| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Linear Mold Shrinkage, Flow |
0.0050
-
0.0080
cm/cm <br>@Thickness 3.20 mm
|
0.0050
-
0.0080
in/in <br>@Thickness 0.126 in
|
SABIC Method |
|
SABIC Innovative Plastics Cycolac® MG34LG ABS
Automotive: Low gloss ABS for unpainted interior applications.
|
|||
| Linear Mold Shrinkage, Flow |
0.0050
-
0.0080
cm/cm <br>@Thickness 3.20 mm
|
0.0050
-
0.0080
in/in <br>@Thickness 0.126 in
|
SABIC Method |
|
SABIC Innovative Plastics Lexan® DMX1435 PC Copolymer (Europe-Africa-Middle East)
This product will be phased out per January 2015 -- Lexan* DMX1435 is a UV stabilized standard flow polycarbonate copolymer resin with improved scratch resistance.
|
|||
| Linear Mold Shrinkage, Flow | 0.0040 - 0.0080 cm/cm | 0.0040 - 0.0080 in/in | on Tensile Bar; SABIC Method |
|
SABIC Innovative Plastics Lexan® EXL1444 PC Copolymer (Asia Pacific)
Lexan* EXL1444 polycarbonate (PC) siloxane copolymer resin is a medium flow opaque injection molding (IM) grade suitable for FDA compliant applications. This resin offers extreme low temperature (-..
|
|||
| Linear Mold Shrinkage, Flow |
0.0040
-
0.0080
cm/cm <br>@Thickness 3.20 mm
|
0.0040
-
0.0080
in/in <br>@Thickness 0.126 in
|
SABIC Method |
|
SABIC Innovative Plastics Lexan® EXL1464T PC Copolymer (Europe-Africa-Middle East)
Lexan* EXL1464T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers extreme low temperature (-40 °C) ductility in combination with medium flo..
|
|||
| Linear Mold Shrinkage, Flow |
0.0040
-
0.0080
cm/cm <br>@Thickness 3.20 mm
|
0.0040
-
0.0080
in/in <br>@Thickness 0.126 in
|
SABIC Method |
|
SABIC Innovative Plastics Lexan® HPX8REU PC Copolymer (Europe-Africa-Middle East)
Very high flow specialty polycarbonate with outstanding processability and ductility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 o..
|
|||
| Linear Mold Shrinkage, Flow |
0.0060
-
0.0080
cm/cm <br>@Thickness 3.20 mm
|
0.0060
-
0.0080
in/in <br>@Thickness 0.126 in
|
SABIC Method |
|
SABIC Innovative Plastics Lexan® LUX9616 PC (Asia Pacific)
Lexan LUX9616 is a flame retardant polycarbonate featuring non brominated and non chlorinated FR system with diffusion effective and thin wall FR performance. It intended to meet WEEE/RoHS requireme..
|
|||
| Linear Mold Shrinkage, Flow |
0.0060
-
0.0080
cm/cm <br>@Thickness 3.20 mm
|
0.0060
-
0.0080
in/in <br>@Thickness 0.126 in
|
SABIC Method |
|
SABIC Innovative Plastics Lexan® OQ3820 PC
High Viscosity, UV-stabilized grade for ophthalmic lenses.
|
|||
| Linear Mold Shrinkage, Flow | 0.0070 - 0.0080 cm/cm | 0.0070 - 0.0080 in/in | ISO 294-4 |
|
Polyplastic Armlen® PP GF MF 30-1 Polypropylene, 30% Glass and Mineral Filled
Injection moldingInformation provided by PolyPlastic Group.
|
|||
| Linear Mold Shrinkage, Flow |
0.0040
-
0.0080
cm/cm <br>@Thickness 3.20 mm
|
0.0040
-
0.0080
in/in <br>@Thickness 0.126 in
|
SABIC Method |
|
SABIC Innovative Plastics Lexan® 143X PC Copolymer (Asia Pacific)
Improved flow PC with excellent processability and mold release.
|
|||
| Linear Mold Shrinkage, Flow |
0.0040
-
0.0080
cm/cm <br>@Thickness 3.20 mm
|
0.0040
-
0.0080
in/in <br>@Thickness 0.126 in
|
SABIC Method |
|
SABIC Innovative Plastics Lexan® EXL9134 PC Copolymer (Asia Pacific)
Lexan* EXL9134 polycarbonate (PC) siloxane copolymer resin is a UV stabilized high flow opaque injection molding (IM) grade. This resin offers UL94 V0 @ 1.5mm flame retardancy based on non-bromine, ..
