| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Linear Mold Shrinkage, Flow | 0.0070 - 0.011 cm/cm | 0.0070 - 0.011 in/in | ASTM D955 |
|
PolyOne Versaflex™ CL2242 Thermoplastic Elastomer (TPE)
Versaflex™ CL2242 is an easy processing compound designed for use in injection molding applications where FDA compliance, clarity and enhanced heat resistance are required. - Excellent Clarity - Ov..
|
|||
| Linear Mold Shrinkage, Flow |
0.0070
cm/cm <br>@Thickness 3.18 mm
|
0.0070
in/in <br>@Thickness 0.125 in
|
ASTM D955 |
|
Solvay Specialty Polymers Udel® P-3700 HC Polysulfone (PSU)
(Unverified Data**)
Udel P-3700 HC is a high-clarity grade of polysulfone (PSU) that is nearly water-white in color. This grade was designed to eliminate the yellow cast and provide design flexibility and improved aest..
|
|||
| Linear Mold Shrinkage, Flow |
0.0070
-
0.012
cm/cm <br>@Thickness 3.20 mm
|
0.0070
-
0.012
in/in <br>@Thickness 0.126 in
|
ASTM D955 |
|
LG Chemical LUMID GP2130B(W) PA66+GF13%, General Purpose
Feature: Injection Molding, PA66+GF13%, General PurposeApplication: Valve CoversCAS No. 32131-17-2, 65997-17-3 and 9010-79-9Information provided by LG Chemical
|
|||
| Linear Mold Shrinkage, Flow |
0.0070
-
0.010
cm/cm <br>@Thickness 3.20 mm
|
0.0070
-
0.010
in/in <br>@Thickness 0.126 in
|
ASTM D955 |
|
LG Chemical Lupox® TE5011M PBT+PC
Description: Injection Molding, PBT+PC, High Impact, Dimensional Stability, Good WeatherabilityApplication: Automotive (Bumper Back Beam)CAS No. 24968-12-5 and 103598-77-2Information provided by LG ..
|
|||
| Linear Mold Shrinkage, Flow |
0.0070
cm/cm <br>@Thickness 2.00 mm
|
0.0070
in/in <br>@Thickness 0.0787 in
|
Mold Temp 80°C; Melt Temp 280°C; 600 bar; ISO 294-4 |
|
Lanxess Durethan® AKV 15 H3.0 000000 Nylon 66, 15% Glass Fibers
PA 66, 15% glass fibers, injection molding, heat-ageing stabilized
|
|||
| Linear Mold Shrinkage, Flow |
0.0070
-
0.0080
cm/cm <br>@Thickness 3.20 mm
|
0.0070
-
0.0080
in/in <br>@Thickness 0.126 in
|
ASTM D955 |
|
LG Chemical LUPOL HM5302W PP+MF30%, High Impact
Description: Injection Molding, PP+MF30%, High Impact, Good WeatherabilityApplication: Automotive Interior PartsCAS: 9003-07-0, 26221-73-8 and 14807-96-6Information provided by LG Chemical
|
|||
| Linear Mold Shrinkage, Flow |
0.0070
-
0.0080
cm/cm <br>@Thickness 3.20 mm
|
0.0070
-
0.0080
in/in <br>@Thickness 0.126 in
|
ASTM D955 |
|
LG Chemical Lupox® TE5000GH PBT+PC
Description: Injection Molding, PBT+PC, High Impact, Dimensional StabilityApplication: Automotive (Door Garnish)CAS No. 24968-12-5 and 103598-77-2Information provided by LG Chemical
|
|||
| Linear Mold Shrinkage, Flow |
0.0070
-
0.0090
cm/cm <br>@Thickness 3.20 mm
|
0.0070
-
0.0090
in/in <br>@Thickness 0.126 in
|
SABIC Method |
|
SABIC Innovative Plastics ULTEM 2110EPR PEI (Asia Pacific)
10% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 and 5VA listing.
|
|||
| Linear Mold Shrinkage, Flow | 0.0070 cm/cm | 0.0070 in/in | |
|
Solvay Specialty Polymers Radel® R-5100 Polyphenylsulfone (PPSU), Filled
Radel® R-5100 is an opaque, general purpose polyphenylsulfone (PPSU) for injection molding, that offers exceptional hydrolytic stability, and toughness superior to other commercially-available, h..
|
|||
| Linear Mold Shrinkage, Flow |
0.0070
cm/cm <br>@Thickness 3.18 mm
|
0.0070
in/in <br>@Thickness 0.125 in
|
|
|
Solvay Specialty Polymers Radel® R-5600 Polyphenylsulfone (PPSU)
Radel® R-5600 is a very high melt flow grade of Radel® polyphenylsulfone (PPSU). It is especially well-suited for parts requiring long flow length with thin walls. Radel® resins offer excep..
