| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Linear Mold Shrinkage, Flow | 0.013 cm/cm | 0.013 in/in | Euronil |
|
Nilit Nilamid A H2 FR HF2 Unfilled, Flame Retardant PA66/6 Co-Polymer
Description: Nilamid A H2 FR HF2 is an unfilled, flame retardant NYLON 66/6 co-polymer that does not contain halogen or red phosphorous. This product combines excellent flow characteristics and extr..
|
|||
| Linear Mold Shrinkage, Flow | 0.013 cm/cm | 0.013 in/in | Nilit |
|
Nilit Polynil® C50L Externally Lubricated PA66/6
Description: Polynil C50L shows better surface finish, flow and elongation than a comparable homopolymer. Key characteristics: Excellent flowHigh elongationGood impact strengthGood overall mechanica..
|
|||
| Linear Mold Shrinkage, Flow | 0.013 - 0.021 cm/cm | 0.013 - 0.021 in/in | ASTM D955 |
|
PolyOne Dynaflex™ G7640-9 (Black) Thermoplastic Elastomer (TPE)
Dynaflex™ G7640-9 (Black) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropyl..
|
|||
| Linear Mold Shrinkage, Flow | 0.013 - 0.019 cm/cm | 0.013 - 0.019 in/in | ASTM D955 |
|
PolyOne Dynaflex™ G7950-9 NSFG Thermoplastic Elastomer (TPE)
Dynaflex™ G7950-9 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,..
|
|||
| Linear Mold Shrinkage, Flow | 0.013 cm/cm | 0.013 in/in | Euronil |
|
Nilit Nilamid A3 H ZE High Impact PA66
Description: Nilamid A3 H ZE was developed for applications which are subjected to very high shock loads, also at minus temperatures. It has good impact performance, whilst maintaining good strength..
|
|||
| Linear Mold Shrinkage, Flow |
0.013
-
0.016
cm/cm @Thickness 3.20 mm |
0.013
-
0.016
in/in @Thickness 0.126 in |
ASTM D955 |
|
LG Chemical LUCEL FW720F Modified POM, Friction Resistance, Abrasion Resistance
Feature: Injection Molding, Modified POM, Friction Resistance, Abrasion ResistanceApplication: Gears, Printer Roller Pumps, Gear Worm WheelsCAS No. 66455-31-0 and 9002-84-2Information provided by LG..
|
|||
| Linear Mold Shrinkage, Flow |
0.013
cm/cm @Thickness 2.00 mm |
0.013
in/in @Thickness 0.0787 in |
|
|
Aardvark Polymers Aardalloy® 3300 POM Alloy Rotational Molding Resin
Aardalloy 3300 is an acetal alloy formulated for enhanced impact resistance and elongation.Aardalloy 3300 maintains the high degree of chemical resistance and low fuel permeation rates of unfilled a..
|
|||
| Linear Mold Shrinkage, Flow | 0.013 cm/cm | 0.013 in/in | 60x60x2; 260°C / MT 80°C; 600 bar; ISO 294-4 |
|
Lanxess Durethan® BC 550 DUSXBL 900116 Nylon 6
PA 6, non-reinforced, extrusion, Blastorm, impact modified, heat-ageing stabilizedInformation provided by LANXESS.
|
|||
| Linear Mold Shrinkage, Flow | 0.013 - 0.016 cm/cm | 0.013 - 0.016 in/in | |
|
LATI Latene® 7H2-V2HF PP Homopolymer, Heat Stabilized, Flame Retardant
Polypropylene homopolymer (PPh) based compound. Heat stabilized. UL94 V-2 classified, halogens-based flame retardants free.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; No..
|
|||
| Linear Mold Shrinkage, Flow | 0.013 - 0.017 cm/cm | 0.013 - 0.017 in/in | on Tensile Bar; SABIC Method |
|
SABIC Innovative Plastics LNP LUBRICOMP RN001XXC PA 66 (Europe-Africa-Middle East)
LNP* Lubricomp* RN001XXC is a compound based on Nylon 66 resin containing MOS2.
