| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Linear Mold Shrinkage, Flow |
0.0010
-
0.0020
cm/cm <br>@Thickness 3.20 mm
|
0.0010
-
0.0020
in/in <br>@Thickness 0.126 in
|
SABIC Method |
|
SABIC Innovative Plastics Lexan® 3414R PC
40% GR, provides improved mechanical properties and UL94V-1 rated at 0.058"". Internal mold release added.
|
|||
| Linear Mold Shrinkage, Flow | 0.0010 - 0.0020 cm/cm | 0.0010 - 0.0020 in/in | ASTM D955 |
|
Ravago Manufacturing Americas Hylex® P1010G40 HB Polycarbonate, 40% Fiberglass Reinforced
Information provided by Ravago.
|
|||
| Linear Mold Shrinkage, Flow | 0.0010 cm/cm | 0.0010 in/in | Conditioned; ASTM D955 |
|
Solvay Specialty Polymers Amodel® A-1145 HS Polyphthalamide (PPA)
(Unverified Data**)
Amodel A-1145 HS is a 45% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, very high flexural modulus and very high tensile strength. Excellent creep ..
|
|||
| Linear Mold Shrinkage, Flow | 0.0010 - 0.0040 cm/cm | 0.0010 - 0.0040 in/in | ASTM D955 |
|
PolyOne Edgetek® ET3500-5001 colored Acrylonitrile Styrene Acrylate + PC (ASA+PC)
The Edgetek™ Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for ..
|
|||
| Linear Mold Shrinkage, Flow | 0.0010 - 0.0030 cm/cm | 0.0010 - 0.0030 in/in | on Tensile Bar; SABIC Method |
|
SABIC Innovative Plastics LNP LUBRICOMP BX05029 SAN (Europe-Africa-Middle East)
LNP* Lubricomp* BX05029 is a compound based on Styrene Acrylonitrile resin containing Mineral, Graphite.
|
|||
| Linear Mold Shrinkage, Flow | 0.0010 - 0.0030 cm/cm | 0.0010 - 0.0030 in/in | |
|
Idemitsu Kosan Xarec® WA 214 SPS, 40% Glass Filled |
|||
| Linear Mold Shrinkage, Flow | 0.0010 cm/cm | 0.0010 in/in | Post-shrinkage, 60x60x2; 120°C; 4 hour; ISO 294-4 |
|
Lanxess Pocan® T 7141 000000 PET + PBT, 40% Glass Fiber/Mineral
PET + PBT, 40% glass fibers/mineral, injection molding, improved flowability, high thermal dimensional stabilityInformation provided by LANXESS.
|
|||
| Linear Mold Shrinkage, Flow | 0.0010 - 0.0020 cm/cm | 0.0010 - 0.0020 in/in | |
|
LATI Larton L K/20 L-PPS, 20% Carbon Fiber Reinforced
Linear Polyphenylene Sulfide (L-PPS) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle..
|
|||
| Linear Mold Shrinkage, Flow |
0.0010
cm/cm <br>@Thickness 3.17 mm
|
0.0010
in/in <br>@Thickness 0.125 in
|
ASTM D955 |
|
Techmer ES HiFill® PA6 G/C50 A240 BK 50% Glass/Ceramic Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Ceramic, 50% Filler by WeightAppearance: BlackTPCI# 9809102Information provided by TP Composites, Inc.
|
|||
| Linear Mold Shrinkage, Flow |
0.0010
-
0.0030
cm/cm <br>@Thickness 3.20 mm
|
0.0010
-
0.0030
in/in <br>@Thickness 0.126 in
|
SABIC Method |
|
SABIC Innovative Plastics LNP THERMOCOMP DX10311 PC (Asia Pacific)
DX10311 is 30% glass fiber reinforced, impact modified polycarbonate resin. High flow and good ductility.
|
|||
| Linear Mold Shrinkage, Flow |
0.0010
-
0.0030
cm/cm <br>@Time 86400 sec
|
0.0010
-
0.0030
in/in <br>@Time 24.0 hour
|
ASTM D955 |
|
SABIC Innovative Plastics LNP THERMOCOMP OF006 PPS - Linear
LNP* THERMOCOMP* OF006 is a compound based on Linear PPS containing 30% Glass Fiber.
|
|||
| Linear Mold Shrinkage, Flow | 0.0010 - 0.0030 cm/cm | 0.0010 - 0.0030 in/in | on tensile bar; SABIC Method |
|
SABIC Innovative Plastics LNP Thermocomp RF007ESS PA 66 (Europe-Africa-Middle East)
LNP* Thermocomp* RF007ESS is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized.This data was supplied by SABIC-IP for..
|
|||
| Linear Mold Shrinkage, Flow | 0.0010 - 0.0030 cm/cm | 0.0010 - 0.0030 in/in | SABIC Method |
|
SABIC Innovative Plastics LNP STAT-KON DEL22P PC (Asia Pacific)
LNP STAT-KON* DEL22P is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive.
|
|||
| Linear Mold Shrinkage, Flow | 0.0010 - 0.0040 cm/cm | 0.0010 - 0.0040 in/in | on Tensile Bar; SABIC Method |
|
SABIC Innovative Plastics Valox® EXVX1403 PBT (Asia Pacific)
33% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin, Good thermal shock resistance and low CTE.
|
|||
| Linear Mold Shrinkage, Flow |
0.0010
-
0.0040
cm/cm <br>@Thickness 3.20 mm
|
0.0010
-
0.0040
in/in <br>@Thickness 0.126 in
|
SABIC Method |
|
SABIC Innovative Plastics Valox® IQNH4565 PBT (Asia Pacific)
Valox* iQNH4565 resin is a non-brominated/non-chlorinated flame retardant product based on an environmentally sustainable Valox iQ* PBT resin. Post-consumer recycle (PCR) usage is 29% based on EPEAT..