|
|||
| Linear Mold Shrinkage, Flow |
0.0070
-
0.011
cm/cm <br>@Thickness 3.20 mm
|
0.0070
-
0.011
in/in <br>@Thickness 0.126 in
|
SABIC Method |
|
SABIC Innovative Plastics Xenoy® HX5600HP PBT+PC (Europe-Africa-Middle East)
Xenoy HX5600HP is PBT based semi-crystalline blend with balanced flow and impact properties. Improved chemical resistance against lab disinfectants and chemicals for healthcare enclosure and housing..
|
|||
| Linear Mold Shrinkage, Flow |
0.0070
-
0.0090
cm/cm <br>@Thickness 3.20 mm
|
0.0070
-
0.0090
in/in <br>@Thickness 0.126 in
|
SABIC Method |
|
SABIC Innovative Plastics Xenoy® X4850 PBT+PC
Xenoy X4850 is a hydrostable, high modulus, high ductile PC/PBT blend. Furthermore, this resin provides high chemicalresistance, very low creep, low CTE, excellent fatique and high heat dimensional ..
|
|||
| Linear Mold Shrinkage, Flow |
0.0070
cm/cm <br>@Thickness 3.17 mm
|
0.0070
in/in <br>@Thickness 0.125 in
|
ASTM D955 |
|
Techmer ES Plastiblend® PC/ABS 830 SS7 BK
Availability: North AmericaForms: PelletsInformation provided by TP Composites, Inc.
|
|||
| Linear Mold Shrinkage, Flow |
0.0070
cm/cm <br>@Thickness 3.17 mm
|
0.0070
in/in <br>@Thickness 0.125 in
|
ASTM D955 |
|
Techmer ES Plastiblend® PC/ABS 8800
Availability: North AmericaForms: PelletsFeatures: High Impact Resistance and High Temperature StrengthProcessing Method: Profile ExtrusionInformation provided by TP Composites, Inc.
|
|||
| Linear Mold Shrinkage, Flow |
0.0070
-
0.011
cm/cm <br>@Thickness 3.20 mm
|
0.0070
-
0.011
in/in <br>@Thickness 0.126 in
|
ASTM D955 |
|
Samsung Cheil Industries Infino® VB-3100G PBT/ABS, Glass Filled FR
Information provided by Samsung Cheil Industries.
|
|||
| Linear Mold Shrinkage, Flow | 0.0070 cm/cm | 0.0070 in/in | |
|
Solvay TECHNYL® A 216 V20 PA66, 20% glass fiber, DRY
Description: Polyamide 66, reinforced with 20% of glass fiber, for injection molding.Available in: Europe Product Applications: TECHNYL® A 216 V20 is used in all sectors of industry, offering and..
|
|||
| Linear Mold Shrinkage, Flow |
0.0070
-
0.0090
cm/cm <br>@Thickness 3.20 mm
|
0.0070
-
0.0090
in/in <br>@Thickness 0.126 in
|
SABIC Method |
|
SABIC Innovative Plastics Noryl GTX CRN500 PPE+PA6 (Asia Pacific)
Pa6 based unfilled GTX for Non-Auto marketThis data was supplied by SABIC-IP for the Asia Pacific region.
|
|||
| Linear Mold Shrinkage, Flow |
0.0070
-
0.0090
cm/cm <br>@Thickness 3.20 mm
|
0.0070
-
0.0090
in/in <br>@Thickness 0.126 in
|
SABIC Method |
|
SABIC Innovative Plastics Xenoy® X5300WX PBT+PC (Asia Pacific)
Unreinforced, opaque PBT+PC alloy. Chemical resistance and good mechanical performance. UV-stabilized. Excellent weatherability.
|
|||
| Linear Mold Shrinkage, Flow | 0.0070 - 0.011 cm/cm | 0.0070 - 0.011 in/in | on tensile bar; SABIC Method |
|
SABIC Innovative Plastics Xenoy® XD1575S PBT+PC (Europe-Africa-Middle East)
XENOY XD1575S is a high flow PC+PBT blend with good impact properties and good resistance to occasional solvent and gasoline contact. XENOY XD1575S has been specially developed for coated exterior b..