|
|||
| Linear Mold Shrinkage, Flow |
0.013
cm/cm @Thickness 3.17 mm |
0.013
in/in @Thickness 0.125 in |
ASTM D955 |
|
Techmer ES Elastoblend® PA6 IM HS L BK
Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impact Modified and LubricatedUL File Number: E157318Processing Method: In..
|
|||
| Linear Mold Shrinkage, Flow |
0.013
cm/cm @Time 86400 sec |
0.013
in/in @Time 24.0 hour |
ASTM D955 |
|
SABIC Innovative Plastics LNP LUBRICOMP WAL34 PBT
LNP* LUBRICOMP* WAL34 is a compound based on (PBT resin containing 15% PTFE, 20% Aramid Fiber. Added features of this material include: Wesr Resistant.
|
|||
| Linear Mold Shrinkage, Flow |
0.013
cm/cm @Thickness 3.17 mm |
0.013
in/in @Thickness 0.125 in |
ASTM D955 |
|
Techmer ES Elastoblend® PA6/66 IM 6040 MB
Availability: North AmericaForms: PelletsAdditive: Nucleating Agent, Heat Stabilizer, Lubricant and Impact ModifierFeatures: Copolymer, Nucleated, Heat Stabilized, Lubricant and Impact ModifiedInfor..
|
|||
| Linear Mold Shrinkage, Flow |
0.013
cm/cm @Thickness 3.17 mm |
0.013
in/in @Thickness 0.125 in |
ASTM D955 |
|
Techmer ES HiFill FR® PA6/6 FR IM BK
Availability: North AmericaForms: PelletsAdditive: Impact ModifierFeatures: Flame Retardant and Impact ModifiedAppearance: BlackTPCI# 9993101Information provided by TP Composites, Inc.
|
|||
| Linear Mold Shrinkage, Flow |
0.013
cm/cm @Thickness 3.17 mm |
0.013
in/in @Thickness 0.125 in |
ASTM D955 |
|
Techmer ES Luriblend® PA6 ML2 HS BK Nylon 6
Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and Molybdenum Disulfide Lubricant(2%)Features: Good Wear Resistance, Low Friction, Heat Stabilized and LubricatedAppearance: Blac..
|
|||
| Linear Mold Shrinkage, Flow |
0.013
-
0.016
cm/cm @Thickness 3.20 mm |
0.013
-
0.016
in/in @Thickness 0.126 in |
SABIC Method |
|
SABIC Innovative Plastics NORYL GTX NX0031 PPE+PA
NORYL GTX* NX0031 resin is a conductive resin specially designed for electrostatic painting and powder coating applications. This material combines high impact, good flow and conductivity. The mate..
|
|||
| Linear Mold Shrinkage, Flow |
0.013
-
0.014
cm/cm @Thickness 3.20 mm |
0.013
-
0.014
in/in @Thickness 0.126 in |
SABIC Method |
|
SABIC Innovative Plastics NORYL GTX GTX626 PPE+PS+PA
Blowmolding and extrusion. High heat and chemical resistant.
|
|||
| Linear Mold Shrinkage, Flow | 0.013 cm/cm | 0.013 in/in | ISO 294-4 2577 |
|
DuPont Performance Polymers Sorona® FG3301 NC010 Polytrimethylene Terephthalate (PTT)
(Unverified Data**)
Unreinforced Renewably Sourced Polytrimethylene Terephthalate Developed for Food Contact Applications Sorona FG3301 NC010 is an unreinforced polytrimethylene terephthalate resin containing 35% renew..
|
|||
| Linear Mold Shrinkage, Flow | 0.013 cm/cm | 0.013 in/in | DAM; ISO 294-4 2577 |
|
DuPont Performance Polymers Zytel® ST7301 BK356 Nylon 6
(Unverified Data**)
Super Toughened Polyamide 6 Zytel ST7301 BK356 is a Super Tough heat stabilized lubricated black polyamide 6 resin for injection molding and extrusion. It offers outstanding impact resistance over a..