|
|||
| Linear Mold Shrinkage, Flow | 0.0010 - 0.0030 cm/cm | 0.0010 - 0.0030 in/in | on Tensile Bar; SABIC Method |
|
SABIC Innovative Plastics LNP THERMOCOMP PC006 PA 6 (Europe-Africa-Middle East)
LNP* Thermocomp* PC006 is a compound based on Nylon 6 resin containing Carbon Fiber.
|
|||
| Linear Mold Shrinkage, Flow |
0.0010
-
0.0040
cm/cm <br>@Time 86400 sec
|
0.0010
-
0.0040
in/in <br>@Time 24.0 hour
|
ASTM D955 |
|
SABIC Innovative Plastics LNP THERMOTUF VC006 Super Tough PA 6/6
LNP* THERMOTUF* VC006 is a compound based on Super Tough Nylon 6/6 resin containing Carbon Fiber. Added features of this material include: High Impact.
|
|||
| Linear Mold Shrinkage, Flow |
0.0010
-
0.0020
cm/cm <br>@Thickness 3.20 mm
|
0.0010
-
0.0020
in/in <br>@Thickness 0.126 in
|
SABIC Method |
|
SABIC Innovative Plastics NORYL EM7430 PPE+PS
30% glass reinforced, high flow PPO. Automotive. Energy management material.
|
|||
| Linear Mold Shrinkage, Flow |
0.0010
cm/cm <br>@Thickness 3.20 mm
|
0.0010
in/in <br>@Thickness 0.126 in
|
|
|
Unitika RUN35-C25 PA6, Dry
High modulus and low warpage nylonInformation provided by Unitika Ltd.
|
|||
| Linear Mold Shrinkage, Flow | 0.0010 cm/cm | 0.0010 in/in | ASTM D955 |
|
Unitika E-RUNG60 Ultra high-rigidity PA6, Dry
Ultra high-rigidityInformation provided by Unitika Ltd.
|
|||
| Linear Mold Shrinkage, Flow | 0.0010 cm/cm | 0.0010 in/in | ISO 294-4, 2577 |
|
EMS-Grivory Grivory® BG-15 S PA6-GF15
Product description: Grilon BG-15 S is a heat stabilized PA6 injection molding grade with 15% glass fibers. Grilon BG-15 S has the following important properties: Excellent surface finishEasy flowin..
|
|||
| Linear Mold Shrinkage, Flow | 0.0010 cm/cm | 0.0010 in/in | ISO 294-4, 2577 |
|
EMS-Grivory Grivory® TSG-30 PA666-GF30
Product description: Grilon TSG-30 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 30% glass fibers. Grilon TSG-30 has the following important properties: Excellent fl..
|
|||
| Linear Mold Shrinkage, Flow | 0.0010 cm/cm | 0.0010 in/in | ISO 294-4, 2577 |
|
EMS-Grivory Grivory® TSGK-30 X PA666-(GF+GB)30
Product description: Grilon TSGK-30 X is a heat stabilized PA66 + PA6 injection molding grade with a 30% reinforcement combination (glass fibers and glass beads). Grilon TSGK-30 X has the following ..
|
|||
| Linear Mold Shrinkage, Flow | 0.0010 cm/cm | 0.0010 in/in | ISO 294-4, 2577 |
|
EMS-Grivory Grivory® TSGZ-15 PA666-GF15
Product description: Grilon TSGZ-15 is a heat stabilized, normal viscosity, and impact modified PA66 + PA6 injection molding grade with 15% glass fibers. Grilon TSGZ-15 has the following important p..
|
|||
| Linear Mold Shrinkage, Flow | 0.0010 cm/cm | 0.0010 in/in | ISO 294-4, 2577 |
|
EMS-Grivory Grivory® XE 4102 black 9238 PA*-CF30
Grivory XE 4102 is a 30% carbon fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. This Grivory HT product is partially based on renewab..
|
|||
| Linear Mold Shrinkage, Flow | 0.0010 cm/cm | 0.0010 in/in | ISO 294-4 2577 |
|
DuPont Performance Polymers Rynite® FR531 NC010 Polyethylene Terephthalate (PET)
(Unverified Data**)
36% Reinforced Flame Retardant Polyethylene Terephthalate Information provided by DuPont Performance Polymers
|
|||
| Linear Mold Shrinkage, Flow | 0.0010 - 0.0020 cm/cm | 0.0010 - 0.0020 in/in | on Tensile Bar; E2P method |
|
Eurostar Staramide ACF3 PA66, 15% Carbon Fiber Reinforced, Heat stabilized, Injection Molding
Staramide ACF3 is a 15% Carbon Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar.
|
|||
| Linear Mold Shrinkage, Flow |
0.0010
-
0.0030
cm/cm <br>@Thickness 4.00 mm
|
0.0010
-
0.0030
in/in <br>@Thickness 0.157 in
|
E2P method |
|
Eurostar Star L PA66 30V D51 PA66, Glass Fiber Filled, Injection Molded
Star L PA66 30V D51 is a PTFE lubricated, Glass Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Eurostar.
|
|||
| Linear Mold Shrinkage, Flow |
0.0010
-
0.0030
cm/cm <br>@Time 86400 sec
|
0.0010
-
0.0030
in/in <br>@Time 24.0 hour
|
ASTM D955 |
|
SABIC Innovative Plastics LNP VERTON PX06418 PA 6
LNP* VERTON* PX06418 is a compound based on Nylon 6 containing proprietary fillers. Added features of this grade are: Heat Stabilized, Structural.
|
|||