| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Linear Mold Shrinkage, Flow | 0.013 cm/cm | 0.013 in/in | Nilit |
|
Nilit Polynil® C50L Externally Lubricated PA66/6
Description: Polynil C50L shows better surface finish, flow and elongation than a comparable homopolymer. Key characteristics: Excellent flowHigh elongationGood impact strengthGood overall mechanica..
|
|||
| Linear Mold Shrinkage, Flow | 0.013 - 0.021 cm/cm | 0.013 - 0.021 in/in | ASTM D955 |
|
PolyOne Dynaflex™ G7640-9 (Black) Thermoplastic Elastomer (TPE)
Dynaflex™ G7640-9 (Black) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropyl..
|
|||
| Linear Mold Shrinkage, Flow | 0.013 - 0.021 cm/cm | 0.013 - 0.021 in/in | ASTM D955 |
|
PolyOne Dynaflex™ G7930-9 NSFG Thermoplastic Elastomer (TPE)
Dynaflex™ G7930-9 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. - NSF 51 approved - FDA (see Notes) - Overmold Adhesion to Polypropylene - Soft To..
|
|||
| Linear Mold Shrinkage, Flow | 0.013 - 0.021 cm/cm | 0.013 - 0.021 in/in | ASTM D955 |
|
PolyOne Dynaflex™ G7940-9001-02 Thermoplastic Elastomer (TPE)
Dynaflex™ G7940-9001-02 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Non-Slip Grip - Overmold Adhesion..
|
|||
| Linear Mold Shrinkage, Flow | 0.013 - 0.019 cm/cm | 0.013 - 0.019 in/in | ASTM D955 |
|
PolyOne Dynaflex™ G7950-1001-00 Thermoplastic Elastomer (TPE)
Dynaflex™ G7950-1001-00 is an easy processing, general purpose material designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypro..
|
|||
| Linear Mold Shrinkage, Flow | 0.013 - 0.021 cm/cm | 0.013 - 0.021 in/in | ASTM D955 |
|
PolyOne Dynaflex™ G7640-1 (Natural) Thermoplastic Elastomer (TPE)
Dynaflex™ G7640-1 (Natural) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Non-Slip Grip - Overmold Adhe..
|
|||
| Linear Mold Shrinkage, Flow | 0.013 cm/cm | 0.013 in/in | ISO 294 |
|
Inno-Comp INNOPOL® CS 2-1000 Polypropylene Block-Copolymer
INNOPOL® CS 2-1000 is a polypropylene block-copolymer compound. This grade is available in natural and custom colored form.INNOPOL® CS 2-1000 is developed for producing injection molded automo..
|
|||
| Linear Mold Shrinkage, Flow |
0.013
cm/cm @Thickness 3.17 mm |
0.013
in/in @Thickness 0.125 in |
1/8" Section |
|
Lucent Polymers 6-01 Nylon 6, General Purpose, Injection Grade
Add "R" for Added ReleaseAdd "U" for UV StabilizedTypical Properties, Dry as MoldedInformation provided by Lucent Polymers, Inc.
|
|||
| Linear Mold Shrinkage, Flow | 0.013 - 0.016 cm/cm | 0.013 - 0.016 in/in | |
|
LATI Latilub 66-20T PA66, PTFE Filled
Self-lubricating product based on Polyamide 66 (PA66). PTFE. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastic..
|
|||
| Linear Mold Shrinkage, Flow | 0.013 - 0.0165 cm/cm | 0.013 - 0.0165 in/in | |
|
LATI Latistat 67-08 PA66, Impact Modified
Dissipative product based on Polyamide 66 (PA66), impact modified. Unfilled.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industr..
|
|||
| Linear Mold Shrinkage, Flow |
0.013
cm/cm @Thickness 3.17 mm |
0.013
in/in @Thickness 0.125 in |
ASTM D955 |
|
Techmer ES Elastoblend® PA6 IM HS L
Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impact Modified and LubricatedInformation provided by TP Composites, Inc.
|
|||
| Linear Mold Shrinkage, Flow |
0.013
cm/cm @Thickness 3.17 mm |
0.013
in/in @Thickness 0.125 in |
ASTM D955 |
|
Techmer ES Elastoblend® PA6/6 GF14 IM4 HS L BKN 14% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 14% Filler by WeightAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubri..
|
|||
| Linear Mold Shrinkage, Flow |
0.013
cm/cm @Time 86400 sec |
0.013
in/in @Time 24.0 hour |
ISO 294 |
|
SABIC Innovative Plastics LNP LUBRICOMP WI001 PBT (Europe-Africa-Middle East)
LNP* LUBRICOMP* WI001 is a compound based on Polybutylene Terephalate resin containing Silicone. Added features include; Inernally Lubricated.
|
|||
| Linear Mold Shrinkage, Flow |
0.013
cm/cm @Thickness 3.17 mm |
0.013
in/in @Thickness 0.125 in |
ASTM D955 |
|
Techmer ES HiFill® PA6/6 GB25 L BK 25% Glass Bead Filler
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 25% Filler by WeightAdditive: LubricantFeatures: LubricatedAppearance: BlackInformation provided by TP Composites, Inc.
|
|||
| Linear Mold Shrinkage, Flow |
0.013
cm/cm @Thickness 3.17 mm |
0.013
in/in @Thickness 0.125 in |
ASTM D955 |
|
Techmer ES HiFill® PA6/6 GF8 IM4 HS L 8% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 8% Filler by WeightAdditive: LubricantFeatures: Lubricated Appearance: BlackInformation provided by TP Compo..