|
|||
| Linear Mold Shrinkage, Flow | 0.013 cm/cm | 0.013 in/in | Eurotec |
|
Eurotec® Tecomid® NA40 NL FA50 PA6.6, unfilled, flame retardant - halogen free, natural
Information provided by Eurotec®
|
|||
| Linear Mold Shrinkage, Flow | 0.013 cm/cm | 0.013 in/in | |
|
BASF Novolen® 1100 L Polypropylene, Injection Molding Grade
Injection molded parts, film tape, fibrillated film and monofilaments.Data was collected by ISO methods and provided by BASF.
|
|||
| Linear Mold Shrinkage, Flow | 0.013 cm/cm | 0.013 in/in | |
|
BASF Novolen® 2348 TC Polypropylene
Grade with nucleating and antistatic agents for injection molded parts.Data was collected by ISO methods and provided by BASF.
|
|||
| Linear Mold Shrinkage, Flow | 0.013 cm/cm | 0.013 in/in | |
|
BASF Novolen® 3240 NC Polypropylene
Grade containing nucleating agent for transparent injection molded parts.Data was collected by ISO methods and provided by BASF.
|
|||
| Linear Mold Shrinkage, Flow | 0.013 cm/cm | 0.013 in/in | |
|
BASF Novolen® 3248 TC Polypropylene
Easy-flowing grade containing nucleating and antistatic agents for transparent injection molded parts.Data was collected by ISO methods and provided by BASF.
|
|||
| Linear Mold Shrinkage, Flow | 0.013 cm/cm | 0.013 in/in | |
|
BASF Procom® C40H 451 Polypropylene
Used for: instrument panels, motor vehicle grills, heater boxes.Data was collected by ISO methods and provided by BASF.
|
|||
| Linear Mold Shrinkage, Flow | 0.013 - 0.017 cm/cm | 0.013 - 0.017 in/in | ASTM D955 |
|
Ravago Manufacturing Americas Hylon® N2200 HL Nylon 6/6
(discontinued **)
Available in North America Additive: Heat Stabilizer and Lubricant Features: Lubricated and Heat StabilizedRoHS CompliantForm: Pellets Color: BlackProcessing Method: Injection MoldingInformation pr..
|
|||
| Linear Mold Shrinkage, Flow | 0.013 cm/cm | 0.013 in/in | |
|
BASF Novolen® 1148 RC Polypropylene
Nucleated grade with antistatic agent for injection molded parts.Data was collected by ISO methods and provided by BASF.
|
|||
| Linear Mold Shrinkage, Flow | 0.013 cm/cm | 0.013 in/in | |
|
BASF Novolen® 3248 RC Polypropylene
Grade containing nucleating and antistatic agents for injection molded parts.Data was collected by ISO methods and provided by BASF.
|
|||
| Linear Mold Shrinkage, Flow | 0.013 - 0.0165 cm/cm | 0.013 - 0.0165 in/in | |
|
LATI Latiohm 66-10 H2 CNT CE/10 PA66, 10% Mineral Fiber Reinforced, Heat Stabilized
Semiconductive/dissipative product based on Polyamide 66 (PA66). Heat stabilized. Carbon nanotubes. Mineral filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North Ame..
|
|||
| Linear Mold Shrinkage, Flow | 0.013 cm/cm | 0.013 in/in | DAM; ISO 294-4 2577 |
|
DuPont Performance Polymers Zytel® 105F BK010 Nylon 66
(Unverified Data**)
Unreinforced UV Stabilized Polyamide 66 Zytel 105F BK010 is a lubricated fast cycling weather resistant PA 66 resin. Zytel 105F BK010 contains finely dispersed carbon black.Information provided by D..
|
|||