|
|||
| Linear Mold Shrinkage, Flow |
0.0020
-
0.0080
cm/cm <br>@Thickness 3.20 mm
|
0.0020
-
0.0080
in/in <br>@Thickness 0.126 in
|
ASTM D955 |
|
LG Chemical LUCON SP9306FL sPS+MF
Description Injection Molding Grade, sPS+MF, Low Thermal Conductivity, Chemical Resistance, High Heat ResistanceApplication: Electrical or Electronic Parts CAS No. 9003-53-6, 65997-17-3, 68928-70-1 ..
|
|||
| Linear Mold Shrinkage, Flow |
0.0050
-
0.0080
cm/cm <br>@Thickness 3.20 mm
|
0.0050
-
0.0080
in/in <br>@Thickness 0.126 in
|
ASTM D955 |
|
LG Chemical LUPOY GN1002FH PC, Halogen Free, Flame Retardant, Heat Resistant
Description: Injection Molding, PC, Halogen Free Flame Retardant, Heat Resistant, Chemical Resistance, High ImpactApplication: IT/OA Housing and Components (Adaptor)CAS: 103598-77-2, 25232-40-0 and ..
|
|||
| Linear Mold Shrinkage, Flow |
0.0050
-
0.0080
cm/cm <br>@Thickness 3.20 mm
|
0.0050
-
0.0080
in/in <br>@Thickness 0.126 in
|
ASTM D955 |
|
LG Chemical LUPOY GN1004FA PC, Halogen Free, Flame Retardant, Chemical Resistance
Description: Injection Molding, PC, Halogen Free Flame Retardant, Chemical Resistance, High Impact at Low TemperatureApplication: IT/OA Housing and ComponentsCAS: 103598-77-2 and 143106-82-5Informat..
|
|||
| Linear Mold Shrinkage, Flow |
0.0060
-
0.0080
cm/cm <br>@Thickness 6.40 mm
|
0.0060
-
0.0080
in/in <br>@Thickness 0.252 in
|
SABIC Method |
|
SABIC Innovative Plastics Prevex BJAX PPE+PS
Foamable resin. All properties at 10% density reduction; 0.250" thick specimens; improved productivity.This data was supplied by SABIC-IP for the Americas region.
|
|||
| Linear Mold Shrinkage, Flow | 0.0040 - 0.0080 cm/cm | 0.0040 - 0.0080 in/in | on Tensile Bar; SABIC Method |
|
SABIC Innovative Plastics Valox® 815 PBT (Europe-Africa-Middle East)
VALOX 815 is a 15% glass reinforced PBT+PET blend with excellent surface finish. Applications: hot air gun housings assemblies, industrial glue guns, appliance housings and handles.
|
|||
| Linear Mold Shrinkage, Flow | 0.0050 - 0.0080 cm/cm | 0.0050 - 0.0080 in/in | on Tensile Bar; SABIC Method |
|
SABIC Innovative Plastics Valox® DR48 PBT (Europe-Africa-Middle East)
VALOX DR48 is a 17% glass reinforced, flame retardant injection moulding PBT resin. Applications: lamp sockets, connectors, switches, electrical housings and bases, bobbins, trimmers and electromoto..
|
|||
| Linear Mold Shrinkage, Flow |
0.0050
-
0.0080
cm/cm <br>@Thickness 3.20 mm
|
0.0050
-
0.0080
in/in <br>@Thickness 0.126 in
|
SABIC Method |
|
SABIC Innovative Plastics Xenoy® X2500UV PC+PET (Europe-Africa-Middle East)
XENOY X2500UV is a medium viscosity, unfilled, elastomer modified PC/PET blend with excellent heat and impact performance. ISO1043-label: PC+PET-I.
|
|||
| Linear Mold Shrinkage, Flow |
0.0050
-
0.0080
cm/cm <br>@Thickness 3.20 mm
|
0.0050
-
0.0080
in/in <br>@Thickness 0.126 in
|
SABIC Method |
|
SABIC Innovative Plastics XYLEX HX8300HP PC+POLYESTER
Medium flow, Transparent PC/Polyester alloy. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contact compliant...
|
|||
| Linear Mold Shrinkage, Flow |
0.0050
-
0.0080
cm/cm <br>@Thickness 3.20 mm
|
0.0050
-
0.0080
in/in <br>@Thickness 0.126 in
|
SABIC Method |
|
SABIC Innovative Plastics XYLEX X8300 PC+POLYESTER (Asia Pacific)
PC+Polyester, UV Stabilized, Transparent
|
|||
| Linear Mold Shrinkage, Flow |
0.0050
-
0.0080
cm/cm <br>@Thickness 3.20 mm
|
0.0050
-
0.0080
in/in <br>@Thickness 0.126 in
|
SABIC Method |
|
SABIC Innovative Plastics XYLEX X8409AC PC+POLYESTER (Asia Pacific)
PC + Polyester, Injection (Blow) Molding, or Extrusion Blow molding grade, Chemical Resistance and Transparency
|
|||
| Linear Mold Shrinkage, Flow |
0.0050
-
0.0080
cm/cm <br>@Thickness 3.20 mm
|
0.0050
-
0.0080
in/in <br>@Thickness 0.126 in
|
SABIC Method |
|
SABIC Innovative Plastics XYLEX X8409AC PC+POLYESTER (Europe-Africa-Middle East)
PC + Polyester, Injection (Blow) Molding, or Extrusion Blow molding grade, Chemical Resistance and Transparency
|
|||
| Linear Mold Shrinkage, Flow |
0.0060
-
0.0080
cm/cm <br>@Thickness 3.20 mm
|
0.0060
-
0.0080
in/in <br>@Thickness 0.126 in
|
SABIC Method |
|
SABIC Innovative Plastics NORYL NH5120C PPE+PS (Europe-Africa-Middle East)
Noryl* NH5120C resin is a modified PPE-PS blend that exhibits an excellent balance of nonhalogenated flame retardance, good chemical resistance, and low specifc gravity for light weight parts. The ..
