0.0015 cm/cm
<br>@Thickness 3.20 mm
0.00050 - 0.0015 in/in
<br>@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics LNP STAT-KON DX09303C PC (Asia Pacific)
LNP* Stat-Kon* DX09303C is carbon fiber filled polycarbonate composite with high modulus, good flow ability, and high level of cleanliness for the most demanding application. A unique feature of thi..
Linear Mold Shrinkage, Flow 0.00050 cm/cm
0.00050 in/in
Compression molding; ISO 2577
Hexion Bakelite™ PF 7595 Phenolic Formaldehyde Resin, Low Coefficient of Friction, Galvanized, Conductive &nbsp;(di
Phenolic molding compound, inorganically/organically filled, modified with graphite, good heat conductivity, good sliding properties, conductive in electrical properties.Application areas: Bearers f..
Linear Mold Shrinkage, Flow 0.00050 - 0.0015 cm/cm
0.00050 - 0.0015 in/in
Solvay Test
Solvay Specialty Polymers Ixef® 3006/9019 Polyarylamide, 30% Carbon Fiber, DAM &nbsp;(discontinued **)
The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A..
Linear Mold Shrinkage, Flow 0.00050 - 0.0020 cm/cm
0.00050 - 0.0020 in/in
ASTM D955
PolyOne Stat-Tech™ NJ-20CF/000 Black Polyamide 12 (Nylon 12)
Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound..
Linear Mold Shrinkage, Flow 0.00050 cm/cm
0.00050 in/in
Post-shrinkage, 60x60x2; 120°C; 4 hour; ISO 294-4
Lanxess Durethan® BKV 35 CX H2.0 900876 Nylon 6, Glass Fiber Reinforced
PA 6, 35% glass fibers, injection molding, heat-aging stabilizedInformation provided by LANXESS.
Copyright © lookpolymers.com All Rights Reserved