Polymer Property : Linear Mold Shrinkage, Flow = 0.0060 in/in Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.0060 - 0.0080 cm/cm
<br>@Thickness 3.20 mm
0.0060 - 0.0080 in/in
<br>@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics Lexan® 4401R PPC+PC (Asia Pacific)
LEXAN 4401R is a high heat resistant poly(ester)carbonate injection molding resin.This data was supplied by SABIC-IP for the Asia Pacific region.
Linear Mold Shrinkage, Flow 0.0060 - 0.0080 cm/cm
0.0060 - 0.0080 in/in
on Tensile Bar; SABIC Method
SABIC Innovative Plastics Lexan® ML3400 PC (Europe-Africa-Middle East)
LEXAN ML3400 is a medium viscosity, impact modified grade with improved chemical resistance. It passes the British Standard 2495 and 5361 solvent tests.
Linear Mold Shrinkage, Flow 0.0060 - 0.0080 cm/cm
<br>@Thickness 3.20 mm
0.0060 - 0.0080 in/in
<br>@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics Lexan® OQ3820 PC
High Viscosity, UV-stabilized grade for ophthalmic lenses.
Linear Mold Shrinkage, Flow 0.0060 - 0.0090 cm/cm
<br>@Thickness 3.20 mm
0.0060 - 0.0090 in/in
<br>@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics Lexan® XHT2146 PC Copolymer (Europe-Africa-Middle East)
XHT2146 resin is a high flow, high heat polycarbonate copolymer with improved release performance compared to Lexan* XHT2141 resin. It is available in a range of opaque and limited transparent colo..
Linear Mold Shrinkage, Flow 0.0060 - 0.0090 cm/cm
<br>@Thickness 3.20 mm
0.0060 - 0.0090 in/in
<br>@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics Lexan® XHT3141 PC Copolymer
XHT3141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors.
Linear Mold Shrinkage, Flow 0.0060 - 0.0080 cm/cm
0.0060 - 0.0080 in/in
ASTM D955
PolyOne Edgetek® XT XT-100-BW01 Natural PC+PBT &nbsp;(discontinued **)
EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of gen..
Linear Mold Shrinkage, Flow 0.0060 - 0.0080 cm/cm
<br>@Thickness 3.20 mm
0.0060 - 0.0080 in/in
<br>@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics Lexan® 925AU PC
Lexan* 925AU Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is UV stabilized, providing addit..
Linear Mold Shrinkage, Flow 0.0060 - 0.0080 cm/cm
<br>@Thickness 3.20 mm
0.0060 - 0.0080 in/in
<br>@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics Lexan® 955 PC
Lexan* 955 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is available in various opaque color..
Linear Mold Shrinkage, Flow 0.0060 - 0.0080 cm/cm
<br>@Thickness 3.20 mm
0.0060 - 0.0080 in/in
<br>@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics Lexan® 955 PC (Asia Pacific)
Lexan* 955 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is available in various opaque color..
Linear Mold Shrinkage, Flow 0.0060 - 0.0080 cm/cm
<br>@Thickness 3.20 mm
0.0060 - 0.0080 in/in
<br>@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics Lexan® DMX1132 PC Copolymer (Europe-Africa-Middle East)
Lexan* DMX1132 is a high flow polycarbonate copolymer resin with improved ammonia resistance over regular polycarbonate resin.This data was supplied by SABIC-IP for the Europe-Africa-Middle East reg..
Linear Mold Shrinkage, Flow 0.0060 - 0.0080 cm/cm
<br>@Thickness 3.20 mm
0.0060 - 0.0080 in/in
<br>@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics Lexan® FXD9810U PC Copolymer (Asia Pacific)
Polycarbonate with high flow, excellent processability, good impact and thermal properties, UV stabilized, non-Chlorine and non-Bromine flame retardant, UL rated V-0 and V-1. Available in limited di..
Linear Mold Shrinkage, Flow 0.0060 cm/cm
0.0060 in/in
ISO 294-4
Mitsubishi Xantar® 22 SR FD Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
Linear Mold Shrinkage, Flow 0.0060 cm/cm
0.0060 in/in
ISO 294-4
Mitsubishi Xantar® 27 U Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
Linear Mold Shrinkage, Flow 0.0060 cm/cm
<br>@Thickness 3.17 mm
0.0060 in/in
<br>@Thickness 0.125 in
1/8&quot; Section
Lucent Polymers PC-1418FD Polycarbonate, FDA Compliant, Injection Grade
High FlowAdd "R" for Added ReleaseAdd "U" for UV StabilizedInformation provided by Lucent Polymers, Inc.
Linear Mold Shrinkage, Flow 0.0060 cm/cm
0.0060 in/in
ISO 294-4
Mitsubishi Xantar® MX 2015 Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
Linear Mold Shrinkage, Flow 0.0060 cm/cm
0.0060 in/in
Solvay TECHNYL® A 218 V25 Black 21 N PA66, 25% glass fiber, DRY
Description: TECHNYL® A 218 V25 is a polyamide 66, reinforced with 25% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The ..