|
|||
| Linear Mold Shrinkage, Flow |
0.0050
-
0.0080
cm/cm <br>@Thickness 3.20 mm
|
0.0050
-
0.0080
in/in <br>@Thickness 0.126 in
|
SABIC Method |
|
SABIC Innovative Plastics NORYL NH6010B PPE+HIPS
Noryl* NH6010B resin is a high performance, modified PPE-PS blend that exhibits an excellent balance of lower smoke production upon burning, nonhalogenated flame retardance and low specific gravity...
|
|||
| Linear Mold Shrinkage, Flow |
0.0050
-
0.0080
cm/cm <br>@Thickness 3.20 mm
|
0.0050
-
0.0080
in/in <br>@Thickness 0.126 in
|
SABIC Method |
|
SABIC Innovative Plastics NORYL NH6010B PPE+HIPS (Asia Pacific)
Noryl* NH6010B resin is a high performance, modified PPE-PS blend that exhibits an excellent balance of lower smoke production upon burning, nonhalogenated flame retardance and low specific gravity...
|
|||
| Linear Mold Shrinkage, Flow | 0.0040 - 0.0080 cm/cm | 0.0040 - 0.0080 in/in | on Tensile Bar; SABIC Method |
|
SABIC Innovative Plastics Valox® 451E PBT (Europe-Africa-Middle East)
VALOX 451E is 20% glass reinforced, flame retardant PBT injection moulding resin.
|
|||
| Linear Mold Shrinkage, Flow | 0.0060 - 0.0080 cm/cm | 0.0060 - 0.0080 in/in | SABIC Method |
|
SABIC Innovative Plastics LNP Thermotuf PK005EI2 PA 6 (Europe-Africa-Middle East)
LNP* THERMOTUF* PK005EI2 is a compound based on PA 6 resin containing Impact Modifier, Mineral. Added features include: High Impact.This data was supplied by SABIC-IP for the Europe-Africa-Middle Ea..
|
|||
| Linear Mold Shrinkage, Flow | 0.0050 - 0.0080 cm/cm | 0.0050 - 0.0080 in/in | on Tensile Bar; E2P method |
|
Eurostar Starflam BFR330A PA6, Glass Bead Reinforced, Flame Retardant, Injection Molded
Starflam BFR330A is a Flame Retardant, Glass Bead Reinforced Polyamide 6, Injection Molding ResinInformation provided by Eurostar.
|
|||
| Linear Mold Shrinkage, Flow |
0.0050
-
0.0080
cm/cm <br>@Thickness 3.20 mm
|
0.0050
-
0.0080
in/in <br>@Thickness 0.126 in
|
SABIC Method |
|
SABIC Innovative Plastics GELOY CR7500 ASA (Asia Pacific)
High heat ASA with optimum flow-impact balance. For Automotive applications and Automotive colors only.
|
|||
| Linear Mold Shrinkage, Flow |
0.0040
-
0.0080
cm/cm <br>@Thickness 3.20 mm
|
0.0040
-
0.0080
in/in <br>@Thickness 0.126 in
|
SABIC Method |
|
SABIC Innovative Plastics Lexan® EXL1433T PC Copolymer
Lexan* EXL1433T polycarbonate (PC) siloxane copolymer resin is a UV stabilized transparent injection molding grade. This resin offers excellent low temperature (-30 C) ductility in combination with ..
|
|||
| Linear Mold Shrinkage, Flow |
0.0060
-
0.0080
cm/cm <br>@Thickness 3.20 mm
|
0.0060
-
0.0080
in/in <br>@Thickness 0.126 in
|
SABIC Method |
|
SABIC Innovative Plastics NORYL FE8000S PPE+PS (Asia Pacific)
Noryl* FE8000S resin is an unfilled modified polyphenylene ether resin designed for fluid handling applications. This resin is suitable for multiple conversion routes and will be available in custom..
|
|||