| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Linear Mold Shrinkage, Flow | 0.011 - 0.012 cm/cm | 0.011 - 0.012 in/in | ASTM D955 |
|
PolyOne Maxxam™ PD 20 TF Black Polypropylene, Unspecified (PP, Unspecified)
PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car..
|
|||
| Linear Mold Shrinkage, Flow | 0.010 - 0.012 cm/cm | 0.010 - 0.012 in/in | ASTM D955 |
|
PolyOne Nymax™ 600 A Natural F Polyamide 6 Alloy (Nylon 6 Alloy)
The Nymax® 600 Blend Series of nylon 6 materials are salt-and-pepper pelletized blends combining select nylon resins and process aids, performance modifiers, and color concentrates. These materials..
|
|||
| Linear Mold Shrinkage, Flow | 0.0080 - 0.012 cm/cm | 0.0080 - 0.012 in/in | ASTM D955 |
|
PolyOne Trilliant™ HC X HC5200-0026 RS Natural Polypropylene, Unspecified (PP, Unspecified)
Information provided by PolyOne
|
|||
| Linear Mold Shrinkage, Flow | 0.0070 - 0.012 cm/cm | 0.0070 - 0.012 in/in | ASTM D955 |
|
PolyOne Versaflex™ HC 2110-57B Thermoplastic Elastomer (TPE)
Versaflex™ HC 2110-57B is a TPE designed for use in the healthcare industry offering low stiction and good compression set. New Product. Commercial specifications have not been established. - Bonds..
|
|||
| Linear Mold Shrinkage, Flow | 0.0080 - 0.012 cm/cm | 0.0080 - 0.012 in/in | ASTM D955 |
|
PolyOne Versaflex™ OM 3060-1 Thermoplastic Elastomer (TPE)
Versaflex™ OM 3060-1 is a clear, medical compliant overmold designed to adhere to multiple substrates. - Excellent bond to PC, ABS, PC/ABS, PC/PETG, and PC/PBT - Rubber Feel - Soft TouchVersaflex™..
|
|||
| Linear Mold Shrinkage, Flow | 0.0090 - 0.012 cm/cm | 0.0090 - 0.012 in/in | ISO 294-4 |
|
Polyplastic Armlen® PP MF 40-3M Polypropylene Copolymer, 40% Calcium Carbonate
Injection moldingInformation provided by PolyPlastic Group.
|
|||
| Linear Mold Shrinkage, Flow |
0.010
-
0.012
cm/cm <br>@Thickness 3.20 mm
|
0.010
-
0.012
in/in <br>@Thickness 0.126 in
|
SABIC Method |
|
SABIC Innovative Plastics EXTEM XH1005 TPI Resin (Asia Pacific)
Thermoplastic Polyimide Extem* XH1005 Resin.
|
|||
| Linear Mold Shrinkage, Flow |
0.010
-
0.012
cm/cm <br>@Thickness 3.20 mm
|
0.010
-
0.012
in/in <br>@Thickness 0.126 in
|
SABIC Method |
|
SABIC Innovative Plastics EXTEM XH1015 TPI Resin (Europe-Africa-Middle East)
Thermoplastic Polyimide Extem* XH1015 Resin.
|
|||
| Linear Mold Shrinkage, Flow | 0.0060 - 0.012 cm/cm | 0.0060 - 0.012 in/in | ASTM D955 |
|
PolyOne Dynaflex™ G7970-9 NSFG Thermoplastic Elastomer (TPE)
Dynaflex™ G7970-9 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,..
|
|||
| Linear Mold Shrinkage, Flow | 0.0070 - 0.012 cm/cm | 0.0070 - 0.012 in/in | ASTM D955 |
|
PolyOne Dynalloy™ 8900-80 Thermoplastic Elastomer (TPE)
Dynalloy™ 8900-series is an innovative thermoplastic elastomer selection formulated to provide the injection molder with a product capable of overmolding and bonding to both low-density polyethylen..