|
|||
| Linear Mold Shrinkage, Flow |
0.013
cm/cm @Thickness 3.17 mm |
0.013
in/in @Thickness 0.125 in |
ASTM D955 |
|
Techmer ES Luriblend® PA6/6 04003 Nylon 66
Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and Molybdenum Disulfide Lubricant(15%)Features: Lubricated, Good Wear Resistance, Low Friction and Heat StabilizedAppearance: Natu..
|
|||
| Linear Mold Shrinkage, Flow |
0.013
cm/cm @Time 86400 sec |
0.013
in/in @Time 24.0 hour |
ASTM D 955 |
|
SABIC Innovative Plastics LNP Thermocomp P1000P PA 6 (Asia Pacific)
LNP* Thermocomp* P1000P is a compound based on Nylon 6 resin. Added features of this material include: Exceptional Processing.This data was supplied by SABIC-IP for the Asia Pacific region.
|
|||
| Linear Mold Shrinkage, Flow |
0.013
-
0.015
cm/cm @Thickness 3.20 mm |
0.013
-
0.015
in/in @Thickness 0.126 in |
SABIC Method |
|
SABIC Innovative Plastics NORYL GTX GTX678 PPE+PA (Asia Pacific)
Noryl GTX678 resin is a high performance blend of PPE/PA that exhibits an excellent balance on non-halogenated flame retardance, conductivity, ductility, and high-heat resistance. This grade can be..
|
|||
| Linear Mold Shrinkage, Flow | 0.013 cm/cm | 0.013 in/in | DAM; ISO 294-4 |
|
DSM Stanyl® 46HF4130 Nylon 46-30% Glass Reinforced (European and Asian Grade) (Cond)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
|
|||
| Linear Mold Shrinkage, Flow | 0.013 cm/cm | 0.013 in/in | DAM; ISO 294-4 |
|
DSM Stanyl® TW200F6 Nylon 46-30% Glass Reinforced (European Grade) (Cond)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
|
|||
| Linear Mold Shrinkage, Flow | 0.013 cm/cm | 0.013 in/in | ISO 294-4 2577 |
|
DuPont Performance Polymers Hytrel® DYM350BK TPC-ET+PBT
(Unverified Data**)
Medium Modulus Polyester Elastomer with Excellent Impact Resistance Developed for Air Bag Door ApplicationsInformation provided by DuPont Performance Polymers
|
|||
| Linear Mold Shrinkage, Flow | 0.013 cm/cm | 0.013 in/in | ISO 294-4 2577 |
|
DuPont Performance Polymers Sorona® 3301 NC010 Polytrimethylene Terephthalate (PTT)
(Unverified Data**)&l
Unreinforced Renewably Sourced Polytrimethylene Terephthalate Sorona 3301 NC010 is an unreinforced polytrimethylene terephthalate resin containing 35% renewably sourced ingredients by weight with su..
|
|||
| Linear Mold Shrinkage, Flow |
0.013
cm/cm @Thickness 2.00 mm |
0.013
in/in @Thickness 0.0787 in |
DAM; ISO 294-4 |
|
DuPont Performance Polymers Zytel® FE310001 NC010 Nylon 612
Zytel® FE310001 NC010 is a high viscosity polyamide 612 resin that is suitable for extrusion applications, such as monofilaments and tubing.Information provided by DuPont Performance Polymers
|
|||
| Linear Mold Shrinkage, Flow | 0.013 cm/cm | 0.013 in/in | DAM; ISO 294-4 2577 |
|
DuPont Performance Polymers Zytel® 103HSL NC010 Nylon 66
(Unverified Data**)
Unreinforced Heat Stabilized Polyamide 66 Zytel 103HSL NC010 is a heat stabilized lubricated polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
|
|||
| Linear Mold Shrinkage, Flow | 0.013 cm/cm | 0.013 in/in | |
|
BASF Novolen® 2660 M Polypropylene
UV stabilized grade for injection molded parts.Data was collected by ISO methods and provided by BASF.
|
|||
| Linear Mold Shrinkage, Flow | 0.013 cm/cm | 0.013 in/in | |
|
BASF Novolen® 3240 NC Polypropylene
Grade containing nucleating agent for transparent injection molded parts.Data was collected by ISO methods and provided by BASF.
|
|||
| Linear Mold Shrinkage, Flow | 0.013 cm/cm | 0.013 in/in | |
|
BASF Novolen® 1148 UC Polypropylene
Nucleated grade with antistatic agent for injection molded parts.Data was collected by ISO methods and provided by BASF.
|
|||
| Linear Mold Shrinkage, Flow | 0.013 cm/cm | 0.013 in/in | |
|
BASF Novolen® 2440 K Polypropylene
Data was collected by ISO methods and provided by BASF.
|
|||
| Linear Mold Shrinkage, Flow | 0.013 - 0.0165 cm/cm | 0.013 - 0.0165 in/in | |
|
LATI Latiohm 66-10 H2 CNT CE/10 PA66, 10% Mineral Fiber Reinforced, Heat Stabilized
Semiconductive/dissipative product based on Polyamide 66 (PA66). Heat stabilized. Carbon nanotubes. Mineral filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North Ame..
|
|||
| Linear Mold Shrinkage, Flow | 0.013 cm/cm | 0.013 in/in | DAM; ISO 294-4 2577 |
|
DuPont Performance Polymers Zytel® 105F BK010 Nylon 66
(Unverified Data**)
Unreinforced UV Stabilized Polyamide 66 Zytel 105F BK010 is a lubricated fast cycling weather resistant PA 66 resin. Zytel 105F BK010 contains finely dispersed carbon black.Information provided by D..
|
|||