|
|||
| Linear Mold Shrinkage, Flow |
0.0070
-
0.0090
cm/cm <br>@Thickness 3.20 mm
|
0.0070
-
0.0090
in/in <br>@Thickness 0.126 in
|
SABIC Method |
|
SABIC Innovative Plastics NORYL GTX GTX600 PPE+PA6 (Asia Pacific)
Pa6 based unfilled GTX
|
|||
| Linear Mold Shrinkage, Flow | 0.0070 - 0.011 cm/cm | 0.0070 - 0.011 in/in | DIS 294-4 |
|
Wellman Wellamid® GFX1717-BK1 Nylon 66, 43% Glass Fiber Reinforced, Silicone Lubricated
All information provided by Wellman Engineered Resins.
|
|||
| Linear Mold Shrinkage, Flow | 0.0070 cm/cm | 0.0070 in/in | ISO 294-4,2577 |
|
Covestro Makrolon® 2856 Polycarbonate
ISO 7391-PC,MR,(,,)-09-9Global gradeMVR (300 °C/1.2 kg) 9.5 cm3/10 minFood contact qualityMedium viscosityEasy releaseGood hydrolysis resistanceInjection molding - Melt temperature 280 - 320 °CAva..
|
|||
| Linear Mold Shrinkage, Flow | 0.0070 cm/cm | 0.0070 in/in | ISO 294-4,2577 |
|
Covestro Makrolon® 3206 Polycarbonate
ISO 7391-PC,M,(,,)-05-9MVR (300 °C/1.2 kg) 4.0 cm3/10 minFood contact qualityHigh viscosityGood hydrolysis resistanceInjection molding - Melt temperature 280 - 320 °CExtrusionAvailable in transpar..
|
|||
| Linear Mold Shrinkage, Flow | 0.0070 cm/cm | 0.0070 in/in | ISO 294-4,2577 |
|
Covestro Makrolon® 6585 Polycarbonate, Flame Retardant Grade
ISO 7391-PC,MFR,(,,)-09-9Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 minFlame retardantUL 94V-0/1.2 mm5VA/3.0 mm and 5VB (WT) /2.0 mmHigh viscosityEasy releaseInjection molding - Melt temperature 28..
|
|||
| Linear Mold Shrinkage, Flow | 0.0070 cm/cm | 0.0070 in/in | DAM; ISO 294-4 |
|
DSM Stanyl® 46HF5041LW Nylon 46-40% Glass Reinforced (European and Asian Grade) (Cond)
Stanyl is a high performance polyamide providing unmatched performance and value across an amazingly broad range of automotive and electronic applications. Stanyl offers:Highest mechanical propertie..
|
|||
| Linear Mold Shrinkage, Flow |
0.0070
-
0.010
cm/cm <br>@Thickness 4.00 mm
|
0.0070
-
0.010
in/in <br>@Thickness 0.157 in
|
E2P method |
|
Eurostar Staramide 6 80E7 PA6, Injection Molded
Staramide 6 80E7 is a high density, Polyamide 6, Injection Molding Resin (also known as 680E7)Information provided by Eurostar.
|
|||
| Linear Mold Shrinkage, Flow | 0.0070 cm/cm | 0.0070 in/in | ISO 294-4,2577 |
|
Covestro Makrolon® SF800Z Polycarbonate, 5% Glass Filled
MVR (300 °C/1.2 kg) 8.0 cm3/10 minStructural foam5 % Glass fiber reinforcedMilled fiberChlorine- and bromine-free flame retardantMedium viscosityEasy releaseInjection moldingAvailable in natural (o..
|
|||
| Linear Mold Shrinkage, Flow | 0.0070 cm/cm | 0.0070 in/in | ISO 294-4, 2577 |
|
EMS-Grivory Grivory® TS V0 X PA666 FR
Product description: Grilon XE 5030 is a heat stabilized, flame retardant and self-extinguishing injection molding grade on the basis of PA6-PA66-alloy. Grilon XE 5030 features the following main pr..
|
|||
| Linear Mold Shrinkage, Flow |
0.0070
-
0.0080
cm/cm <br>@Thickness 3.20 mm
|
0.0070
-
0.0080
in/in <br>@Thickness 0.126 in
|
SABIC Method |
|
SABIC Innovative Plastics XYLEX X7519HP PC+POLYESTER (Europe-Africa-Middle East)
Good Chemical Resistance, XYLEX grade with good dishwasher performance, USA/Europe Food Contact Comment: While molding of thicker parts, cooling speed has an influence of transparency. Thicker parts..
|
|||
| Linear Mold Shrinkage, Flow | 0.0070 cm/cm | 0.0070 in/in | ISO 2577 |
|
BASF Ultradur® B 4300 G3 High Speed 15% Glass Filled BK 15045 PBT
Description: Easy flowing injection molding grade with 15 % glass fibers; for rigid, tough and dimensionally stable technical parts (eg timer dials, toggles, knobs, parts for thermostats, oven-door ..
|
|||