|
|||
| Linear Mold Shrinkage, Flow | 0.0070 - 0.012 cm/cm | 0.0070 - 0.012 in/in | ASTM D955 |
|
PolyOne Dynalloy™ 8900-60 Thermoplastic Elastomer (TPE)
Dynalloy™ 8900-series is an innovative thermoplastic elastomer selection formulated to provide the injection molder with a product capable of overmolding and bonding to both low-density polyethylen..
|
|||
| Linear Mold Shrinkage, Flow | 0.0080 - 0.012 cm/cm | 0.0080 - 0.012 in/in | ASTM D955 |
|
PolyOne Geon™ Vinyl Flexible B5D02 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
|
|||
| Linear Mold Shrinkage, Flow |
0.0050
-
0.012
cm/cm <br>@Thickness 3.20 mm
|
0.0050
-
0.012
in/in <br>@Thickness 0.126 in
|
ASTM D955 |
|
LG Chemical Lupox® SG3250A PBT+PET+MF25%
Description: Injection Molding, PBT+PET+MF25%, Good SurfaceApplication: Automotive (Head Lamp Bezel)CAS No. 24968-12-5, 25038-59-9 and 14807-96-6Information provided by LG Chemical
|
|||
| Linear Mold Shrinkage, Flow |
0.0050
-
0.012
cm/cm <br>@Thickness 3.20 mm
|
0.0050
-
0.012
in/in <br>@Thickness 0.126 in
|
ASTM D955 |
|
LG Chemical Lupox® SG3250M PBT+PET+MF25%
Description: Injection Molding, PBT+PET+MF25%, Good SurfaceApplication: Automotive (Head Lamp Bezel)CAS No. 24968-12-5, 25038-59-9 and 14807-96-6Information provided by LG Chemical
|
|||
| Linear Mold Shrinkage, Flow | 0.0090 - 0.012 cm/cm | 0.0090 - 0.012 in/in | |
|
LATI Latamid 66 S/30 PA 66, 30% Glass Bead Reinforced
Polyamide 66 (PA66) based compound. Glass beads. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p.A.
|
|||
| Linear Mold Shrinkage, Flow | 0.0090 - 0.012 cm/cm | 0.0090 - 0.012 in/in | |
|
LATI Latilub 62-15ST PA6
Self-lubricating product based on Polyamide 6 (PA6). Silicone / PTFE.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Term..
|
|||
| Linear Mold Shrinkage, Flow | 0.0080 - 0.012 cm/cm | 0.0080 - 0.012 in/in | |
|
LATI Latistat 83-05 POM, Impact Modified
Dissipative product based on Polyamide 12 (PA12), impact modified. Unfilled. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indust..
|
|||
| Linear Mold Shrinkage, Flow |
0.010
-
0.012
cm/cm <br>@Thickness 3.20 mm
|
0.010
-
0.012
in/in <br>@Thickness 0.126 in
|
SABIC Method |
|
SABIC Innovative Plastics Xenoy® 5720U PBT+PC (Europe-Africa-Middle East)
Unfilled PBT+PC alloy. Outstanding low temperature impact/chemical resistance. UV stabilized version of XENOY
|
|||
| Linear Mold Shrinkage, Flow |
0.0090
-
0.012
cm/cm <br>@Thickness 3.20 mm
|
0.0090
-
0.012
in/in <br>@Thickness 0.126 in
|
SABIC Method |
|
SABIC Innovative Plastics Xenoy® CL402 PBT+PC (Asia Pacific)
XENOY CL402 is a high viscosity, unfilled, elastomer modified PC/PBT blend for extrusion/blowmolding applications. ISO1043-label: PC+PBT-I.This data was supplied by SABIC-IP for the Asia Pacific reg..
|
|||
| Linear Mold Shrinkage, Flow |
0.0080
-
0.012
cm/cm <br>@Thickness 3.20 mm
|
0.0080
-
0.012
in/in <br>@Thickness 0.126 in
|
SABIC Method |
|
SABIC Innovative Plastics Xenoy® IQ1103 PBT+PC (Asia Pacific)
Xenoy iQ*1103 resin - Environmentally responsible and sustainable low carbon footprint resin. Xenoy iQ1103 is an unreinforced, impact modified alloy of PC (polycarbonate) + Valox iQ* PBT (polybuty..