Linear Mold Shrinkage, Flow 0.0060 - 0.0090 cm/cm
0.0060 - 0.0090 in/in
on Tensile Bar; SABIC Method
SABIC Innovative Plastics Valox® 4012G PBT
VALOX 4012G is a 10% glass fiber reinforced PBT injection molding resin with excellent mechanical properties. Applications: connectors. This grade is a 4012 with improved cycle time and ductility.
Linear Mold Shrinkage, Flow 0.0060 cm/cm
0.0060 in/in
Solvay Specialty Polymers Veradel® 3250 Polyethersulfone (PESU)
Veradel® 3250 polyethersulfone (PESU) has a slightly higher melt flow rate than Veradel® 3200. This transparent resin offers a high heat deflection temperature, excellent toughness and dimensi..
Linear Mold Shrinkage, Flow 0.0060 cm/cm
<br>@Thickness 3.17 mm
0.0060 in/in
<br>@Thickness 0.125 in
ASTM D955
Techmer ES HiFill® HDPE GF10 CC 10% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by WeightFeatures: Chemically CoupledInformation provided by TP Composites, Inc.
Linear Mold Shrinkage, Flow 0.0060 cm/cm
<br>@Thickness 3.17 mm
0.0060 in/in
<br>@Thickness 0.125 in
ASTM D955
Techmer ES HiFill® PA6/6 GF/M35 HS BK 35% Glass/Mineral Fiber Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 35% Filler by Weight and Mineral Filler, 35% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures..
Linear Mold Shrinkage, Flow 0.0060 cm/cm
<br>@Thickness 3.17 mm
0.0060 in/in
<br>@Thickness 0.125 in
ASTM D955
Techmer ES HiFill® PA6/6 GF40 HS L BK 40% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedUL File N..
Linear Mold Shrinkage, Flow 0.0060 cm/cm
<br>@Time 86400 sec
0.0060 in/in
<br>@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP THERMOCOMP WF006H PBT
LNP* THERMOCOMP* WF006H is a compound based on PBT resin containing 30% Glass Fiber. Added feature of this grade is: Healthcare.
Linear Mold Shrinkage, Flow 0.0060 - 0.0070 cm/cm
<br>@Thickness 3.20 mm
0.0060 - 0.0070 in/in
<br>@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics NORYL PPX PPX7112 PPE+PP
PPE+PP blend. Suitable for painted exterior automotive applications.
Linear Mold Shrinkage, Flow 0.0060 cm/cm
<br>@Thickness 3.17 mm
0.0060 in/in
<br>@Thickness 0.125 in
ASTM D955
Techmer ES Electrablend® ABS SS10 FR BK 10% Stainless Steel Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel Fiber, 10% Filler by WeightFeatures: Flame Retardant and Electromagnetic Shielding (EMI)Appearance: BlackInformation pr..
Linear Mold Shrinkage, Flow 0.0060 cm/cm
<br>@Thickness 3.17 mm
0.0060 in/in
<br>@Thickness 0.125 in
ASTM D955
Techmer ES HiFill® PA4/6 GF30 HS NAT 30% Glass Filled (Conditioned)
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedAppearance: Natural ColorInformation p..
Linear Mold Shrinkage, Flow 0.0060 - 0.0080 cm/cm
<br>@Time 86400 sec
0.0060 - 0.0080 in/in
<br>@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP THERMOCOMP TF002 PU
LNP* THERMOCOMP* TF002 is a compound based on Polyurethane resin containing 10% Glass Fiber.
Linear Mold Shrinkage, Flow 0.0060 cm/cm
0.0060 in/in
DAM; ISO 294-4 2577
DuPont Performance Polymers Zytel® 7335F NC010 Nylon 6 &nbsp;(Unverified Data**)
Unreinforced Polyamide 6 Zytel 7335F NC010 is a nucleated lubricated polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers
Linear Mold Shrinkage, Flow 0.0060 cm/cm
0.0060 in/in
ISO 294-4,2577
Covestro Makrolon® DP1-1887* Polycarbonate, 10% Glass Filled
ISO 7391-PC,MR,(,,)-18-9,GF10Developmental productMVR (300 °C/1.2 kg) 16 cm3/10 min10 % Glass fiber reinforcedMilled fiberLow viscosityEasy releasegood surface qualityInjection molding - Melt tempe..
Linear Mold Shrinkage, Flow 0.0060 cm/cm
0.0060 in/in
DAM; ISO 294-4 2577
DuPont Performance Polymers Minlon® IG38C1 BK434 Nylon 66 &nbsp;(Unverified Data**)
38% Mineral/Glass Reinforced Polyamide 66 Minlon IG38C1 BK434 is a 38% mineral/glass reinforced heat stabilized black polyamide 66 resin for injection molding.Information provided by DuPont Performa..