|
|||
| Linear Mold Shrinkage, Flow | 0.010 - 0.012 cm/cm | 0.010 - 0.012 in/in | SABIC Method |
|
SABIC Innovative Plastics LNP STAT-KON PX08024 PA 6 (Europe-Africa-Middle East)
LNP* STAT-KON* PX08024 is a compound based on PA 6 resin containing Mineral. Added features include; Electrically Conductive, Easy Molding.
|
|||
| Linear Mold Shrinkage, Flow |
0.0090
-
0.012
cm/cm <br>@Thickness 3.20 mm
|
0.0090
-
0.012
in/in <br>@Thickness 0.126 in
|
SABIC Method |
|
SABIC Innovative Plastics NORYL GTX GTX902 PPE+PS+PA (Asia Pacific)
Unreinforced. Excellent chemical resistance and paintability. 312F (155C) HDT.
|
|||
| Linear Mold Shrinkage, Flow |
0.010
-
0.012
cm/cm <br>@Thickness 3.20 mm
|
0.010
-
0.012
in/in <br>@Thickness 0.126 in
|
SABIC Method |
|
SABIC Innovative Plastics Noryl GTX GTX966 PPE+PA66
>PPE+PA66-I-TD10
|
|||
| Linear Mold Shrinkage, Flow |
0.0080
-
0.012
cm/cm <br>@Thickness 3.20 mm
|
0.0080
-
0.012
in/in <br>@Thickness 0.126 in
|
SABIC Method |
|
SABIC Innovative Plastics NORYL PPX PPX7110 PPE+PP (Asia Pacific)
PPE+PP blend. High Impact, Good Heat Resistance
|
|||
| Linear Mold Shrinkage, Flow |
0.0030
-
0.012
cm/cm <br>@Thickness 3.20 mm
|
0.0030
-
0.012
in/in <br>@Thickness 0.126 in
|
ASTM D955 |
|
Samsung Cheil Industries Infino® XP-2130A PPS
Information provided by Samsung Cheil Industries.
|
|||
| Linear Mold Shrinkage, Flow |
0.0080
-
0.012
cm/cm <br>@Thickness 3.20 mm
|
0.0080
-
0.012
in/in <br>@Thickness 0.126 in
|
SABIC Method |
|
SABIC Innovative Plastics NORYL GTX GTX675 PPE+PA6
Noryl GTX* GTX675 Resin is a blend of Polyphenylene Ether(PPE) + Polyamide(PA) resin that is mineral filled, conductive, and suitable for injection molding. The conductivity level is optimized to a..
|
|||
| Linear Mold Shrinkage, Flow | 0.0080 - 0.012 cm/cm | 0.0080 - 0.012 in/in | DIS 294-4 |
|
Wellman Wellamid® GFT1835-WBK1 Nylon 66, 17% Glass Fiber Reinforced, Impact Modified
All information provided by Wellman Engineered Resins.
|
|||
| Linear Mold Shrinkage, Flow | 0.010 - 0.012 cm/cm | 0.010 - 0.012 in/in | on Tensile Bar; ISO 294 |
|
Eurostar Staramide AST43 PA66, Impact Modified, Injection Molded
AST43 is a Low Temperature Impact Modified Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier.
|
|||
| Linear Mold Shrinkage, Flow | 0.010 - 0.012 cm/cm | 0.010 - 0.012 in/in | on Tensile Bar; E2P method |
|
Eurostar Staramide R1000HI620 PA66, Impact Modified, Injection Molded
Staramide R1000HI620 is an Impact Modified Polyamide 66 Injection Molding Resin (also known as R1000HI010)Information provided by Eurostar.
|
|||
| Linear Mold Shrinkage, Flow | 0.0080 - 0.012 cm/cm | 0.0080 - 0.012 in/in | on Tensile Bar; E2P method |
|
Eurostar Staramide BG3ST42 PA6, Glass Fiber Filled, Impact Modified, Injection Molded
Staramide BG3ST42 is an Impact Modified and Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar.
|
|||